# US 2022/0395810 A1 · Systems and methods for processing ammonia

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0395810 A1
- Document ID: US20220395810A1
- Status: Published application
- Kind: A1
- Application number: 17/886,307
- Filed: 2022-08-11
- Published: 2022-12-15
- Earliest claimed: 2021-06-11
- Assignees: AMOGY Inc.
- Applicants: AMOGY Inc.
- Inventors: Boris SHELUDKO; Jongwon CHOI; Young Suk JO
- Web page: https://patentgrep.com/patent/US20220395810A1

## CPC

- B01J 21/066: {Zirconium or hafnium; Oxides or hydroxides thereof}
- B01J 23/10: of rare earths
- B01J 21/04: Alumina
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/462: {Ruthenium}
- B01J 23/63: with rare earths or actinides
- B01J 23/83: with rare earths or actinides
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 37/0205: {in several steps}
- B01J 37/0209: {involving a reaction between the support and a fluid}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01B 3/047: Decomposition of ammonia
- C01C 1/0411: {characterised by the catalyst}
- B01J 2523/13: Potassium
- B01J 2523/14: Rubidium
- B01J 2523/15: Caesium
- B01J 2523/31: Aluminium
- B01J 2523/3706: Lanthanum
- B01J 2523/3712: Cerium
- B01J 2523/48: Zirconium
- B01J 2523/821: Ruthenium
- C01B 2203/0277: containing a catalytic decomposition step
- C01B 2203/066: with fuel cells
- C01B 2203/1029: Catalysts in the form of a foam
- C01B 2203/1047: Group VIII metal catalysts
- C01B 2203/1058: Nickel catalysts
- C01B 2203/1064: Platinum group metal catalysts
- C01B 2203/1082: Composition of support materials
- C01B 2203/1094: Promotors or activators
- Y02E 60/36: Hydrogen production from non-carbon containing sources, e.g. by water electrolysis
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01C: AMMONIA; CYANOGEN; COMPOUNDS THEREOF ({metal hydrides, monoborane, diborane or addition complexes thereof C01B6/00}; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; azides C01B21/08; {compounds other than ammonia or cyanogen, containing nitrogen, non-metals and optionally metals C01B21/082}; metal imides or amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; compounds containing silicon C01B33/00; compounds containing boron C01B35/00)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure provides methods for fabricating catalysts for ammonia decomposition. The method may comprise (a) subjecting a catalyst support to one or more physical or chemical processes to optimize one or more pores, morphologies, and/or surface chemistry or property of the catalyst support; (b) depositing a composite support material on the catalyst support, wherein the composite support material comprises a morphology or surface chemistry or property; and (c) depositing one or more active metals on at least one of the composite support material and the catalyst support, wherein the one or more active metals comprise one or more nanoparticles configured to conform to the morphology of the composite support material and/or catalyst support material, thereby optimizing one or more active sites on the nanoparticles for ammonia processing.

## Claims

### Claim 1

A catalyst for ammonia decomposition, comprising:
a support comprising aluminum and oxygen, and a layer adjacent to the support, wherein the layer comprises (1) aluminum and oxygen, and (2) an oxide of at least one of (i) cerium (Ce) and (ii) lanthanum (La); and
one or more active metal particles adjacent to the layer, wherein the one or more active metal particles comprise at least one member selected from the group consisting of Ru, Ni, Rh, Ir, Co, Fe, Pt, Cr, Mo, Pd, and Cu, wherein a concentration of the one or more active metal particles ranges from about 0.5 wt % to about 10 wt %.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein the support comprises a phase comprising at least one of theta alumina (θ-alumina) or gamma alumina (γ-alumina), and wherein the layer comprises an alumina-supported perovskite phase.

### Claim 3 (depends on 2)

The catalyst of claim 2, wherein the layer comprises La at a concentration ranging from about 5 mol % to about 25 mol %.

### Claim 4 (depends on 3)

The catalyst of claim 3, wherein the layer further comprises Ce, and wherein a molar ratio of the La to the Ce ranges from about 90:10 to about 10:90.

### Claim 5 (depends on 3)

The catalyst of claim 3, wherein the one or more active metal particles comprises nanoparticles of ruthenium (Ru), after the layer is contacted with hydrogen (H2) gas at a temperature ranging from about 600° C. to about 1000° C. for at least 1 hour and not more than 40 hours.

### Claim 6 (depends on 5)

The catalyst of claim 5, wherein the support or the layer further comprises one or more promoters selected from the group consisting of K, Cs and Rb.

### Claim 7 (depends on 6)

The catalyst of claim 6, wherein a molar ratio of the one or more promoters to the one or more active metal particles ranges from about 1:1 to about 10:1.

### Claim 8 (depends on 7)

The catalyst of claim 7, wherein the concentration of Ru is not more than about 1.5 wt %.

### Claim 9

A method of producing a catalyst for ammonia decomposition, comprising:
(a) (i) using at least Al2O3 or precursors thereof to form a support comprising at least one member selected from the group consisting of θ-alumina and γ-alumina, and (ii) using at least one of La2O3 or precursors thereof and CeO2 or precursors thereof to produce a layer comprising an alumina-supported perovskite phase;
(b) depositing at least one precursor of one or more active metal particles adjacent to the layer, wherein the one or more active metal particles comprise at least one member selected from the group consisting of Ru, Ni, Rh, Ir, Co, Fe, Pt, Cr, Mo, Pd, and Cu, wherein the concentration of the one or more active metal particles ranges from about 0.5 wt % to about 10 wt %; and
(c) contacting the catalyst with hydrogen (H2) gas at a temperature ranging from about 600° C. to about 1000° C. for at least 1 hour and not more than 40 hours.

### Claim 10 (depends on 9)

The method of claim 9, wherein the layer comprises La at a concentration ranging from about 5 mol % to about 25 mol %.

### Claim 11 (depends on 10)

The method of claim 10, wherein the La2O3 or precursors thereof comprise La and the CeO2 or precursors thereof comprise Ce, wherein a molar ratio of the La to the Ce ranges from about 90:10 to about 10:90.

### Claim 12 (depends on 11)

The method of claim 11, wherein (a) further comprises (iii) incorporating one or more promoters or promoter precursors, and wherein the one or more promoters are selected from K, Cs and Rb.

### Claim 13 (depends on 12)

The method of claim 12, wherein a molar ratio of the promoter to the active metal ranges from about 1:1 to about 10:1.

### Claim 14 (depends on 13)

The catalyst of claim 13, wherein the one or more active metal particles comprise ruthenium (Ru), and wherein the concentration of Ru is not more than about 1.5 wt %.

### Claim 15 (depends on 10)

The method of claim 10, wherein the Al2O3 or precursor(s) thereof comprise beads or pellets, and wherein the beads or the pellets comprise at least one of (i) a diameter ranging from about 0.1 millimeters (mm) to about 10 mm, or (ii) a surface area per unit mass ranging from about 50 m2/g to about 500 m2/g.

### Claim 16 (depends on 10)

The method of claim 10, wherein the one or more active metal particles comprise ruthenium (Ru), and the precursor of the one or more active metals comprises ruthenium nitrosyl nitrate (Ru(NO)(NO3)3).

### Claim 17 (depends on 10)

The method of claim 10, wherein the one or more active metal particles comprise ruthenium (Ru), and wherein the concentration of Ru is not more than about 1.5 wt %.

### Claim 18

A method of ammonia decomposition comprising:
(a) providing a catalyst comprising:
a support comprising aluminum and oxygen, and a layer adjacent to the support, wherein the layer comprises (1) aluminum and oxygen, and (2) an oxide of at least one of (i) cerium (Ce) and (ii) lanthanum (La); and
one or more active metal particles adjacent to the layer, wherein the one or more active metal particles comprise at least one member selected from the group consisting of Ru, Ni, Rh, Ir, Co, Fe, Pt, Cr, Mo, Pd, and Cu, wherein a concentration of the one or more active metal particles ranges from about 0.5 wt % to about 10 wt %; and
(b) contacting ammonia on the catalyst at a temperature ranging from about 300° C. to about 600° C. to generate hydrogen and nitrogen at an ammonia conversion efficiency from about 70% to about 99%.

### Claim 19 (depends on 18)

The method of claim 18, wherein the ammonia is contacted on the catalyst at a space velocity of under 10 liters per hour per gram of catalyst.

### Claim 20 (depends on 18)

The method of claim 18, further comprising generating electricity by providing the produced hydrogen to one or more fuel cells.