# US 2023/0026102 A1 · Preparation method of self-crimping elastic combined filament yarn for knitting

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0026102 A1
- Document ID: US20230026102A1
- Status: Published application
- Kind: A1
- Application number: 17/787,951
- Filed: 2020-06-10
- Published: 2023-01-26
- Earliest claimed: 2019-12-24
- Assignees: Jiangsu Hengli Chemical Fibre Co., Ltd.
- Applicants: Jiangsu Hengli Chemical Fibre Co., Ltd.
- Inventors: Hongwei FAN; Fangming TANG; Shanshui WANG; Lixin YIN; Lili WANG
- Web page: https://patentgrep.com/patent/US20230026102A1

## CPC

- D01D 5/32: Side-by-side structure; Spinnerette packs therefor
- D01D 5/08: Melt spinning methods {(D01D5/0023 takes precedence)}
- D01D 5/082: {of mixed yarn}
- D01D 5/22: with a crimped or curled structure; with a special structure to simulate wool (producing crimped or curled effects in filaments or threads after formation D02G1/00)
- D01D 10/02: Heat treatment (heating for finishing D02J13/00)
- D01F 8/12: with at least one polyamide as constituent
- D01F 8/14: with at least one polyester as constituent
- D02G 1/004: {by heating fibres, filaments, yarns or threads so as to create a temperature gradient across their diameter, thereby imparting them latent asymmetrical shrinkage properties}
- D02G 1/205: {After-treatments for fixing crimp or curl}
- D02G 3/326: {the elastic properties due to the construction rather than to the use of elastic material}
- D02J 1/229: {Relaxing (in combination with crimping D02G1/20)}
- D10B 2331/02: polyamides (D10B2331/08 takes precedence)
- D10B 2331/04: polyesters, e.g. polyethylene terephthalate [PET]
- D10B 2401/061: elastic
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D02G: CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, OR YARNS; YARNS OR THREADS
- D02J: FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS, ROPES OR THE LIKE (curling or crimping D02G; by treatment with liquids, gases or vapours D06B; finishing other than by liquid treatment, of yarns in warp or sheet form D06C; for chemical matters, see D06L, D06M, D06P, D06Q; treatment during rope-making, apparatus for treating ropes auxiliary to rope-making D07B)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

A preparation method of self-crimping elastic combined filament yarns for knitting is disclosed, wherein the combined filament yarns are extruded from the same spinneret; a first fiber-forming polymer melt is divided into two ways, one is directly extruded after distribution; and the other is extruded after distribution by side-by-side composite spinning together with a second fiber-forming polymer melt; the first fiber-forming polymer and the second fiber-forming polymer are compatible or partially compatible; on the same spinneret, a ratio of the number of spinneret holes m for direct extrusion to the number of spinneret holes n for extrusion after distribution by side-by-side composite spinning is 1:(5-10); the self-crimping elastic combined filament yarns for knitting are prepared according to specific spinning processes, wherein the combined filament yarn mainly comprises a first fiber-forming polymer monofilament and a first/second fiber-forming polymer side-by-side composite monofilament; wherein the monofilament crimping directions are randomly distributed.

## Claims

### Claim 1

A method for preparing a self-crimping elastic combined filament yarn for knitting, comprising: extruding the self-crimping elastic combined filament yarn for knitting from a same spinneret;
wherein a first fiber-forming polymer melt is divided into two ways: one is directly extruded after distribution; and the other is extruded after distribution by side-by-side composite spinning together with a second fiber-forming polymer melt;
wherein the first fiber-forming polymer melt and the second fiber-forming polymer melt are compatible or partially compatible;
on the same spinneret, wherein a ratio of a number of spinneret holes for direct extrusion to a number of spinneret holes for extrusion after the distribution by side-by-side composite spinning is 1:(5-10); wherein all the spinneret holes are distributed in concentric circles, and the spinneret holes on a same circle are all the spinneret holes for the direct extrusion or all the spinneret holes for the extrusion after the distribution by side-by-side composite spinning, while the spinneret holes on an outermost circle are all the spinneret holes for the extrusion after the distribution by side-by-side composite spinning;
wherein each of the spinneret holes for the direct extrusion comprises a first guide hole, a first transition hole and a first capillary micropore connected sequentially, each of the spinneret holes for the extrusion after the distribution by side-by-side composite spinning comprises a second guide hole, a second transition hole and a second capillary micropore connected sequentially, the first guide hole is connected with a first distribution hole, and the second guide hole is connected with a second distribution hole and a third distribution hole at the same time; wherein the first distribution hole, the second distribution hole and the third distribution hole are located on a distribution plate in a third spinning box; wherein a division is to transport the first fiber-forming polymer melt through a first spinning box to the first distribution hole and the second distribution hole, while transport the second fiber-forming polymer melt through a second spinning box to the third distribution hole;
after the extrusion, wherein the self-crimping elastic combined filament yarn for knitting is prepared according to specific spinning processes: a POY process, an FDY process, a POY-DTY process or a POY-DT process, wherein the POY process, the FDY process and the POY-DT process are followed by a relaxation heat treatment of a fiber, and monofilament crimping directions are randomly distributed after the relaxation heat treatment; wherein the relaxation heat treatment has a temperature of 90-120° C. and a time of 20-30 min.

### Claim 2 (depends on 1)

The method of claim 1, wherein a ratio of a mass of the first fiber-forming polymer melt extruded from the spinneret holes for the extrusion after the distribution by side-by-side composite spinning to a mass of the second fiber-forming polymer melt extruded from the spinneret holes for the extrusion after the distribution by side-by-side composite spinning is 50:50, and a ratio of an equivalent diameter of the spinneret holes for the direct extrusion to an equivalent diameter of the spinneret holes for the extrusion after the distribution by side-by-side composite spinning is 1:1; wherein the first fiber-forming polymer melt and the second fiber-forming polymer melt are of same materials with different viscosities, or of different materials; wherein the materials of the first fiber-forming polymer melt and the second fiber-forming polymer melt are selected from polyester or polyamide, wherein the polyester is PET, PBT, or PTT, and the polyamide is PA6.

### Claim 3 (depends on 1)

The method of claim 1, wherein each of the spinneret holes for the direct extrusion is a circular, oval, triangular, Y-shaped, cross-shaped, “8”-shaped, rectangular or in-line spinneret hole, and each of the spinneret holes for the extrusion after the distribution by side-by-side composite spinning is a circular, oval or “8”-shaped spinneret hole.

### Claim 4

(canceled)

### Claim 5

(canceled)

### Claim 6 (depends on 1)

The method of claim 1, wherein an apparent viscosity of the first fiber-forming polymer melt differs from an apparent viscosity of the second fiber-forming polymer melt by no more than 5% in the spinning components.

### Claim 7

(canceled)