# US 2023/0025008 A1 · A method for controlling the size of lithium peroxide and a method for preparing lithium oxide with controlled size

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0025008 A1
- Document ID: US20230025008A1
- Status: Published application
- Kind: A1
- Application number: 17/787,010
- Filed: 2020-12-07
- Published: 2023-01-26
- Earliest claimed: 2019-12-20
- Assignees: Posco; Research Institute of Industrial Science & Technology
- Applicants: Posco; Research Institute of Industrial Science & Technology
- Inventors: Jae Myung LEE; Jun-Kyu AHN; Woo Chul JUNG; Kee Uek JEUNG; Jung Kwan PARK; Sang Won KIM
- Web page: https://patentgrep.com/patent/US20230025008A1

## CPC

- C01D 15/02: Oxides; Hydroxides
- C01B 15/0435: {of alkali metals}
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/03: obtained by SEM
- C01P 2004/32: Spheres
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a novel method for preparing lithium oxide. In the present invention, the particle size and shape of lithium oxide may be controlled during the preparing process. In addition, the present invention relates to lithium oxide with controlled particle size and shape prepared by this preparing method.

## Claims

### Claim 1

A method of controlling a particle size of lithium peroxide,
wherein the lithium peroxide is produced by reacting lithium hydroxide hydrate with hydrogen peroxide in a reactor to prepare lithium peroxide,
a shape of the lithium peroxide is spherical,
the particle size is determined by adjusting a tip velocity of a stirrer in the reactor, and
the tip velocity is calculated by the equation:
V_tip=2pi×R_impellor*(RPM)/60
wherein, in the above equation, V-tip is a tip velocity, Pi is a circumference, R-impellor is a radius of the stirrer blade, and RPM is the number of revolutions per minute of the stirrer blade.

### Claim 2 (depends on 1)

The method of claim 1, wherein the particle size of the prepared lithium peroxide is in the range of 1 μm to 130 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein an equivalent ratio of lithium hydroxide hydrate to hydrogen peroxide is 4:1 to 1:1.

### Claim 4 (depends on 1)

The method of claim 1, wherein a reaction temperature is in the range of 30° C. to 60° C. and a reaction time is 1 minute or more, or 30 minutes to 90 minutes.

### Claim 5

A method of preparing a lithium peroxide having a controlled particle size, comprising
(1) reacting lithium hydroxide hydrate with hydrogen peroxide to prepare lithium peroxide; and
(2) decomposing the lithium peroxide at a high temperature under an inert atmosphere to prepare lithium oxide,
wherein in the (1) process, the particle size of lithium peroxide is determined by adjusting a tip velocity of a stirrer in a reactor, and
the tip velocity is calculated by the following equation:
V_tip=2pi×R_impellor*(RPM)/60
wherein, in the above equation, V-tip is a tip velocity, Pi is a circumference, R-impellor is a radius of the stirrer blade, and RPM is the number of revolutions per minute of the stirrer blade.

### Claim 6 (depends on 5)

The method of claim 5, wherein
a particle size of lithium oxide prepared in the (2) process is determined by the following equation:
(lithium oxide particle size)=a×exp(b×V-tip), wherein a and b are process constants
wherein, in the above equation, a and b are engineering constant values, 20<a<60, and −0.3<b<−0.1.

### Claim 7 (depends on 5)

The method of claim 5, wherein the particle size of lithium oxide prepared in the (2) process is 50 to 80%, or 60 to 70% of the particle size of lithium peroxide prepared in the (1) process.

### Claim 8 (depends on 5)

The method of claim 5, wherein the particle size of lithium oxide produced in the (2) process is 60 to 70% of the particle size of lithium peroxide produced in the (1) process.

### Claim 9 (depends on 5)

The method of claim 5, wherein in the (1) process, the tip velocity of the stirrer in the reactor is in the range of 0.2 m/sec. to 20 m/sec.

### Claim 10 (depends on 5)

The method of claim 5, wherein the particle size of lithium oxide is in the range of 1 μm to 100 μm.

### Claim 11 (depends on 5)

The method of claim 5, wherein the faster the tip velocity, the smaller the size of the produced particles.

### Claim 12 (depends on 5)

The method of claim 5, wherein in the (2) process, a reaction temperature is greater than or equal to 300° C.

### Claim 13 (depends on 5)

The method of claim 5, wherein a reaction time of the (2) process is greater than or equal to 10 minutes, or 30 minutes to 3 hours.