# US 2022/0393080 A1 · Composite Wavelength Converter

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0393080 A1
- Document ID: US20220393080A1
- Status: Published application
- Kind: A1
- Application number: 17/775,772
- Filed: 2020-12-01
- Published: 2022-12-08
- Earliest claimed: 2019-12-05
- Assignees: Friedrich-Alexander-Universität Erlangen-Nürnberg
- Applicants: Friedrich-Alexander-Universität Erlangen-Nürnberg
- Inventors: Yuriy Zorenko; Miroslaw Batentschuk; Christoph Brabec; Andres Osvet; Vitalii Gorbenko; Ievgen Levchuk; Tetiana Zorenko; Liudmyla Chepyga; Anton Markovskyi; Sandra Witkiewicz-Lukaszek
- Web page: https://patentgrep.com/patent/US20220393080A1

## CPC

- C09K 11/7774: {Aluminates}
- H10H 20/8513: {having two or more wavelength conversion materials}
- C09K 11/77742: {Silicates}
- C30B 19/02: using molten solvents, e.g. flux
- C30B 19/04: the solvent being a component of the crystal composition
- C30B 19/12: characterised by the substrate
- C30B 29/28: with formula A3Me5O12 wherein A is a rare earth metal and Me is Fe, Ga, Sc, Cr, Co or Al, e.g. garnets
- C30B 31/04: by contacting with diffusion materials in the liquid state
- G02B 5/208: {for use with infrared or ultraviolet radiation, e.g. for separating visible light from infrared and/or ultraviolet radiation}
- H10H 20/062: {Light-emitting semiconductor devices having field effect type light-emitting regions, e.g. light-emitting High-Electron Mobility Transistors}
- H10H 20/0361: {of wavelength conversion means}
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

The invention refers to a composite wavelength converter (1) for an LED (100), comprising a substrate (10) and an epitaxial film (20) formed by liquid phase epitaxy on the top and bottom of the substrate (10). Furthermore, the invention refers to a method of preparation of a composite wavelength converter (1) for an LED (100). Furthermore, the invention refers to a white LED light source comprising an LED (100) and an inventive composite wavelength converter (1) mounted on a light emitting surface of the LED (100).

## Claims

### Claim 1

A composite wavelength converter for an LED, comprising
a substrate (10) formed by a first layer of single crystalline garnet phosphor presenting first emission and excitation spectra, having a cubic crystal structure, a first lattice parameter and oriented crystal planes, wherein the substrate (10) contains a first activator, and
an epitaxial film (20) formed by liquid phase epitaxy on the top and bottom of the substrate (10) as a second layer of single crystalline garnet phosphor with the first activator and preferably at least with one second activator, presenting second emission and excitation spectra, having a cubic crystal structure and a second lattice parameter, wherein the epitaxial film (20) is arranged directly on the top and bottom of the substrate (10) on the oriented crystalline planes of the substrate (10),
wherein the second emission and excitation spectra are different from the first emission and excitation spectra,
wherein the difference between the first lattice parameter and the second lattice parameter results in a lattice mismatch within a range of about −2.0 and +2.0%, preferably of about −1.0 and +1.0%, and
wherein the thickness of the epitaxial film (20) on the top and on the bottom of the substrate (10), respectively, is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm.

### Claim 2 (depends on 1)

The converter according to claim 1, wherein the converter (1) comprises one or two additional epitaxial films, namely a first (30) and optionally a second (40) additional epitaxial film,
wherein the first additional epitaxial film (30) is formed by liquid phase epitaxy as a third layer of single crystalline garnet phosphor with the first activator and preferably at least with one second activator, arranged directly on the epitaxial film (20) on the top and bottom side of the substrate (10), presenting third emission and excitation spectra, having a cubic crystal structure and a third lattice parameter,
wherein the third layer of single crystalline garnet phosphor is preferably different from the second layer of single crystalline garnet phosphor, wherein the third emission and excitation spectra are different from the first emission and excitation spectra and preferably different from the second emission and excitation spectra,
wherein the difference between the third lattice parameter and the second lattice parameter results in a lattice mismatch within a range of about −2.0 and +2.0%, preferably of about −1.0 and +1.0%, and wherein the thickness of the first additional epitaxial film (30) on the top and on the bottom side of the substrate (10), respectively, is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm,
wherein the second additional epitaxial film (40) is formed by liquid phase epitaxy as a fourth layer of single crystalline garnet phosphor with the first activator and preferably at least with one second activator, arranged directly on the first additional epitaxial film (30) on the top and bottom side of the substrate (10), presenting fourth emission and excitation spectra, having a cubic crystal structure and a fourth lattice parameter,
wherein the fourth layer of single crystalline garnet phosphor is preferably different from the second and/or third layer of single crystalline garnet phosphor, wherein the fourth emission and excitation spectra are different from the first emission and excitation spectra and preferably different from the second and/or third emission and excitation spectra,
wherein the difference between the fourth lattice parameter and the third lattice parameter results in a lattice mismatch within a range of about −2.0 and +2.0%, preferably of about −1.0 and +1.0%, and wherein the thickness of the second additional epitaxial film (40) on the top and on the bottom side of the substrate (10), respectively, is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm, and
wherein the second activator of the epitaxial film (20), of the first additional epitaxial film (30) and/or of the second additional epitaxial film (40) are preferably different.

### Claim 3 (depends on 1)

The converter according to claim 1, wherein the first activator is Ce3+ ions, preferably having a concentration in the substrate (10) from about 0.001 to about 1% of Ce3+ ions per mole, more preferably from 0.05 to 0.15 mole %, and/or having a concentration in the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) from about 0.001 to about 1% of Ce3+ ions per mole, more preferably from 0.05 to 0.1 mole %.

### Claim 4 (depends on 1)

The converter according to claim 1, wherein the second activator is one from Eu3+, Pr3+, Tb3+ and Mn2+ ions, wherein the second activator is preferably a second dopant (R), the second dopant being one from R=Eu3+, Pr3+, Tb3+ and Mn2+ ions, preferably having a concentration from about 0.001 to about 5% of Eu3+, Pr3+ or Tb3+ ions per mole, more preferably from 1 to 3 mole %, or from about 0.001 to about 3% of Mn2+ ions per mole, more preferably from 0.1 to 1 mole %.

### Claim 5 (depends on 1)

The converter according to claim 1, wherein the substrate (10) is Y3Al5O12:Ce garnet, Lu3Al5-sGasO12:Ce garnet or Gd3Al5-sGasO12:Ce garnet, wherein s is between 2.5 and 3.

### Claim 6 (depends on 1)

The converter according to claim 1, wherein the thickness of the substrate (10) is between 0.3 and 1 mm, preferably between 0.45 and 0.5 mm.

### Claim 7 (depends on 4)

The converter according to claim 4, wherein the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) is/are formed by a mixed garnet compound having a composition
represented by a formula X=A13B12C13O12:Ce,R, wherein A1 is Ca2+ ions; B1 is Sc3+ or Al3+ or Ga3+ ions, C1 is Si4+ or Ge4+ ions and R is the second dopant, or
represented by a formula Y=A13-xA2xB12-yB2yC13-zC2zO12:Ce,R, wherein A1 is Ca2+ ions; A2 is Y3+, Lu3+, La3+, Tb3+ and Gd3+ ions; B1 is Mg2+ ions, B2 is Sc3+ or Al3+ or Ga3+ ions, C1 is Si4+ ions, C2 is Ge4+ ions and R is the second dopant, wherein 0<x<1.0, 0<y<2, and 0<z<3.

### Claim 8 (depends on 1)

The converter according to claim 1, wherein the thickness of the epitaxial film (20) on the top and/or on the bottom side of the substrate (10), respectively, is at most 200 μm, preferably at most 100 μm,
wherein the thickness of the first additional epitaxial film (30) on the top and/or on the bottom side of the substrate (10), respectively, is at most 200 μm, preferably at most 100 μm, and/or
wherein the thickness of the second additional epitaxial film (40) on the top and/or on the bottom side of the substrate (10), respectively, is at most 200 μm, preferably at most 100 μm.

### Claim 9

A method of preparation of a composite wavelength converter (1) for an LED (100), comprising the steps of
providing a substrate (10) formed by a first layer of single crystalline garnet phosphor, having a cubic crystal structure, oriented crystal planes and containing a first activator, wherein the substrate (10) is preferably Y3Al5O12:Ce garnet, Lu3Al5-sGasO12:Ce garnet or Gd3Al5-sGasO12:Ce garnet with Ce3+ ions being the first activator, wherein s is between 2.5 and 3, and
depositing an epitaxial film (20) forming a second layer of single crystalline garnet phosphor with the first activator and at least with a second activator onto both sides of the oriented planes of the substrate (10) using the liquid phase epitaxy method, wherein the thickness of the epitaxial film (20) on each side of the substrate (10) is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm.

### Claim 10 (depends on 9)

The method of preparation according to claim 9, comprising the additional step of depositing a first additional epitaxial film (30) forming a third layer of single crystalline garnet phosphor with the first activator and at least with one second activator onto the epitaxial film (20) on both sides of the substrate (10) using the liquid phase epitaxy method, wherein the thickness of the first additional epitaxial film (30) on each side of the substrate (10) is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm, and optionally comprising the additional step of
depositing a second additional epitaxial film (40) forming a fourth layer of single crystalline garnet phosphor with the first activator and at least with one second activator onto the first additional epitaxial film (30) on both sides of the substrate (10) using the liquid phase epitaxy method, wherein the thickness of the second additional epitaxial film (40) on each side of the substrate (10) is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm.

### Claim 11 (depends on 9)

The method of preparation according to claim 9, wherein the substrate (10) is embedded in a melt-solution containing flux oxides and garnet crystal forming components,
wherein the melt-solution preferably contains PbO and B2O3 as flux oxides or Bi2O3 and B2O3 as flux oxides, and the garnet crystal forming components for producing the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) formed by a mixed garnet compound having a composition
represented by a formula X=A13B12C13O12:Ce,R, wherein A1 is Ca2+ ions; B1 is Sc3+ or Al3+ or Ga3+ ions, C1 is Si4+ or Ge4+ ions and R is a second dopant, or
represented by a formula Y=A13-xA2xB12-yB2yC13-zC2zO12:Ce,R, wherein A1 is Ca2+ ions; A2 is Y3+, Lu3+, La3+, Gd3+ and/or Tb3+ ions; B1 is Mg2+ ions, B2 is Sc3+ or Al3+ or Ga3+ ions, C1 is Si4+ ions, C2 is Ge4+ ions and R is the second dopant, wherein 0<x<1.0, 0<y<2, and 0<z<3.

### Claim 12 (depends on 11)

The method of preparation according to claim 11, wherein, for producing the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) formed by the mixed garnet compound having a composition represented by a formula X, the melt-solution contains PbO, B2O3 as flux oxides or Bi2O3 and B2O3 as flux oxides; AO, B12O3, C1O2, CeO2 and one of R2O3 or R4O7 or RO2 oxides as garnet crystal forming components, wherein R2O3 is preferably Eu2O3, R4O7 is preferably Pr4O7 and/or Tb4O7, and RO2 is preferably MnO2, chosen in the respective concentrations of 90 mole % of PbO or Bi2O3, 7.5 mole % of B2O3; 0.85 mole % of AO, 0.56 mole % of B12O3, 0.835 mole % of C1O2, 0.015 mole % of CeO2 and 0.24 mole % of R2O3 or R4O7 or RO2 oxides,
and/or wherein the substrate (10) is Y3Al5O12:Ce garnet or Lu3Al5-sGasO12:Ce garnet, wherein s is between 2.5 and 3, or
wherein, for producing the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) formed by the mixed garnet compound having a composition represented by the formula Y, the melt-solution contains PbO, B2O3 as flux oxides or Bi2O3 and B2O3 as flux oxides; A1O, A22O3, B1O, B22O3; C1O2, CeO2 and one of R2O3 or R4O7 or RO2 oxides as garnet crystal forming components, wherein R2O3 is preferably Eu2O3, R4O7 is preferably Pr4O7 and/or Tb4O7, and RO2 is preferably MnO2,
chosen in respective concentrations of 90 mole % of PbO or Bi2O3, 7.5 mole % of B2O3; 0.57 mole % of A1O, 0.28 mole % of A22O3, 0.29 mole % of B1O, 0.27 mole % of B22O3; 0.835 mole % of C1O2, 0.015 mole % of CeO2 and 0.24 mole % of R2O3 or R4O7 or RO2 oxides,
and/or wherein the substrate (10) is Gd3Al5-sGasO12:Ce garnet, wherein s is between 2.5 and 3.

### Claim 13 (depends on 9)

The method of preparation according to claim 9, wherein the deposition of the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) occurs at growth temperatures in the range of 850-1100° C., preferably at growth temperatures in the range of 950-1050° C., and/or
wherein the deposition of the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) occurs at an overcooling rate of the melt-solution in the range of 1 to 90° C., preferably in the range of 10 to 30° C.

### Claim 14 (depends on 9)

The method of preparation according to claim 9, wherein the deposition of the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) occurs at a growth rate in the range of 0.01 to 3 μm/min, preferably in the range of 0.1 to 0.5 μm/min.

### Claim 15 (depends on 14)

The method of preparation according to claim 14, wherein the substrate (10) having the epitaxial film (20), first additional epitaxial film (30) and/or second additional epitaxial film (40) deposited thereon forms an epitaxial structure, and wherein the method comprises the additional step of cutting the epitaxial structure in a plurality of individual samples, each having identical optical properties.

### Claim 16

A white LED light source comprising an LED (100) and a composite wavelength converter (1) mounted on a light emitting surface of the LED (100), the converter (1) converting at least a portion of light having a wavelength lying within a first range emitted by the LED (100) into light having a wavelength lying in a second range, wherein the wavelength lying within the second range is higher than the wavelength lying within the first range
the composite wavelength converter comprising
a substrate (10) formed by a first layer of single crystalline garnet phosphor presenting first emission and excitation spectra, having a cubic crystal structure, a first lattice parameter and oriented crystal planes, wherein the substrate (10) contains a first activator, and
an epitaxial film (20) formed by liquid phase epitaxy on the top and bottom of the substrate (10) as a second layer of single crystalline garnet phosphor with the first activator and preferably at least with one second activator, presenting second emission and excitation spectra, having a cubic crystal structure and a second lattice parameter, wherein the epitaxial film (20) is arranged directly on the top and bottom of the substrate (10) on the oriented crystalline planes of the substrate (10),
wherein the second emission and excitation spectra are different from the first emission and excitation spectra,
wherein the difference between the first lattice parameter and the second lattice parameter results in a lattice mismatch within a range of about −2.0 and +2.0%, preferably of about −1.0 and +1.0%, and
wherein the thickness of the epitaxial film (20) on the top and on the bottom of the substrate (10), respectively, is at least 2 μm, preferably at least 20 μm, more preferably at least 30 μm, most preferably at least 50 μm.

### Claim 17 (depends on 16)

The white LED light source according to claim 16, wherein the wavelength lying within the first range belongs to the blue wavelength range, and wherein the converter (1) is adapted to convert an appropriate portion of the light having the wavelength lying within the first range into light having the wavelength lying within the second range for creating a white light spectrum comprising the remaining portion of the light having the wavelength lying within the first range and the portion converted into light having the wavelength lying within the second range, or
wherein the wavelength lying within the first range belongs to the UV wavelength range, wherein the wavelength lying within the second range belongs to the visible wavelength range, and wherein the converter (1) is adapted to convert essentially 100% of the light having the wavelength lying within the first range into light having the wavelength lying within the second range.