# US 2022/0402756 A1 · Hydrogen storage and release material and method of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0402756 A1
- Document ID: US20220402756A1
- Status: Published application
- Kind: A1
- Application number: 17/776,470
- Filed: 2020-11-06
- Published: 2022-12-22
- Earliest claimed: 2019-11-18
- Assignees: University of Tsukuba; Tokyo Institute of Technology
- Applicants: University of Tsukuba; Tokyo Institute of Technology
- Inventors: Takahiro Kondo; Ryota Ishibiki; Taiga Goto; Shin-Ichi Ito; Yoshihiro Kinoshita
- Web page: https://patentgrep.com/patent/US20220402756A1

## CPC

- C01B 3/001: characterised by the uptaking media; Treatment thereof
- C01B 3/0084: Solid storage media characterised by their shape, e.g. porous compacts or hollow particles
- C01B 6/10: Monoborane; Diborane; Addition complexes thereof
- C01B 35/026: {Higher boron hydrides, i.e. containing at least three boron atoms}
- Y02E 60/32: Hydrogen storage
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a hydrogen storage and release material including a two-dimensional hydrogen boride-containing sheet including a two-dimensional network containing n(HxBy) (n≥4, 0.001≤x/y≤0.999) having a molar ratio of boron to hydrogen from 1:0.999 to 1:0.001, the molar ratio being determined by thermal desorption spectroscopy, and mass measurement before and after a temperature rise, wherein the hydrogen storage and release material has: peaks derived from B1s of boron at 187.5±1.0 eV and 191.2±1.0 eV to 193±1.0 eV in X-ray photoelectron spectroscopy, and a peak derived from a B—H stretching vibration at from 2400 cm−1 to 2600 cm−1 and also a peak derived from a B—H—B stretching vibration at from 1200 cm−1 to 1800 cm−1 in infrared spectroscopy.

## Claims

### Claim 1

A material for reversible hydrogen storage and release comprising a two-dimensional hydrogen boride-containing sheet including a two-dimensional network containing n(HxBy) (n≥4, 0.001≤x/y≤0.999) having a molar ratio of boron to hydrogen from 1:0.999 to 1:0.001, the molar ratio being determined by thermal desorption spectroscopy, and mass measurement before and after temperature rise,
wherein the material for reversible hydrogen storage and release:
has peaks derived from B1s of boron at 187.5±1.0 eV and 191.2±1.0 eV to 193±1.0 eV in X-ray photoelectron spectroscopy, and
has a peak derived from a B—H stretching vibration at from 2400 cm−1 to 2600 cm−1 and also has a peak derived from a B—H—B stretching vibration at from 1200 cm−1 to 1800 cm−1 in infrared spectroscopy,
the material for reversible hydrogen storage and release reversibly stores and releases hydrogen,
the material for reversible hydrogen storage and release releases hydrogen by heating it to from 120° C. to 450° C., and
the material for reversible hydrogen storage and release that has released hydrogen stores hydrogen by bringing it into contact with water.

### Claim 2 (depends on 1)

The material for reversible hydrogen storage and release according to claim 1, wherein the two-dimensional hydrogen boride-containing sheet has a mesh-shaped planar structure in which boron atoms are arranged in a cyclic hexagon, a plurality of the hexagons formed by the boron atoms are connected to each other, and
hydrogen atoms are randomly bonded to the boron atoms forming the plurality of the hexagons, without having specific periodic regularity and without aggregating.

### Claim 3 (depends on 1)

The material for reversible hydrogen storage and release according to claim 1, wherein the two-dimensional hydrogen boride-containing sheet has a length of 100 nm or more in at least one direction.

### Claim 4 (depends on 1)

A method of producing the material for reversible hydrogen storage and release described in claim 1, comprising:
mixing, in a polar organic solvent, magnesium diboride having an MgB2 type structure and an ion exchange resin to which an ion that is ion-exchangeable with a magnesium ion constituting the magnesium diboride is coordinated, to form a hydrogen storage and release material precursor; and
heat-treating the hydrogen storage and release material precursor at from 120° C. to 450° C.

### Claim 5 (depends on 4)

The method of producing the material for reversible hydrogen storage and release according to claim 4,
wherein the hydrogen storage and release material precursor:
includes a two-dimensional network containing (HB)n (n≥4) having a molar ratio of boron to hydrogen at 1:1, the molar ratio being determined by thermal desorption spectroscopy, and mass measurement before and after temperature rise, and
has a spectrum showing a peak derived from B1s of negatively charged boron at 188 eV±1.0 eV in X-ray photoelectron spectroscopy, and showing a peak derived from an sp2 structure of boron at 191 eV±1.0 eV in electron energy loss spectroscopy.

### Claim 6 (depends on 4)

The method of producing the material for reversible hydrogen storage and release according to claim 4, wherein the hydrogen storage and release material precursor has a mesh shape in which boron atoms are arranged in a cyclic hexagon, and a plurality of hexagons formed by the boron atoms are connected to each other, and includes a two-dimensional network having a site where adjacent two boron atoms, among the boron atoms, are bonded to the same hydrogen atom.

### Claim 7 (depends on 4)

The method of producing the material for reversible hydrogen storage and release according to claim 4, wherein the ion exchange resin has a sulfo group.

### Claim 8 (depends on 4)

The method of producing the material for reversible hydrogen storage and release according to claim 4, wherein the polar organic solvent is acetonitrile.

### Claim 9

A reversible hydrogen storage and release method, comprising:
heating a hydrogen storage and release material to from 120° C. to 450° C. to release hydrogen and bringing the hydrogen storage and release material that has released hydrogen into contact with water to store hydrogen,
wherein the hydrogen storage and release material:
comprises a two-dimensional hydrogen boride-containing sheet including a two-dimensional network containing n(HxBy) (n≥4, 0.001≤x/y≤0.999) having a molar ratio of boron to hydrogen from 1:0.999 to 1:0.001, the molar ratio being determined by thermal desorption spectroscopy, and mass measurement before and after temperature rise,
has peaks derived from B1s of boron at 187.5±1.0 eV and 191.2±1.0 eV to 193±1.0 eV in X-ray photoelectron spectroscopy, and
has a peak derived from a B—H stretching vibration at from 2400 cm−1 to 2600 cm−1 and also has a peak derived from a B—H—B stretching vibration at from 1200 cm−1 to 1800 cm−1 in infrared spectroscopy.