# US 2022/0379539 A1 · Acrylic resin film and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0379539 A1
- Document ID: US20220379539A1
- Status: Published application
- Kind: A1
- Application number: 17/883,107
- Filed: 2022-08-08
- Published: 2022-12-01
- Earliest claimed: 2016-09-29
- Assignees: Kuraray Co., Ltd.
- Applicants: Kuraray Co., Ltd.
- Inventors: Takuro NIIMURA; Taketomo YAMASHITA; Atsuhiro NAKAHARA; Nariaki FUJII; Tomoyuki MATSUI
- Web page: https://patentgrep.com/patent/US20220379539A1

## CPC

- B32B 27/22: using plasticisers
- C08J 5/18: Manufacture of films or sheets
- B29B 9/06: in the form of filamentary material, e.g. combined with extrusion
- B29B 13/06: by drying (B29B13/08 takes precedence {; drying moulded articles or half products B29C37/0092})
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/04: Particle-shaped (making granules B29B9/00)
- B29C 48/08: flexible, e.g. films
- B29C 48/21: the layers being joined at their surfaces
- B32B 27/08: of synthetic resin
- B32B 27/18: characterised by the use of special additives
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/302: {comprising aromatic vinyl (co)polymers, e.g. styrenic (co)polymers}
- B32B 27/304: {comprising vinyl halide (co)polymers, e.g. PVC, PVDC, PVF, PVDF}
- B32B 27/306: {comprising vinyl acetate or vinyl alcohol (co)polymers}
- B32B 27/308: {comprising acrylic (co)polymers}
- B32B 27/365: {comprising polycarbonates}
- C08F 2/22: Emulsion polymerisation
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 265/06: Polymerisation of acrylate or methacrylate esters on to polymers thereof
- C08F 285/00: Macromolecular compounds obtained by polymerising monomers on to preformed graft polymers
- C08L 51/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C08L51/04, C08L51/06 take precedence)}
- B29K 2033/12: {Polymers of methacrylic acid esters, e.g. PMMA, i.e. polymethylmethacrylate}
- B29L 2007/008: {Wide strips, e.g. films, webs}
- B29L 2009/00: Layered products
- B32B 2250/02: 2 layers
- B32B 2250/03: 3 layers
- B32B 2250/24: All layers being polymeric
- B32B 2250/246: All polymers belonging to those covered by groups B32B27/32 and B32B27/30
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/412: Transparent
- B32B 2307/70: Other properties
- B32B 2307/732: Dimensional properties
- B32B 2307/736: Shrinkable
- B32B 2307/738: Thermoformability
- C08J 2333/12: Homopolymers or copolymers of methyl methacrylate
- C08J 2351/00: Characterised by the use of graft polymers in which the grafted component is obtained by reactions only involving carbon-to-carbon unsaturated bonds; Derivatives of such polymers
- C08J 2409/10: Latex (C08J2409/04, C08J2409/08 take precedence)
- C08J 2433/12: Homopolymers or copolymers of methyl methacrylate
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A resin film comprising a multilayer structure acrylic polymer and the film having an acid value of not more than 0.018 mmol/g in an acetone insoluble matter, an acid value of not more than 0.012 mmol/g in an acetone soluble matter, a glass transition temperature of not less than 80° C. and a thickness of 5 to 300 μm is obtained by a method comprising emulsion polymerization for producing a latex comprising multilayer structure acrylic polymer, coagulating the latex comprising the multilayer structure acrylic polymer to obtain a slurry, washing and dehydrating the slurry, drying the dehydrated slurry to remove the multilayer structure acrylic polymer, mixing 0 to 35% by mass of an acrylic resin and 65 to 100% by mass of the removed multilayer structure acrylic polymer and subjecting the resultant mixture melted to an extrusion molding.

## Claims

### Claim 1

A method for producing a resin film comprising a multilayer structure acrylic polymer,
wherein the resin film has an acid value of not more than 0.018 mmol/g in an acetone insoluble matter, an acid value of not more than 0.012 mmol/g in an acetone soluble matter, a glass transition temperature of not less than 80° C., a haze variation width (ΔH80) before and after a hot water whitening resistance test with water of 80° C. of 5% or less, a haze variation width (ΔH100) before and after a boiling water whitening resistance test with water of 100° C. of 5% or less, and a thickness of 5 to 300 μm, and
wherein the multilayer structure acrylic polymer comprises a polymer (a), a polymer (b) and a polymer (c), the polymer (a) is a polymer composed of 40 to 98.99% by mass of a structural unit derived from methyl methacrylate, not less than 1% by mass of a structural unit derived from an alkyl acrylate having a 1 to 8 carbon alkyl group, 0.01 to 1% by mass of a structural unit derived from a grafting agent and 0 to 0.5% by mass of a structural unit derived from a crosslinking agent;
the polymer (b) is a polymer composed of 70 to 99.5% by mass of a structural unit derived from alkyl acrylate having a 1 to 8 carbon alkyl group, 0.5 to 5% by mass of a structural unit derived from a grafting agent, 0 to 5% by mass of a structural unit derived from a crosslinking agent and the balance of a structural unit derived from methyl methacrylate; and
the polymer (c) is a polymer composed of 80 to 99% by mass of a structural unit derived from methyl methacrylate and 1 to 20% by mass of a structural unit derived from an alkyl acrylate having a 1 to 8 carbon alkyl group and has a glass transition temperature of not less than 80° C.,
the method comprising:
conducting emulsion polymerization to obtain a latex containing the multilayer structure acrylic polymer;
coagulating the latex to obtain a slurry;
washing and dewatering the slurry;
drying the dewatered slurry to isolate the multilayer structure acrylic polymer; and
melting and extrusion molding a mixture of 0 to 35% by mass of an acrylic resin and 65 to 100% by mass of the isolated multilayer structure polymer using an extruder for film formation.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising:
after the drying of the dewatered slurry to isolate the multilayer structure acrylic polymer,
feeding the isolated multilayer structure acrylic polymer to an extruder for pelletization to obtain a pelletized multilayer structure acrylic polymer; and
drying the pelletized multilayer structure acrylic polymer to be used for producing the mixture.

### Claim 3

A method for producing a resin film comprising a multilayer structure acrylic polymer,
wherein the resin film has an acid value of not more than 0.018 mmol/g in an acetone insoluble matter, an acid value of not more than 0.012 mmol/g in an acetone soluble matter, a glass transition temperature of not less than 80° C., a haze variation width (ΔH80) before and after a hot water whitening resistance test with water of 80° C. of 5% or less, a haze variation width (ΔH100) before and after a boiling water whitening resistance test with water of 100° C. of 5% or less, and a thickness of 5 to 300 μm, and
wherein the multilayer structure acrylic polymer comprises a polymer (a), a polymer (b) and a polymer (c), the polymer (a) is a polymer composed of 40 to 98.99% by mass of a structural unit derived from methyl methacrylate, not less than 1% by mass of a structural unit derived from an alkyl acrylate having a 1 to 8 carbon alkyl group, 0.01 to 1% by mass of a structural unit derived from a grafting agent and 0 to 0.5% by mass of a structural unit derived from a crosslinking agent;
the polymer (b) is a polymer composed of 70 to 99.5% by mass of a structural unit derived from an alkyl acrylate having a 1 to 8 carbon alkyl group, 0.5 to 5% by mass of a structural unit derived from a grafting agent, 0 to 5% by mass of a structural unit derived from a crosslinking agent and the balance of a structural unit derived from methyl methacrylate; and
the polymer (c) is a polymer composed of 80 to 99% by mass of a structural unit derived from methyl methacrylate and 1 to 20% by mass of a structural unit derived from an alkyl acrylate having a 1 to 8 a carbon alkyl group and has a glass transition temperature of not less than 80° C.,
the method comprising:
polymerizing 40 to 98.99% by mass of methyl methacrylate, not less than 1% by mass of an alkyl acrylate having a 1 to 8 carbon alkyl group, 0.01 to 1% by mass of a grafting agent, and 0 to 0.5% by mass of a crosslinking agent in the presence of an emulsifying agent to obtain a latex (I) containing the polymer (a);
polymerizing 70 to 99.5% by mass of an alkyl acrylate having a 1 to 8 carbon alkyl group, 0.5 to 5% by mass of a grafting agent, 0 to 5% by mass of a crosslinking agent, and the balance of methyl methacrylate in the presence of the latex (I) to obtain a latex (II) containing the polymer (a) and the polymer (b);
polymerizing 80 to 99% by mass of methyl methacrylate and 1 to 20% by mass of an alkyl acrylate having a 1 to 8 carbon alkyl group in the presence of the latex (II) to obtain a latex (III) containing the polymer (a), the polymer (b) and the polymer (c);
coagulating the latex (III) to obtain a slurry;
washing and dewatering the slurry;
drying the dewatered slurry to isolate a multilayer structure acrylic polymer comprising the polymer (a), the polymer (b) and the polymer (c); and
melting and extrusion molding a mixture of 0 to 35% by mass of an acrylic resin and 65 to 100% by mass of the isolated multilayer structure acrylic polymer using an extruder for film formation.

### Claim 4 (depends on 3)

The method according to claim 3, further comprising:
after the drying of the dewatered slurry to isolate the multilayer structure acrylic polymer comprising the polymer (a), the polymer (b) and the polymer (c),
feeding the isolated multilayer structure acrylic polymer to an extruder for pelletization to obtain a pelletized multilayer structure acrylic polymer; and
drying the pelletized multilayer structure acrylic polymer to be used for producing the mixture.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the washing and dewatering of the slurry are performed at least twice by use of a screw decanter centrifuge.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the drying of the slurry is performed so that a moisture percentage is less than 0.1% by mass.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the washing and dewatering of the slurry are repeatedly performed so that the isolated multilayer structure acrylic polymer has an acid value of not more than 0.008 mmol/g in an acetone insoluble matter and an acid value of not more than 0.012 mmol/g in an acetone soluble matter.

### Claim 8 (depends on 1)

The method according to claim 1, wherein a residence time in the extruder for film formation is 5 minutes or less, and a temperature is 280° C. or less in the extruder for film formation.

### Claim 9 (depends on 2)

The method according to claim 2, wherein the drying of the pelletized multilayer structure acrylic polymer is performed so that a moisture percentage is less than 0.1% by mass.

### Claim 10 (depends on 2)

The method according to claim 2, wherein a residence time in the extruder for pelletization is 5 minutes or less, and a temperature is 280° C. or less in the extruder for pelletization.

### Claim 11 (depends on 3)

The method according to claim 3, wherein the washing and dewatering of the slurry are performed at least twice by use of a screw decanter centrifuge.

### Claim 12 (depends on 3)

The method according to claim 3, wherein the drying of the slurry is performed so that a moisture percentage is less than 0.1% by mass.

### Claim 13 (depends on 3)

The method according to claim 3, wherein the washing and dewatering of the slurry are repeatedly performed so that the isolated multilayer structure acrylic polymer has an acid value of not more than 0.008 mmol/g in an acetone insoluble matter and an acid value of not more than 0.012 mmol/g in an acetone soluble matter.

### Claim 14 (depends on 3)

The method according to claim 3, wherein a residence time in the extruder for film formation is 5 minutes or less, and a temperature is 280° C. or less in the extruder for film formation.

### Claim 15 (depends on 4)

The method according to claim 4, wherein the drying of the pelletized multilayer structure acrylic polymer is performed so that a moisture percentage is less than 0.1% by mass.

### Claim 16 (depends on 4)

The method according to claim 4, wherein a residence time in the extruder for pelletization is 5 minutes or less, and a temperature is 280° C. or less in the extruder for pelletization.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the acrylic resin has a moisture percentage of less than 0.1% by mass.

### Claim 18 (depends on 3)

The method according to claim 3, wherein the acrylic resin has a moisture percentage of less than 0.1% by mass.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the extruder for pelletization has a vent.

### Claim 20 (depends on 4)

The method according to claim 4, wherein the extruder for pelletization has a vent.