# US 2022/0411899 A1 · Bearing formed of an aluminum alloy material and method of manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0411899 A1
- Document ID: US20220411899A1
- Status: Published application
- Kind: A1
- Application number: 17/358,858
- Filed: 2021-06-25
- Published: 2022-12-29
- Earliest claimed: 2021-06-25
- Assignees: Tenneco Inc.
- Applicants: Tenneco Inc.
- Inventors: David Michael Saxton; Andrew R. Zeagler; Terri Ann Giroux; Michael Wagner; Katherine Theresa Vaida
- Web page: https://patentgrep.com/patent/US20220411899A1

## CPC

- C22C 21/10: with zinc as the next major constituent
- B22D 11/003: {Aluminium alloys}
- C22C 18/02: with copper as the next major constituent
- C22C 30/06: containing zinc
- C22F 1/053: of alloys with zinc as the next major constituent
- F16C 33/121: {Use of special materials}
- F16C 33/14: Special methods of manufacture; Running-in
- F16C 2202/04: Hardness
- F16C 2204/20: Alloys based on aluminium
- F16C 2220/02: by casting
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS

## Abstract

A sliding element, such as a bearing, and a method of manufacturing the sliding element, is provided. The sliding element is formed of an aluminum alloy material which includes zinc in an amount of 5 wt. % to 83 wt. %. The sliding element may also include silicon and/or magnesium. The sliding element is typically formed by casting, heat treating at a temperature of 400° C. to 577° C., and cooling at a rate of less than 50° C. per hour to a temperature ranging from 400° C. to 200° C. The aluminum alloy material is then heat treated at a temperature of 100° to 275° C. for at least 5 hours to form a soft phase consisting essentially of the zinc. The second heat treatment, or possibly both heat treatments, may not be required when the aluminum alloy material includes the magnesium.

## Claims

### Claim 1

A sliding element, comprising:
an aluminum alloy material, the aluminum alloy material including aluminum in an amount of 17 weight percent (wt. %) to 95 wt. % and zinc in an amount of 5 wt. % to 83 wt. %, based on the total weight of the aluminum alloy material,
the aluminum alloy material including a soft phase consisting essentially of zinc, and the soft phase having a Vickers hardness of not greater than 60 HV0.01 kg.

### Claim 2 (depends on 1)

The sliding element of claim 1, wherein the aluminum alloy material includes the aluminum in an amount of at least 52.5 wt. %, the zinc in an amount of 10 wt. % to 40 wt. %, and lead, if present, in an amount of not greater than 0.1 wt. %, based on the total weight of the aluminum alloy material.

### Claim 3 (depends on 2)

The sliding element of claim 2 including the aluminum in an amount of at least 58.5 wt. % and the zinc in an amount of 20 wt. % to 40 wt. %, based on the total weight of the aluminum alloy material.

### Claim 4 (depends on 1)

The sliding element of claim 1 including silicon in an amount of 0.5 wt. % to 12 wt. %, based on the total weight of the aluminum alloy material.

### Claim 5 (depends on 4)

The sliding element of claim 4 including the silicon in an amount of 1 wt. % to 6 wt. %, based on the total weight of the aluminum alloy material.

### Claim 6 (depends on 1)

The sliding element of claim 1 including magnesium in an amount of 0.5 wt. % to 12 wt. %, based on the total weight of the aluminum alloy material.

### Claim 7 (depends on 6)

The sliding element of claim 6 including the magnesium in an amount of 1 wt. % to 6 wt. %, based on the total weight of the aluminum alloy material.

### Claim 8 (depends on 1)

The sliding element of claim 1 including silicon in an amount of 0.5 wt. % to 12 wt. % and magnesium in an amount of 0.5 wt. % to 12 wt. %, based on the total weight of the aluminum alloy material.

### Claim 9 (depends on 8)

The sliding element of claim 8 including a hard phase consisting essentially of magnesium and/or silicon.

### Claim 10 (depends on 1)

The sliding element of claim 1, wherein the aluminum alloy material has an ultimate tensile strength of 150-300 MPa, a yield strength of 100-300 MPa, and Vickers hardness of 50-150 HV0.01 kg.

### Claim 11

A method of manufacturing a sliding element, comprising the steps of:
casting an aluminum alloy material, the aluminum alloy material including zinc in an amount of at least 5 wt. %, based on the total weight of the material, and
heat treating the cast aluminum alloy material at a temperature of 100° to 275° C. for at least 5 hours to form a soft phase consisting essentially of the zinc.

### Claim 12 (depends on 11)

The method of claim 11 including heat treating the cast aluminum alloy material at a temperature of 400° C. to 577° C. and cooling the cast aluminum alloy material at cooling rate of less than 50° C. per hour to a temperature ranging from 400° C. to 200° C., before the step of heat treating the aluminum alloy material at the temperature of 100° C. to 275° C. for at least 5 hours.

### Claim 13 (depends on 12)

The method of claim 12, wherein the aluminum alloy material includes silicon and/or magnesium, and the silicon and/or magnesium forms a hard phase during the step of heat treating the cast aluminum alloy material to the temperature of 400° C. to 577° C.

### Claim 14 (depends on 13)

The method of claim 13 including the silicon in an amount of 0.5 wt. % to 12 wt. %, based on the total weight of the aluminum alloy material.

### Claim 15 (depends on 11)

The method of claim 11, wherein the zinc of the aluminum alloy material forms a soft phase during the step of heat treating the aluminum alloy material at the temperature of 100° C. to 275° C. for at least 5 hours.

### Claim 16 (depends on 11)

The method of claim 11, wherein the casting step is a continuous process and includes twin roll casting, belt casting, and/or extraction casting.

### Claim 17 (depends on 11)

The method of claim 11 including rolling the cast aluminum alloy material and bonding the rolled aluminum alloy material to a steel backing before the step of heat treating the aluminum alloy material at the temperature of 100° C. to 275° C. for at least 5 hours.

### Claim 18 (depends on 11)

The method of claim 11, wherein the aluminum alloy material includes the aluminum in an amount of 17 weight percent (wt. %) to 95 wt. %, the zinc in an amount of 5 wt. % to 83 wt. %, and lead, if present, in an amount not greater than 0.1 wt. %, based on the total weight of the aluminum alloy material.

### Claim 19 (depends on 11)

The method of claim 11 including the aluminum in an amount of at least 52.5 wt. % and the zinc in an amount of 20 wt. % to 40 wt. %, based on the total weight of the aluminum alloy material.

### Claim 20

A method of manufacturing a sliding element, comprising the step of:
casting an aluminum alloy material, the aluminum alloy material including zinc in an amount of at least 5 wt. % and magnesium in an amount of 0.5 wt. % to 12 wt. %, based on the total weight of the aluminum alloy material.