# US 2023/0011769 A1 · Ni-BASED ALLOY, HEAT-RESISTANT AND CORROSION-RESISTANT COMPONENT, AND HEAT TREATMENT FURNACE COMPONENT

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0011769 A1
- Document ID: US20230011769A1
- Status: Published application
- Kind: A1
- Application number: 17/783,495
- Filed: 2020-12-23
- Published: 2023-01-12
- Earliest claimed: 2019-12-27
- Assignees: Kubota Corporation
- Applicants: Kubota Corporation
- Inventors: Ayano KAMITSUJI; Soichi ASANO; Yohei ENJO; Kunihide HASHIMOTO
- Web page: https://patentgrep.com/patent/US20230011769A1

## CPC

- C22C 19/03: based on nickel
- C22C 19/007: {with a light metal (alkali metal Li, Na, K, Rb, Cs; earth alkali metal Be, Mg, Ca, Sr, Ba, Al Ga, Ge, Ti) or B, Si, Zr, Hf, Sc, Y, lanthanides, actinides, as the next major constituent}
- C22C 19/05: with chromium
- C22C 19/057: {with the maximum Cr content being less 10%}
- C22F 1/10: of nickel or cobalt or alloys based thereon
- F27B 5/08: Arrangements of linings
- F27D 1/0006: {Linings or walls formed from bricks or layers with a particular composition or specific characteristics}
- F27B 5/10: Muffles
- Y02E 60/10: Energy storage using batteries
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a Ni-based alloy, a heat-resistant and corrosion-resistant component, and a heat treatment furnace component, all of which have excellent corrosion resistance and mechanical strength at high temperatures. The Ni-based alloy of the present invention consists of, by mass %, Al: more than 5.0% and up to 26.0%, and Zr: more than 0% and up to 5.0%, the balance being Ni and unavoidable impurities. The Ni-based alloy preferably contains more than 0% and up to 5.0% of B, by mass %, in a combined amount with Zr. Moreover, it is preferable that the Ni-based alloy has P value and Q value and satisfies a relationship of Q value ≥ 0.89 × P value - 0.53, when the P value is obtained from a formula -18.95 + 0.1956 × Ni% + 0.1977 × Al% + 0.2886 × Zr% + 12.4 × B%, and the Q value is obtained by dividing an area percentage of Ni3Al precipitated on the surface of the alloy by 100.

## Claims

### Claim 1

-14. (canceled)

### Claim 15

A Ni-based alloy consisting of, by mass %:
Al: more than 5.0% and up to 26.0%, and
Zr: more than 0% and up to 5.0%,
the balance being Ni and unavoidable impurities.

### Claim 16 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy contains more than 0% and up to 5.0% of B, by mass %, in a combined amount with Zr.

### Claim 17 (depends on 16)

The Ni-based alloy according to claim 16, wherein the alloy contains at least 0.001% of B, by mass %.

### Claim 18 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy has Ni3Al precipitated on a surface thereof.

### Claim 19 (depends on 18)

The Ni-based alloy according to claim 18, wherein the alloy has P value and Q value, and satisfies a relationship of Q value ≥ 0.89 xP value - 0.53, when the P value is obtained from a formula -18.95 + 0.1956 × Ni% + 0.1977 ×Al% + 0.2886 × Zr% + 12.4 × B%, and the Q value is obtained by dividing an area percentage of Ni3Al precipitated on the surface of the alloy by 100.

### Claim 20 (depends on 18)

The Ni-based alloy according to claim 18, wherein the alloy has P value and Q value, and satisfies a relationship of Q value ≥ 1.75 × P value - 1.1, when the P value is obtained from a formula 5.91 - 0.0512 × Ni% - 0.0612 × Al%, and the Q value is obtained by dividing an area percentage of Ni3Al precipitated on the surface of the alloy by 100.

### Claim 21 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy contains at least 8.0% of Al, by mass %.

### Claim 22 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy further contains 0.001% to 4.0% of Y, by mass %.

### Claim 23 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy further contains 0.001% to 4.0% of Ta, by mass %.

### Claim 24 (depends on 15)

The Ni-based alloy according to claim 15, wherein the alloy further contains 0.001% to 5.0% of W, by mass %.

### Claim 25 (depends on 15)

A heat-resistant and corrosion-resistant component made of the Ni-based alloy according to claim 15.

### Claim 26 (depends on 15)

A heat treatment furnace component made of the Ni-based alloy according to claim 15.

### Claim 27 (depends on 26)

The heat treatment furnace component according to claim 26, wherein
the heat treatment furnace component is a retort used for firing a cathode material, and has an inner surface to come into contact with the cathode material and an outer surface to be heated by heating means; and
the outer surface has a hardness higher than the inner surface.

### Claim 28

A heat treatment furnace component made of a Ni-based alloy consisting of, by mass %,
Al: more than 5.0% and up to 26.0%, the balance being Ni and unavoidable impurities.