# US 2022/0403120 A1 · A method for preparing a pre-treated synthetic latex emulsion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0403120 A1
- Document ID: US20220403120A1
- Status: Published application
- Kind: A1
- Application number: 17/777,707
- Filed: 2019-12-05
- Published: 2022-12-22
- Earliest claimed: 2019-11-19
- Assignees: Ci Technology Sdn Bhd
- Applicants: Ci Technology Sdn Bhd
- Inventors: Kok Ho TEE
- Web page: https://patentgrep.com/patent/US20220403120A1

## CPC

- C08J 3/21: the polymer being premixed with a liquid phase
- C08J 3/215: at least one additive being also premixed with a liquid phase
- C08J 2309/04: Latex
- C08J 2407/02: Latex
- C08J 2409/10: Latex (C08J2409/04, C08J2409/08 take precedence)
- C08J 2411/02: Latex
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The present invention relates to a method (100) for preparing a pre-treated synthetic latex emulsion, the method comprising the steps of, adding a synthetic latex into a tank (101), characterized by mixing a surfactant with the synthetic latex in the tank (102), adding alkaline material into a mixture of the synthetic latex added with the surfactant (103), adding a reactive metal ion into the mixture (104) and continue mixing the mixture for at least two hours (105), wherein the reactive metal ion is obtained by heating a metal oxide or metal hydroxide with supply of alkaline material at 120 to 180° C.

## Claims

### Claim 1

A method (100) for preparing a pre-treated synthetic latex emulsion, the method comprising the steps of:
adding a synthetic latex into a tank (101);
characterized by;
mixing a surfactant with the synthetic latex in the tank (102);
adding alkaline material into a mixture of the synthetic latex added with the surfactant (103);
adding a reactive metal ion into the mixture (104); and
continue mixing the mixture for at least two hours (105);
wherein the reactive metal ion is obtained by heating a metal oxide or metal hydroxide with supply of alkaline material at 120 to 180° C.

### Claim 2 (depends on 1)

The method (100) as claimed in claim 1, wherein the synthetic latex is carboxylated acrylonitrile butadiene rubber.

### Claim 3 (depends on 1)

The method (100) as claimed in claim 1, wherein the synthetic latex is selected from a polymer with carboxylic acid monomer such as acrylonitrile, butadiene and carboxylic acid or styrene, butadiene and carboxylic acid and a combination thereof.

### Claim 4 (depends on 1)

The method (100) as claimed in claim 1, wherein the synthetic latex is selected from a polymer without carboxylic acid monomer such as acrylic, styrene acrylic, polychloroprene, polyisoprene, polyurethane, polyacrylates, polyvinyl chloride, polyvinyl acetate and a combination thereof.

### Claim 5 (depends on 1)

The method (100) as claimed in claim 1, wherein the synthetic latex is strained using a strainer comprising single or multiple filtering media capable of removing particulates before adding into the tank.

### Claim 6 (depends on 1)

The method (100) as claimed in claim 1, wherein the surfactant mixed with the synthetic latex in the tank at 30 to 100 rpm for 1 to 4 hours.

### Claim 7 (depends on 1)

The method (100) as claimed in claim 1, wherein the maximum amount of the surfactant is at 7.0 phr.

### Claim 8 (depends on 1)

The method (100) as claimed in claim 1, wherein the surfactant diluted at 1:3 to 1.15.

### Claim 9 (depends on 1)

The method (100) as claimed in claim 1, wherein the surfactant comprises of anionic surfactant, non-ionic surfactants or a combination thereof.

### Claim 10 (depends on 9)

The method (100) as claimed in claim 9, wherein the anionic surfactant is selected from sulfonic acid salts, alcohol ether sulphates, alcohol sulphates, alkyl benzene sulfonates, phosphoric acid esters, alkyl carboxylates, alkyl ethoxylated carboxylates, alkyl sulfates, alkyl ethoxylated sulfates, olefin sulfonates and isethionates.

### Claim 11 (depends on 9)

The method (100) as claimed in claim 9, wherein the non-ionic surfactant is selected from alkyl ethoxylates, alcohol ethoxylates, fatty acid alkanolamides, alkylamine oxides, alkyl polyglucosides, polyglycerol alkyl ethers, glucosyl dialkyl ethers, polyethylene glycol, alkyl polyethylene glycol ether, sorbitan esters, polysorbates and alkyl, fluorinated and silicone based polyethylene oxide, oligomeric surfactants and poly alkylene oxide block copolymers.

### Claim 12 (depends on 1)

The method (100) as claimed in claim 1, the maximum amount of the reactive metal ion is at 0.25 phr.

### Claim 13 (depends on 1)

The method (100) as claimed in claim 1, wherein the metal oxide or metal hydroxide whereby the metal is selected from Zinc, Aluminium or Copper.

### Claim 14 (depends on 1)

The method (100) as claimed in claim 1, wherein the maximum amount of the alkaline material is at 5.0 phr.

### Claim 15 (depends on 1)

The method (100) as claimed in claim 1, wherein the alkaline material is potassium hydroxide.

### Claim 16 (depends on 15)

The method (100) as claimed in claim 15, wherein the potassium hydroxide is diluted at 2 to 5% of potassium hydroxide.

### Claim 17 (depends on 1)

The method (100) as claimed in claim 1, wherein the steps further comprising addition of ammonium hydroxide diluted at the range of 1:2 to 1:20 to boost the pH during adding of the reactive metal ion.

### Claim 18 (depends on 1)

The method (100) as claimed in claim 1, wherein the steps further comprising
the step of adding covalent bonding agent after addition of the reactive metal ion.

### Claim 19 (depends on 18)

The method (100) as claimed in claim 18, wherein the covalent bonding agent is in a solubilized form and/or micronized form.

### Claim 20 (depends on 18)

The method (100) as claimed in claim 18, wherein the maximum amount of the covalent bonding agent is at 0.25 phr.

### Claim 21 (depends on 18)

The method (100) as claimed in claim 18, wherein the covalent bonding agent is selected from sulphur and/or sulphur donor.

### Claim 22 (depends on 1)

An additive for producing dipping articles characterized by: a reactive metal ion of claim 1; wherein said reactive metal ion is an activated metal of higher oxidation state consisting of Zinc or combination with other higher oxidation metal selected from Aluminum and/or other metals selected from transitional or post transitional group; wherein said metal is activated by heating at a temperature of 120° C. to 180° C. in alkaline condition for addition in a latex emulsion.

### Claim 23 (depends on 22)

The additive for producing dipping articles as claimed in claim 22, wherein the activated metal of higher oxidation state consisting of Zinc and other like material in the form of solid or in a heterogeneous or homogeneous solution with water.