# US 2023/0036173 A1 · Casting elements and methods of making the same using low temperature solidification

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0036173 A1
- Document ID: US20230036173A1
- Status: Published application
- Kind: A1
- Application number: 17/757,950
- Filed: 2020-12-24
- Published: 2023-02-02
- Earliest claimed: 2019-12-24
- Assignees: Rutgers, The State University of New Jersey
- Applicants: Rutgers, The State University of New Jersey
- Inventors: Richard E. Riman; Kevin Blinn
- Web page: https://patentgrep.com/patent/US20230036173A1

## CPC

- B22C 1/12: for manufacturing permanent moulds or cores
- B22C 1/14: for separating the pattern from the mould
- B22C 1/162: {use of a gaseous treating agent for hardening the binder}
- B22C 1/18: of inorganic agents {(B22C1/162 takes precedence)}
- B22C 1/181: {Cements, oxides or clays}
- B22C 1/183: {Sols, colloids or hydroxide gels}
- B22C 1/185: {containing phosphates, phosphoric acids or its derivatives}
- B22C 1/186: {contaming ammonium or metal silicates, silica sols}
- B22C 3/00: Selection of compositions for coating the surfaces of moulds, cores, or patterns
- B22C 9/02: Sand moulds or like moulds for shaped castings
- B22C 9/04: Use of lost patterns
- B22C 9/061: {Materials which make up the mould}
- B22C 9/123: {Gas-hardening}
- C04B 28/005: {containing gelatineous or gel forming binders, e.g. gelatineous Al(OH)3, sol-gel binders}
- C04B 28/105: {Magnesium oxide or magnesium carbonate cements}
- C04B 28/188: {the Ca-silicates being present in the starting mixture}
- C04B 28/24: containing alkyl, ammonium or metal silicates; containing silica sols {(reaction mixtures resulting in mineral polymers C04B28/006; polymeric reaction products of alkali metal silicates with isocyanates C08G18/3895)}
- C04B 28/34: containing cold phosphate binders
- C04B 28/348: {the starting mixture also containing one or more reactive oxides}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Foundry casting elements and methods of forming the same, the methods including: forming an aqueous slurry including an inorganic binder precursor, shaping the slurry using a pattern, curing the shaped slurry using a low temperature solidification process to form a casting element, and removing the pattern from the casting element.

## Claims

### Claim 1

A method of forming a foundry casting element, the method comprising:
forming an aqueous slurry comprising a solid inorganic binder material or a precursor thereof;
shaping the slurry using a pattern;
curing the shaped slurry at a temperature of less than 350° C. to form a casting element; and
removing the pattern from the casting element,
wherein the slurry optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder material or the precursor thereof.

### Claim 2 (depends on 1)

The method of claim 1, wherein the curing occurs only after the slurry is shaped.

### Claim 3 (depends on 1, 2)

The method of any one of claims 1-2, wherein:
the solid inorganic binder material comprises at least one component selected from the group consisting of magnesium oxide, magnesium hydroxide, magnesium carbonate, magnesium carbonate hydrate, calcium oxide, calcium hydroxide, calcium carbonate, mono-calcium silicate, di-calcium silicate, tri-calcium silicate, calcium aluminate, calcium aluminosilicate, and a rare earth oxide, wherein the at least one component is combined with one or more of clay, colloidal silica, and one or more elements selected from the group consisting of magnesium, aluminum, iron, zinc, zirconium, titanium, vanadium, yttrium, lithium, sodium, potassium, bismuth, cerium, strontium, calcium, barium, lanthanum, copper, and boron, wherein the one or more elements are in a form of oxide, hydroxide and/or hydrous oxide;
the slurry further comprises H3PO4 and a refractory sand;
the shaping the slurry comprises packing the slurry against the pattern; and allowing the binder material or the precursor thereof to harden.

### Claim 4 (depends on 1, 2, 3)

The method of any one of claims 1-3, wherein the curing comprises infiltrating the shaped slurry with a steam at a temperature ranging from about 100° C. to about 350° C., for a time period ranging from about 1 minute to about 60 minutes.

### Claim 5 (depends on 1, 2, 3)

The method of any one of claims 1-3, wherein:
the solid inorganic binder material comprises at least one component selected from the group consisting of magnesium oxide, magnesium hydroxide, calcium oxide, calcium hydroxide, mono-calcium silicate, di-calcium silicate, tri-calcium silicate, calcium aluminate, calcium aluminosilicate, and a rare earth oxide,
wherein the at least one component is combined with one or more of clay, colloidal silica, and one or more elements selected from the group consisting of magnesium, aluminum, iron, zinc, zirconium, titanium, vanadium, yttrium, lithium, sodium, potassium, bismuth, cerium, strontium, calcium, barium, lanthanum, copper, and boron, wherein the one or more elements are in a form of oxide, hydroxide and/or hydrous oxide;
the shaping the slurry comprises packing the slurry against the pattern; and
the curing comprises infiltrating the shaped slurry with CO2 at a temperature ranging
from about 15° C. to about 350° C. and at a pressure ranging from about 0.5 psig to about 5000 psig.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The method of any one of claims 1-5, wherein the solid inorganic binder material comprises calcium monosilicate of 95 wt % purity or greater prior to being added to the binder material.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

The method of any one of claims 1-6, wherein the solid inorganic binder comprises calcium mono-silicate of a purity ranging from 25-95 wt % purity prior to being added to the binder material, where impurities are kiln-derived calcium silicate cement.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The method of any one of claims 1-7, wherein the solid inorganic binder comprises calcium monosilicate of 25-100 wt % purity prior to being added to the binder material.

### Claim 9 (depends on 4, 5, 6, 7, 8)

The method of any one of claims 4-8, wherein the solid inorganic binder material comprises the mono-calcium silicate, and the infiltrating the shaped slurry with CO2 at least partially converts the mono-calcium silicate to a calcium carbonate and silica in a sand mold foundry casting element.

### Claim 10 (depends on 4, 5, 6, 7, 8, 9)

The method of any one of claims 4-9, wherein:
the solid inorganic binder material comprises the magnesium oxide;
the infiltrating the shaped slurry with CO2 partially converts the magnesium oxide to magnesium carbonate to form a refractory element for bricks, castable, gunning mix or ramming mixes wherein resulting refractory product comprises MgO particles bonded to each other by magnesium carbonate particles, wherein the MgO particles are larger than the magnesium carbonate particles.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The method of any one of claims 1-10, wherein the slurry further comprises a thermoreversible additive comprising a carrageenan gum, potassium chloride, calcium chloride, agarose, hydroxymethyl cellulose, or any combination thereof.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

The method of any one of claims 1-11, wherein:
the shaping the slurry comprises:
heating the slurry to a temperature ranging from about 4° C. to about 350° C.;
dipping the pattern into the slurry to form a coating on the pattern; and
gelating the coating by allowing the coating to cool to a temperature below about 40° C.

### Claim 13 (depends on 12)

The method of claim 12, wherein the shaping the slurry further comprises repeating the dipping and the gelating at least one time to form the shaped slurry, and further comprising melting the pattern to form an investment casting mold.

### Claim 14 (depends on 12, 13)

The method of any one of claims 12-13, wherein the solid inorganic binder material comprises at least one component selected from the group consisting of magnesium oxide, magnesium hydroxide, calcium oxide, calcium hydroxide, mono-calcium silicate, di-calcium silicate, tri-calcium silicate, calcium aluminate, calcium aluminosilicate, and a rare earth oxide, wherein the at least one component is combined with one or more of clay, colloidal silica, and one or more elements selected from the group consisting of magnesium, aluminum, iron, zinc, zirconium, titanium, vanadium, yttrium, lithium, sodium, potassium, bismuth, cerium, strontium, calcium, barium, lanthanum, copper, and boron, wherein the one or more elements are in a form of oxide, hydroxide and/or hydrous oxide;
wherein the shaping the slurry comprises packing the slurry against the pattern; and
the curing comprises infiltrating the shaped slurry with CO2 at a temperature ranging from about 15° C. to about 350° C. and at a pressure ranging from about 0.5 psig to about 5000 psig; and
wherein the slurry further comprises a refractory sand.

### Claim 15 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14)

The method of any one of claims 1-14, wherein:
the binder precursor comprises at least one of ZrO2 and TiO2;
the slurry further comprises a refractory stand; and
the curing comprises infiltrating the casting element with an aqueous solution comprising
KOH and at least one of calcium, strontium or barium precursors.

### Claim 16 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15)

The method of any one of claims 1-15, wherein:
the binder precursor comprises at least one of zirconia and titania;
the slurry further comprises a refractory sand; and
the curing comprises infiltrating the casting element with an aqueous solution comprising
a hydroxide at least one of calcium, strontium, barium and precursors thereof.

### Claim 17 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16)

The method of any one of claims 1-16, wherein the binder precursor comprises at least one of the chemical formula, ABO3 wherein A is magnesium, calcium, strontium or barium, B is titanium or zirconium, ABO3 is a form of line compound, solid solution or multiphase mixture ABO3 compounds;
wherein the method comprises infiltrating the shaped slurry with CO2 and at least partially converts the ABO3 to a A-site metal carbonate and B-site metal dioxide.

### Claim 18 (depends on 16)

The method of claim 16, wherein the curing comprises infiltrating the casting element with an aqueous solution at a temperature ranging from about 150° C. to about 350° C., at a pressure ranging from about 0.5 psig to about 3000 psig, for a time period ranging from about 5 minutes to about 48 hours.

### Claim 19 (depends on 17)

The method of claim 17, wherein the curing comprises infiltrating the casting element with the aqueous solution at a temperature ranging from about 15° C. to about 350° C., at a pressure ranging from about 0.5 psig to about 3000 psig, for a time period ranging from about 5 minutes to about 48 hours.

### Claim 20 (depends on 1)

The method of claim 1, wherein the solid inorganic binder material comprises at least one of MgO and Fe2O3; wherein the slurry further comprises a refractory sand, at least one of aluminum trihydroxide and aluminum hydrous oxide, and phosphoric acid; and
the shaping the slurry comprises packing the slurry against the pattern.

### Claim 21 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15)

The method of any one of claims 1-15, wherein the curing comprises holding the shaped slurry in the pattern for a time period ranging from about 30 seconds to about 48 hours.

### Claim 22 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21)

The method of any one of claims 1-21, wherein the slurry further comprises a silica sand, an olivine sand, a chromate sand, a zircon sand, a chamotte sand, aluminosilicate sand, or any combinations thereof.

### Claim 23 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22)

The method of any one of claims 1-22, further comprising applying a molten metal to the casting element, wherein the casting element comprises a sand casting mold, a sand casting mold core, an investment casting shell, a refractory mix, wherein the refractory is a brick, castable, gunning or ramming mix.

### Claim 24

A method of forming a foundry casting element, the method comprising:
forming an aqueous first slurry comprising a refractory sand, colloidal silica and a binding polymer;
forming an aqueous second slurry comprising a solid inorganic binder material and a thermoreversible additive;
applying the first slurry to a pattern to form a first coating;
heating the second slurry to a temperature ranging from about 40° C. to about 250° C.; dipping the pattern into the heated second slurry to form a second coating on the first coating;
gelating the second coating by allowing the second coating to cool to a temperature below about 40° C.; and
infiltrating the second coatings with CO2 to cure the coating to form a casting element with 2-coating layers;
wherein the first slurry and/or second slurry optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder material or the binding polymer.

### Claim 25 (depends on 24)

The method of claim 24, wherein the dipping and the gelating are performed at least twice to form a three-layer structure.

### Claim 26 (depends on 24, 25)

The method of any one of claims 24-25, wherein the refractory sand comprises a zircon sand;
wherein the method further comprises applying additional zircon sand to the first coating; and the solid inorganic binder material comprises at least one component selected from the group consisting of magnesium oxide, magnesium hydroxide, calcium oxide, calcium hydroxide, mono-calcium silicate, di-calcium silicate, tri-calcium silicate, calcium aluminate, calcium aluminosilicate, and a rare earth oxide.

### Claim 27

A foundry casting element, comprising:
a refractory sand; and
a binder comprising an aqueous magnesium aluminum phosphate gel admixed with one or more of clay, fumed silica and a soluble precursor of zinc or a rare earth lanthanide ion; and
optionally an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the binder.

### Claim 28 (depends on 27)

The casting element of claim 27, wherein the refractory sand comprises a silica sand, an olivine sand, a chromate sand, a zircon sand, a chamotte sand, aluminosilicate sand, or any combinations thereof, and wherein the casting element comprises a sand casting mold, a sand casting mold core, an investment casting shell, or a refractory mix, wherein the refractory mix is a brick, castable, gunning or ramming mix.

### Claim 29

A refractory brick, castable, gunning or ramming mix, comprising MgO particles bonded to each other by magnesium carbonate particles, wherein the MgO particles are larger than the magnesium carbonate particles; and
optionally an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the MgO particles and the magnesium carbonate particles.

### Claim 30 (depends on 29)

The refractory brick of claim 29, wherein the refractory brick consists essentially of larger MgO particles bonded to each other by smaller magnesium carbonate particles, and the refractory brick excludes organic material.

### Claim 31 (depends on 29)

A molten metal holding ladle or blast furnace having an inner surface lined with the refractory bricks of claim 29.

### Claim 32

A method of forming a foundry casting element, the method comprising:
forming an aqueous slurry comprising a solid inorganic oxide material;
and infiltrating the slurry with CO2 to at least partially convert the solid inorganic oxide material to a solid inorganic carbonate material and to form the foundry casting element or refractory element for bricks, castable, gunning, or ramming mixes;
wherein the foundry casting element optionally comprises an inert component selected from the group consisting of oxide sands, diamond, graphite, carbon black, graphene, graphene oxide, metal carbides, silicon carbide, boron carbide, tungsten carbide, niobium carbide, titanium boride, zirconium boride, zirconia, titania, alumina, olivine, diopside, garnet, spinel, quartz, cristobalite, tridymite, calcium carbonate and dolomite, wherein the inert component does not react with the inorganic oxide material.

### Claim 33 (depends on 32)

The method of claim 32, wherein the solid inorganic oxide material comprises CaSiO3, and the infiltrating the slurry with CO2 at least partially converts the CaSiO3 to a calcium carbonate in a sand mold foundry casting element.

### Claim 34 (depends on 32)

The method of claim 32, wherein:
the solid inorganic oxide material comprises MgO;
the infiltrating the shaped slurry with CO2 partially converts the MgO to magnesium carbonate to form a refractory element for bricks, castable, gunning or ramming mixes;
wherein the refractory brick comprises MgO particles bonded to each other by magnesium carbonate particles, wherein the MgO particles are larger than the magnesium carbonate particles.

### Claim 35 (depends on 32, 33, 34)

The method of any one of claims 32-34, wherein the slurry comprises the inert component and the resulting casting element is admixed with the inert component.