# US 2023/0022624 A1 · Method for processing semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0022624 A1
- Document ID: US20230022624A1
- Status: Published application
- Kind: A1
- Application number: 17/453,837
- Filed: 2021-11-05
- Published: 2023-01-26
- Earliest claimed: 2021-07-20
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Ning XI
- Web page: https://patentgrep.com/patent/US20230022624A1

## CPC

- H10P 70/20: {Cleaning during device manufacture}
- B08B 3/00: Cleaning by methods involving the use or presence of liquid or steam (B08B9/00 takes precedence)
- B08B 5/02: Cleaning by the force of jets, e.g. blowing-out cavities {(airguns or nozzles per se B05B1/005)}
- H01J 37/3244: {Gas supply means}
- H01J 37/32522: {Temperature}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/283: {by chemical means}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H01J 2237/2001: Maintaining constant desired temperature
- H01J 2237/3355: Holes or apertures, i.e. inprinted circuit boards
- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/73: {using masks for insulating materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B08B: CLEANING IN GENERAL; PREVENTION OF FOULING IN GENERAL
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method for processing a semiconductor structure includes: a substrate is provided, which has feature parts, in which an aspect ratio of the feature parts is greater than a preset aspect ratio, a barrier layer is disposed on tops of the feature parts, a hydrophilic layer is disposed on side walls of the feature parts, and there are particulate impurities on a surface of the hydrophilic layer; at least one cleaning treatment to the substrate is performed, in which the cleaning treatment includes: initial water vapor is introduced to the side walls of the feature parts, and a cooling treatment is performed to liquefy the initial water vapor adhering to a surface of the hydrophilic layer into water which carries the particulate impurities and flows into grooves; and a heating treatment is performed to evaporate the water into water vapor which carries the particulate impurities and escapes.

## Claims

### Claim 1

A method for processing a semiconductor structure, comprising:
providing a substrate, which has feature parts, wherein an aspect ratio of the feature parts is greater than a preset aspect ratio, a barrier layer is disposed on tops of the feature parts, a hydrophilic layer is disposed on side walls of the feature parts, and there are particulate impurities on a surface of the hydrophilic layer;
performing at least one cleaning treatment to the substrate, wherein the cleaning treatment comprises:
introducing initial water vapor to the side walls of the feature parts, and performing a cooling treatment to liquefy the initial water vapor adhering to the surface of the hydrophilic layer into water; and
performing a heating treatment to evaporate the water into water vapor which carries the particulate impurities and escapes.

### Claim 2 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein a method for forming the hydrophilic layer comprises: performing a hydrophilic treatment on the side walls of the feature parts to form the hydrophilic layer.

### Claim 3 (depends on 2)

The method for processing a semiconductor structure of claim 2, further comprising: after forming the hydrophilic layer and before performing the cleaning treatment, removing the barrier layer, and introducing purge gas.

### Claim 4 (depends on 3)

The method for processing a semiconductor structure of claim 3, wherein removing the barrier layer and performing the hydrophilic treatment on the side walls of the feature parts are completed in a same process step.

### Claim 5 (depends on 4)

The method for processing a semiconductor structure of claim 4, wherein performing the hydrophilic treatment on the side walls of the feature parts comprises:
introducing the water vapor and carrier gas to the side walls of the feature parts; and
subjecting the water vapor to a treatment of forming plasma during introducing the water vapor.

### Claim 6 (depends on 5)

The method for processing a semiconductor structure of claim 5, wherein:
a gas flow rate of the introduced water vapor ranges from 10 sccm to 300 sccm; and
a flow rate of the introduced carrier gas ranges from 100 sccm to 5000 sccm.

### Claim 7 (depends on 5)

The method for processing a semiconductor structure of claim 5, wherein in a process of removing the barrier layer:
a pressure of a reaction environment ranges from 0 mTorr to 10000 mTorr;
a temperature of the substrate ranges from 20° C. to 100° C.; and
a temperature of the introduced water vapor ranges from 100° C. to 250° C.

### Claim 8 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein the preset aspect ratio is not less than 10.

### Claim 9 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein during the cleaning treatment:
a flow rate of the introduced initial water vapor ranges from 1000 sccm to 20000 sccm;
a temperature after the cooling treatment ranges from 20° C. to 60° C.;
a temperature after the heating treatment ranges from 60° C. to 100° C.;
a temperature change rate of the cooling treatment ranges from 0.5 s/° C. to 1.5 s/° C.; and
a temperature change rate of the heating treatment ranges from 0.5 s/° C. to 1.5 s/° C.

### Claim 10 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein,
performing at least one cleaning treatment to the substrate comprises: cyclically performing a preset number of times of the cleaning treatment;
wherein, the cleaning treatment further comprises: before introducing water vapor to the side walls of the feature part, removing a part of thickness of the barrier layer, and introducing purge gas; and
during performing a last cleaning treatment, removing a part of thickness of the barrier layer is: removing the barrier layer.

### Claim 11 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein the barrier layer is an amorphous carbon layer doped with boron atoms.

### Claim 12 (depends on 1)

The method for processing a semiconductor structure of claim 1, wherein a process for forming the feature parts comprises:
providing the substrate, and forming the barrier layer on a top surface of the substrate;
patterning the barrier layer and part of thickness of the substrate to form grooves, wherein the remaining substrate between adjacent grooves constitutes the feature parts; and
performing a hydrophilic treatment on surfaces of the grooves to form the hydrophilic layer.

### Claim 13 (depends on 12)

The method for processing a semiconductor structure of claim 12, wherein patterning the barrier layer and part of thickness of the substrate to form the grooves comprises:
forming a patterned mask layer on a top surface of the barrier layer;
patterning the barrier layer based on the patterned mask layer until the surface of the substrate is exposed;
patterning part of thickness of the substrate to form the grooves based on the patterned mask layer; and
removing the patterned mask layer.

### Claim 14 (depends on 1)

The method for processing a semiconductor structure of claim 1, further comprising: after the cleaning treatment, removing the hydrophilic layer, which comprises:
introducing NH3 and HF, and performing a first temperature treatment; and
introducing N2, and performing a second temperature treatment.

### Claim 15 (depends on 14)

The method for processing a semiconductor structure of claim 14, wherein the temperature after the first temperature treatment ranges from 20° C. to 40° C., and the temperature after the second temperature treatment ranges from 100° C. to 200° C.