# US 2022/0393257 A1 · Diagnosis of Cause of Degradation of Lithium Secondary Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0393257 A1
- Document ID: US20220393257A1
- Status: Published application
- Kind: A1
- Application number: 17/641,225
- Filed: 2021-04-28
- Published: 2022-12-08
- Earliest claimed: 2020-05-27
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Hyo Jung Yoon; Eun Ju Lee; So Young Kim
- Web page: https://patentgrep.com/patent/US20220393257A1

## CPC

- G01N 23/2055: Analysing diffraction patterns
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/42: Methods or arrangements for servicing or maintenance of secondary cells or secondary half-cells (H01M10/60 takes precedence)
- G01N 23/207: Diffractometry using detectors, e.g. using a probe in a central position and one or more displaceable detectors in circumferential positions
- G01N 2223/056: diffraction
- G01N 2223/606: texture
- G01N 2223/611: patterned objects; electronic devices
- G01N 2223/632: residual life, life expectancy
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- H01M 10/48: Accumulators combined with arrangements for measuring, testing or indicating the condition of cells, e.g. the level or density of the electrolyte (constructional details of current conducting connections for detecting conditions inside cells or batteries, e.g. details of voltage sensing terminals, H01M50/569)
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a method of diagnosing the degradation of a lithium secondary battery in a non-destructive manner without disassembling the battery, which includes: obtaining, from X-ray diffraction (XRD) data obtained during first charging of the lithium secondary battery, a first graph showing the change of the c-axis d-spacing value of the layered positive electrode active material according to the number of moles of lithium ions deintercalated from the layered positive electrode active material during the charging; obtaining, from XRD data obtained during second charging of the lithium secondary battery, a second graph showing the change of the c-axis d-spacing value of the layered positive electrode active material according to the number of moles of lithium ions deintercalated from the layered positive electrode active material during the charging; and classifying a cause of degradation of the secondary battery by comparing the first graph and the second graph.

## Claims

### Claim 1

A method of diagnosing a cause of degradation of a lithium secondary battery, comprising:
(A) manufacturing a lithium secondary battery including a positive electrode including a layered positive electrode active material, a negative electrode, separator interposed between the positive electrode and the negative electrode, and an electrolyte;
(B) obtaining, from a first X-ray diffraction data obtained during first charging of the lithium secondary battery, a first graph showing the change of the c-axis d-spacing value of the layered positive electrode active material according to a number of moles of lithium ions deintercalated from the layered positive electrode active material during the first charging;
(C) obtaining, from a second X-ray diffraction data obtained during second charging of the lithium secondary battery, a second graph showing the change of the c-axis d-spacing value of the layered positive electrode active material according to a number of moles of lithium ions deintercalated from the layered positive electrode active material during the second charging; and
(D) classifying the cause of degradation of the secondary battery by comparing the first graph and the second graph.

### Claim 2 (depends on 1)

The method of claim 1, wherein the cause of the degradation of the secondary battery is one or more of a loss of available lithium or a loss of positive electrode capacity.

### Claim 3 (depends on 1)

The method of claim 1, wherein the step (D) includes:
classifying the cause of the degradation of the secondary battery as the loss of available lithium when a maximum value of the number of moles of deintercalated lithium ions in the second graph is smaller than a maximum value of the number of moles of deintercalated lithium ions in the first graph; and
after horizontally shifting the second graph in an x-axis direction so that the number of moles of deintercalated lithium ions corresponding to the maximum c-axis d-spacing value of the layered positive electrode active material in the second graph is the same as the number of moles of deintercalated lithium ions corresponding to the maximum c-axis d-spacing value of the layered positive electrode active material in the first graph, classifying the cause of the degradation of the secondary battery as a loss of positive electrode capacity when a sum of the maximum number of moles of deintercalated lithium ions in the second graph and a degree by which the second graph is horizontally shifted is greater than the maximum number of moles of deintercalated lithium ions in the first graph.

### Claim 4 (depends on 3)

The method of claim 3, wherein the step (D) includes quantifying an amount of the loss of the available lithium as a value obtained by subtracting the maximum number of moles of deintercalated lithium ions in the second graph from the maximum number of moles of deintercalated lithium ions in the first graph.

### Claim 5 (depends on 3)

The method of claim 3, wherein the step (D) includes quantifying an amount of the loss of the positive electrode capacity as a value obtained by subtracting the maximum number of moles of deintercalated lithium ions in the first graph from a sum of the maximum number of moles of deintercalated lithium ions in the second graph and a degree by which the second graph is horizontally shifted.

### Claim 6 (depends on 4)

The method of claim 4, wherein, determining that the degradation of the lithium secondary battery is due to the loss of the available lithium when a rate of the loss of the available lithium according to the following Equation 1 is 14% or more:
Rate of loss of available lithium=(Amount of loss of available lithium)/(Maximum number of moles of deintercalated lithium ions in first graph)×100. [Equation 1]

### Claim 7 (depends on 1)

The method of claim 1, wherein the layered positive electrode active material is a lithium transition metal oxide including nickel at 60 mol % or more relative to a total number of moles of transition metals excluding lithium.

### Claim 8 (depends on 1)

The method of claim 1, wherein the layered positive electrode active material is represented by the following Chemical Formula 1:
Li1+aNixCoyMzO2, [Chemical Formula 1]
wherein, in Chemical Formula 1,
0≤a≤0.3, 0.6≤x≤1.0, 0≤y≤0.2, 0≤z≤0.2, and x+y+z=1, and M is one or more of manganese or aluminum.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second charging is:
charging performed after discharging the lithium secondary battery subjected to the first charging and subsequently repeatedly charging and discharging the lithium secondary battery for one or more cycles; or
charging performed after discharging the lithium secondary battery subjected to the first charging and subsequently storing the lithium secondary battery for a long period of time at a temperature of −20° C. to 70° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first charging and the second charging are performed in a voltage range of 2.5 V to 4.2 V.

### Claim 11 (depends on 1)

The method of claim 1, wherein the X-ray diffraction data is obtained using a transmission X-ray diffraction analyzer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the d-spacing value is a d-spacing value in the (003) plane of the layered positive electrode active material.