# US 2022/0411351 A1 · Method for the depolymerisation of polystyrene in the presence of foreign polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0411351 A1
- Document ID: US20220411351A1
- Status: Published application
- Kind: A1
- Application number: 17/641,842
- Filed: 2020-09-17
- Published: 2022-12-29
- Earliest claimed: 2019-09-18
- Assignees: Ineos Styrolution Group GmbH
- Applicants: Ineos Styrolution Group GmbH
- Inventors: Norbert NIESSNER; Bianca WILHELMUS; Achim SCHMIDT-RODENKIRCHEN; Konstantin MIERDEL; Frank NEUNER
- Web page: https://patentgrep.com/patent/US20220411351A1

## CPC

- C07C 4/22: by depolymerisation to the original monomer, e.g. dicyclopentadiene to cyclopentadiene
- B01J 8/24: according to "fluidised-bed" technique (B01J8/20 takes precedence)
- C08J 11/12: by dry-heat treatment only
- C07C 2527/224: Silicon carbide
- C07C 2601/16: the ring being unsaturated
- C08J 2325/06: Polystyrene
- C08J 2423/06: Polyethene
- C08J 2423/12: Polypropene
- C08J 2455/02: Acrylonitrile-Butadiene-Styrene [ABS] polymers
- C08J 2467/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08J2467/06 takes precedence)
- Y02W 30/62: Plastics recycling; Rubber recycling
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The invention relates to a method for producing styrene monomers by the depolymerisation of polystyrene in the presence of foreign polymers, such as polyolefins. Said method comprises the following steps: a) introducing a polymer composition (A) containing: I) 10 to 99.5% by weight, based on the polymer composition (A), of polystyrene (I); and II) 0.1 to 89.9% by weight of polyolefin (II); and/or III) 0.1 to 4.9% by weight of acrylonitrile-based polymer (III); and/or IV) 0.1 to 4.9% by weight of polyester (IV), into the reaction zone (R) of a pyrolysis reactor (P); b) thermal cracking the polystyrene contained in the polymer composition (A) in the reaction zone (R) of the pyrolysis reactor (P) at a temperature of between 400-1000° C., c) removing the product mixture (G) obtained from the reaction zone (R), d) cooling of the product mixture (G), and e) separating the styrene monomers from the further components.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A process for the production of styrene monomers by depolymerization of a polystyrene-containing polymer composition, comprising the steps of:
a) introducing a polymer composition (A) containing:
I) 10% to 99.5% by weight of a polystyrene (I), based on the total weight of the polymer composition (A); and
II) 0.1% to 89.9% by weight of a polyolefin (II), based on the total weight of the polymer composition (A); and/or
III) 0.1% to 4.9% by weight of an acrylonitrile-based polymer (III), based on the total weight of the polymer composition (A); and/or
IV) 0.1% to 4.9% by weight of a polyester (IV), based on the total weight of the polymer composition (A),
into a reaction zone (R) of a pyrolysis reactor (P);
b) thermally cleaving the polystyrene (I) present in the polymer composition (A) in the reaction zone (R) of the pyrolysis reactor (P) at a temperature of from 400° C. to 1000° C. to obtain a product mixture (G) containing styrene monomers and further components;
c) withdrawing the product mixture (G) obtained in step b) from the reaction zone (R) of the pyrolysis reactor (P);
d) cooling the product mixture (G) withdrawn in step c) to obtain a condensed product mixture (K) containing styrene monomers and further components; and
e) separating the styrene monomers from the further components of the condensed product mixture (K) obtained in step d),
wherein an average residence time (Z) of the polymer composition (A) in the reaction zone (R) of the pyrolysis reactor (P) is from 0.01 s to 10 s.

### Claim 17 (depends on 16)

The process of claim 16, wherein the polyolefin (II) is polyethylene (PE) and/or polypropylene (PP), and/or the acrylonitrile-based polymer (Ill) is acrylonitrile-butadiene-styrene graft copolymer (ABS), and/or the polyester (IV) is polyethylene terephthalate (PET).

### Claim 18 (depends on 16)

The process of claim 16, wherein the polymer composition (A) contains the polystyrene (I) in an amount of from 85% to 99.5% by weight, based on the total weight of the polymer composition (A), and the polyolefin (II) in an amount of from 0.1% to 15% by weight, based on the total weight of the polymer composition (A), and/or the acrylonitrile-based polymer (III) in an amount of from 0.1% to 2% by weight, based on the total weight of the polymer composition (A), and/or the polyester (IV) in an amount of from 0.1% to 2% by weight, based on the total weight of the polymer composition (A).

### Claim 19 (depends on 16)

The process of claim 16, wherein the temperature in the reaction zone (R) of the pyrolysis reactor (P) is 580° C. to 630° C. and the average residence time (Z) of the polymer composition (A) in the reaction zone (R) of the pyrolysis reactor (P) is 0.4 s to 0.6 s.

### Claim 20 (depends on 16)

The process of claim 16, wherein the condensed product mixture (K) obtained in step d) contains from 75% to 99% by weight of styrene and 1% to 25% by weight of the further components, based on the total weight of the condensed product mixture (K).

### Claim 21 (depends on 16)

The process of claim 16, wherein the pyrolysis reactor (P) is a fluidized bed reactor.

### Claim 22 (depends on 16)

The process of claim 16, wherein at least a portion of the further components obtained in step e) is recycled into the reaction zone (R) of the pyrolysis reactor (P).

### Claim 23 (depends on 22)

The process of claim 22, wherein the further components obtained in step e) which are recycled into the reaction zone (R) of the pyrolysis reactor (P) consist essentially of styrene oligomers.

### Claim 24 (depends on 16)

The process of claim 16, wherein the polystyrene (I) component in the polymer composition (A), which in step a) is introduced into the reaction zone (R) of the pyrolysis reactor (P), consists essentially of general purpose polystyrene (GPPS).

### Claim 25 (depends on 16)

The process of claim 16, wherein in step d) the product mixture (G) that is withdrawn in step c) is cooled to a temperature of from 0° C. to 50° C.

### Claim 26 (depends on 16)

The process of claim 16, wherein the separation of the styrene monomers in step e) comprises a step of fractional distillation.

### Claim 27 (depends on 21)

The process of claim 21, wherein the fluidized bed reactor comprises a silicon carbide fluidized bed in the reaction zone (R).

### Claim 28 (depends on 22)

The process of claim 22, wherein the recycling of the further components into the reaction zone (R) of the pyrolysis reactor (P) is continuous.

### Claim 29

A process for the depolymerization of a polystyrene-containing polymer composition (A), comprising the use of a fluidized bed reactor with a temperature in a reaction zone (R) of the fluidized bed reactor of from 400° C. to 1000° C. and with an average residence time (Z) of the polystyrene-containing polymer composition (A) in the reaction zone (R) of from 0.01 s to 10 s, wherein the polystyrene-containing polymer composition (A) on entry into the reaction zone (R) of the reactor contains:
I) 10% to 99.5% by weight of a polystyrene (I), based on the total weight of the polystyrene-containing polymer composition (A); and
II) 0.1% to 89.9% by weight of a polyolefin (II), based on the total weight of the polystyrene-containing polymer composition (A); and/or
III) 0.1% to 4.9% by weight of an acrylonitrile-based polymer (III), based on the total weight of the polystyrene-containing polymer composition (A); and/or
IV) 0.1% to 4.9% by weight of a polyester (IV), based on the total weight of the polystyrene-containing polymer composition (A).

### Claim 30 (depends on 29)

The process of claim 29, wherein the fluidized bed reactor comprises a silicon carbide fluidized bed.

### Claim 31 (depends on 16)

An apparatus for conducting the process of claim 16, wherein the reaction zone (R) and the pyrolysis reactor (P) are configured such that gentle depolymerization of polystyrene is possible.

### Claim 32 (depends on 31)

The apparatus of claim 31, wherein the pyrolysis reactor (P) is a fluidized bed reactor.

### Claim 33 (depends on 32)

The apparatus of claim 32, wherein the fluidized bed reactor comprises a silicon carbide fluidized bed.

### Claim 34 (depends on 16)

The process of claim 16, wherein the polymer composition (A) contains the polystyrene (I), the polyolefin (II), the acrylonitrile-based polymer (III), and the polyester (IV).

### Claim 35 (depends on 34)

The process of claim 34, wherein the polyolefin (II) is polyethylene (PE) and/or polypropylene (PP), the acrylonitrile-based polymer (III) is acrylonitrile-butadiene-styrene graft copolymer (ABS), and the polyester (IV) is polyethylene terephthalate (PET).