# US 2023/0012857 A1 · Operation method of ladle refining treatment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0012857 A1
- Document ID: US20230012857A1
- Status: Published application
- Kind: A1
- Application number: 17/756,478
- Filed: 2020-10-21
- Published: 2023-01-19
- Earliest claimed: 2019-11-29
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Kazuaki HIRAKAWA; Koichiro HIRATA; Isao SHIMODA; Takashi YAMAUCHI; Hirohide UEHARA
- Web page: https://patentgrep.com/patent/US20230012857A1

## CPC

- B22D 1/002: {Treatment with gases (C21C7/072, C22B9/05 take precedence)}
- B22D 2/006: {for the temperature of the molten metal (measuring temperature in general G01K)}
- B22D 1/00: Treatment of fused masses in the ladle or the supply runners before casting {(for continuous casting B22D11/10; metallurgical processing, e.g. refining of iron or other metal C21, C22, C25C)}
- B22D 11/113: by vacuum treating
- B22D 11/117: by treating with gases (B22D11/118, B22D11/119 take precedence)
- C21C 5/4673: {Measuring and sampling devices}
- C21C 7/00: Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/00 - C21C5/00 (treating molten metals during moulding B22D1/00, B22D27/00)
- C21C 7/0075: {Treating in a ladle furnace, e.g. up-/reheating of molten steel within the ladle}
- C21C 7/10: Handling in a vacuum
- F27B 3/28: Arrangement of controlling, monitoring, alarm or the like devices
- F27D 19/00: Arrangements of controlling devices
- G01K 1/105: {for siderurgical use}
- G01K 1/125: {for siderurgical use}
- G01K 13/026: {of moving liquids}
- C21C 2005/5288: {Measuring or sampling devices}
- C21C 2300/06: Modeling of the process, e.g. for control purposes; CII
- F27D 2019/0003: {Monitoring the temperature or a characteristic of the charge and using it as a controlling value}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- G01K: MEASURING TEMPERATURE; MEASURING QUANTITY OF HEAT; THERMALLY-SENSITIVE ELEMENTS NOT OTHERWISE PROVIDED FOR (radiation pyrometry G01J5/00)

## Abstract

Provided is a method of, in ladle refining treatment of a molten steel, accurately estimating the molten steel temperature after the ladle refining treatment. An operation method of ladle refining treatment by which ladle refining treatment of a molten steel is performed while continuously measuring a molten steel temperature during operation of the ladle refining treatment of the molten steel comprises setting a time earlier than a scheduled ending time of the ladle refining treatment in a continuous measurement period of the molten steel temperature as a determination timing, and estimating the molten steel temperature at the scheduled ending time on the basis of a change with time of the molten steel temperature in continuous measured data of the molten steel temperature from a start of continuous measurement of the molten steel temperature to the determination timing.

## Claims

### Claim 1

An operation method of ladle refining treatment by which ladle refining treatment of a molten steel is performed while continuously measuring a molten steel temperature during operation of the ladle refining treatment of the molten steel, the operation method comprising
setting a time earlier than a scheduled ending time of the ladle refining treatment in a continuous measurement period of the molten steel temperature as a determination timing, and estimating the molten steel temperature at the scheduled ending time on the basis of a change with time of the molten steel temperature in continuous measured data of the molten steel temperature from a start of continuous measurement of the molten steel temperature to the determination timing.

### Claim 2 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein the continuous measured data of the molten steel temperature is of measured values corrected depending on an immersion depth of a temperature sensor for continuous temperature measurement.

### Claim 3 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein in a case where an estimated value of the molten steel temperature is within a target range of the molten steel temperature at the scheduled ending time, operation conditions at the determination timing are maintained until the scheduled ending time,
wherein in a case where an estimated value of the molten steel temperature is higher than a target range of the molten steel temperature at the scheduled ending time, an operation of decreasing the molten steel temperature is performed in a period from the determination timing to the scheduled ending time, or
wherein in a case where an estimated value of the molten steel temperature is lower than a target range of the molten steel temperature at the scheduled ending time, an operation of increasing the molten steel temperature is performed in a period from the determination timing to the scheduled ending time.

### Claim at position 4

4-5. (canceled)

### Claim 6 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein the determination timing is 3 minutes to 8 minutes before the scheduled ending time.

### Claim 7 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein an estimated value Tf of the molten steel temperature is calculated according to the following Formula (1):
Tf=BMAtd+(BMAtd−BMAtdα)/α×tr (1)
where Tf is the estimated value in ° C. of the molten steel temperature at the scheduled ending time, BMAtd is a backward moving average value in ° C. of a continuous temperature measured value at time td, BMAtd−α is a backward moving average value in ° C. of a continuous temperature measured value at time (td−α), td is an operation time in minutes from the start of the continuous measurement of the molten steel temperature to the determination timing, td−α is an operation time in minutes from the start of the continuous measurement of the molten steel temperature to α minutes before td, and tr is a time in minutes from obtainment of the estimated value of the molten steel temperature at the scheduled ending time to the scheduled ending time.

### Claim 8 (depends on 7)

The operation method of ladle refining treatment according to claim 7, wherein α is 0.5 minutes to 2.0 minutes.

### Claim 9 (depends on 7)

The operation method of ladle refining treatment according to claim 7, wherein a range of backward moving average is determined on the basis of a variation cycle of a continuous measured value of the molten steel temperature measured beforehand.

### Claim 10 (depends on 2)

The operation method of ladle refining treatment according to claim 2, wherein the immersion depth of the temperature sensor for continuous temperature measurement is increased with an increase of the number of uses of a measuring element of the temperature sensor for continuous temperature measurement.

### Claim 11 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein the molten steel temperature at the scheduled ending time is estimated on the basis of the change with time of the molten steel temperature in the continuous measured data of the molten steel temperature during killing treatment from after end of at least one of alloying addition and oxygen supply to the determination timing in the continuous measurement period of the molten steel temperature.

### Claim 12 (depends on 1)

The operation method of ladle refining treatment according to claim 1, wherein the ladle refining treatment is RH degassing treatment.