# US 2022/0386720 A1 · Eco-friendly wearable dipped article and method of manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0386720 A1
- Document ID: US20220386720A1
- Status: Published application
- Kind: A1
- Application number: 17/338,623
- Filed: 2021-06-03
- Published: 2022-12-08
- Earliest claimed: 2021-06-03
- Assignees: Shen Wei (USA), Inc.
- Applicants: Shen Wei (USA) Inc.
- Inventors: Belle L. Chou; Sisitha Sudarshana; Ranthi Dias; Samantha S. Chang
- Web page: https://patentgrep.com/patent/US20220386720A1

## CPC

- A41D 19/0058: {Three-dimensional gloves}
- B29C 37/0092: {Drying moulded articles or half products, e.g. preforms, during or after moulding or cooling}
- B29C 41/003: {characterised by the choice of material}
- B29C 41/14: Dipping a core {(B29C41/10 takes precedence)}
- B29C 41/46: Heating or cooling
- C08K 3/16: Halogen-containing compounds
- C08K 3/30: Sulfur-, selenium- or tellurium-containing compounds
- C08L 21/00: Compositions of unspecified rubbers
- A41D 2400/52: Disposable
- A41D 2500/54: in coated form
- B29K 2021/006: {Thermosetting elastomers}
- B29K 2105/0017: {Agents activating degradation}
- B29L 2031/4864: {Gloves}
- C08J 5/02: Direct processing of dispersions, e.g. latex, to articles
- C08J 7/048: Forming gas barrier coatings
- C08J 2309/04: Latex
- C08J 2321/02: Latex
- C08J 2409/00: Characterised by the use of homopolymers or copolymers of conjugated diene hydrocarbons
- C08J 2421/02: Latex
- C08J 2475/04: Polyurethanes
- C08K 2003/3063: {Magnesium sulfate}
- C08K 2003/3072: {Iron sulfates}
- Y02C 20/20: of methane
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]

## Abstract

The present invention generally relates to an eco-friendly wearable article comprising a nutrient complex capable of efficiently able to reduce or eliminate methane gas emission during biodegradation of the article, and a method of making the eco-friendly wearable article containing the nutrient complex. Preferably, the nutrient complex typically comprises anionic sulphate ions and cationic salts of iron(II) and copper(II), thereby facilitating methane oxidation in an anaerobic environment such as a landfill.

## Claims

### Claim 1

An eco-friendly wearable article comprising a nutrient complex, wherein the article is prepared by dipping in a coagulant dipping system, the coagulant dipping system comprising:
a multiple application of the coagulant, the coagulant comprising anionic sulphate ions and cationic salts of iron(II) and copper(II) to form the nutrient complex during coagulation; and
wherein the nutrient complex effectively integrates into the article, thereby forming the eco-friendly wearable article which efficiently reduces or eliminates methane gas emission during landfill biodegradation of the article.

### Claim 2 (depends on 1)

The eco-friendly wearable article of claim 1, wherein the nutrient complex comprises ferrous sulphate, present in a concentration of at least 0.009 μg/cm2, cupric chloride present in a concentration of at least 0.003 μg/cm2, and magnesium sulphate present in a concentration of at least 0.083 μg/cm2.

### Claim 3 (depends on 1)

The eco-friendly wearable article according to claim 1, wherein the eco-friendly wearable article comprises an elastomeric material.

### Claim 4 (depends on 1)

The eco-friendly wearable article according to claim 1, wherein the eco-friendly wearable article is a disposable glove.

### Claim 5 (depends on 1)

A method of making an eco-friendly wearable article according to claim 1, the method comprising the steps of:
a) providing a mold of the article;
b) dipping the mold into the coagulant dipping system comprising the nutrient complex;
c) dipping the mold into an elastomeric mixture;
d) repeating steps b) and c) to form an elastomeric layer comprising the nutrient complex;
e) drying the elastomeric layer;
f) dipping the elastomeric layer into a donning coating to form a donning coated elastomeric layer;
g) curing the donning coated elastomeric layer; and,
h) drying the donning coated elastomeric layer to form the eco-friendly wearable article.

### Claim 6 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the nutrient complex comprises ferrous sulphate, present in a concentration of at least 0.009 μg/cm2, cupric chloride present in a concentration of at least 0.003 μg/cm2, and magnesium sulphate present in a concentration of at least 0.083 μg/cm2.

### Claim 7 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the method further comprises the step of spraying the elastomeric layer with a phyllosilicate clay mineral prior to drying step.

### Claim 8 (depends on 7)

The method of making the eco-friendly wearable article according to claim 7, wherein the phyllosilicate clay mineral is present in a total solid content between about 2.0% to about 4.5%.

### Claim 9 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the donning coating further comprises the nutrient complex.

### Claim 10 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the drying steps occur at a temperature from about 60° C. to about 80° C.

### Claim 11 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the curing step is at a temperature between about 100° C. to about 110° C.

### Claim 12 (depends on 5)

The method of making the eco-friendly wearable article according to claim 5, wherein the eco-friendly wearable article is a disposable glove.