Method for the activation or rejuvenation of a catalyst
AssigneeEmerging Fuels Technology, Inc.
InventorKenneth L. Agee
Life of this patent
Estimating the term…
Abstract
A method is disclosed for rejuvenation a cobalt Fischer Tropsch catalyst used in a Fischer Tropsch process operating in recycle mode. The method permits the use of specific inert gases to adjust the mole weight of the gas so that the recycle compressor designed for normal steady state operation can also be used in the method. Hydrogen from a membrane permeate stream is added to the reactor loop at a temperature between 300 F and 400 F and the carbon oxides are reacted out to purify the hydrogen. This stream is continuously recycled and the temperature is raised to between 425 F and 500 F and held at the final temperature for between 4 hours and 48 hours. The cobalt Fischer Tropsch catalyst is effectively rejuvenated in-situ by the method.
Claims14
A method to activate or rejuvenate a cobalt Fischer Tropsch catalyst used in a Fischer Tropsch process, the method comprising:
- A) purging a Fischer Tropsch reactor loop with a feed gas, argon, or a mixture thereof;
- B) adding permeate hydrogen from a hydrogen membrane to the Fischer Tropsch reactor loop to between 10% and 80% while recycling the loop with little or no purge, at a temperature below 300 F in the Fischer Tropsch reactor;
- C) raising the temperature in the Fischer Tropsch reactor to between 300 F and 400 F to hydrogenate carbon oxides from the permeate hydrogen, thus making methane and other heavier hydrocarbons, resulting in a circulating gas comprising hydrogen and relatively inert hydrocarbon gases or argon, that is substantially depleted of carbon oxides;
- and
- D) raising the temperature of the Fischer Tropsch reactor to between 425 F and 500 F and holding for between 4 hours and 48 hours while recycling the hydrogen-containing gas with little or no purge.
Dependencies are inferred from the claim text.