# US 2022/0372391 A1 · Method for applying a coating onto a non-silicone hydrogel lens

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0372391 A1
- Document ID: US20220372391A1
- Status: Published application
- Kind: A1
- Application number: 17/659,972
- Filed: 2022-04-20
- Published: 2022-11-24
- Earliest claimed: 2021-04-22
- Assignees: Alcon Inc.
- Applicants: Alcon Inc.
- Inventors: Chung-Yuan Chiang; Yongxing Qiu
- Web page: https://patentgrep.com/patent/US20220372391A1

## CPC

- C08J 7/056: Forming hydrophilic coatings
- C10M 107/42: Macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- B29D 11/00038: {Production of contact lenses}
- B29D 11/00125: {Auxiliary operations, e.g. removing oxygen from the mould, conveying moulds from a storage to the production line in an inert atmosphere}
- B29D 11/00865: {Applying coatings; tinting; colouring (printing, marking or copying processes B41M; identification in general G09F3/00; producing decorative effects in general B44C; positioning or marking of lenses B24B13/0055)}
- C08J 3/245: {Differential crosslinking of one polymer with one crosslinking type, e.g. surface crosslinking}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C10M 107/28: containing monomers having an unsaturated radical bound to a carboxyl radical, e.g. acrylate
- C10M 107/48: containing phosphorus
- G02C 7/04: Contact lenses for the eyes (disinfection or sterilisation of contact lenses A61L12/00)
- B29K 2029/04: {PVOH, i.e. polyvinyl alcohol (B29K2031/04 takes precedence)}
- B29K 2105/0061: {Gel or sol}
- C08J 2329/04: Polyvinyl alcohol; Partially hydrolysed homopolymers or copolymers of esters of unsaturated alcohols with saturated carboxylic acids
- C08J 2433/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- C08J 2433/14: of esters containing halogen, nitrogen, sulfur, or oxygen atoms in addition to the carboxy oxygen
- C08J 2433/26: Homopolymers or copolymers of acrylamide or methacrylamide
- C08J 2471/03: Polyepihalohydrins
- C10M 2209/0845: used as base material
- C10M 2217/0245: used as base material
- C10M 2225/025: used as base material
- C10N 2050/023: {Multi-layer lubricant coatings}
- C10N 2070/00: Specific manufacturing methods for lubricant compositions
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- G02C: SPECTACLES; SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURES AS SPECTACLES; CONTACT LENSES (trial frames for testing the eyes A61B3/04; goggles or eyeshields not having the same features as spectacles A61F9/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

The present invention generally relates to a method for applying a coating of hydrophilic polymers onto polyvinylalcohol-based hydrogel contact lenses to improve lubricity. In particular, the present invention is directed to a method for forming a coating on a contact lens, preferably a polyvinylalcohol-based hydrogel contact lens, directly in the primary package and maintaining the coated contact lens within said primary package until insertion of the coated contact lens in the eye of the contact lens user. The resultant polyvinylalcohol-based hydrogel contact lens has a coating with improved lubricity and good durability and also can be used directly from the lens package by a patient without washing and/or rinsing.

## Claims

### Claim 1

A method for applying an ophthalmic product having a lubricious and wettable surface, comprising the steps of:
(1) obtaining a polyvinylalcohol-based hydrogel contact lens,
(2) placing the polyvinylalcohol-based hydrogel contact lens in a lens package containing an in-package-coating solution, wherein the in-package-coating solution comprises:
(A) a polyanionic polymer having carboxyl groups,
(B) Prefer at least one water-soluble and thermally-crosslinkable polymeric material comprising azetidinium groups,
(C) at least one decomposable-at-autoclave material, wherein the in-package-coating solution has a pH of from about 1.0 to about 4.0, provided that the molar charge ratio of the polyanionic polymer and the water-soluble and thermal-crosslinkable polymeric material comprising azetidinium groups is from 1:100 to 100:1 and no precipitation is formed after mixings, wherein the polyanionic polymer attaching and forming at least one layer coating on the surface of the polyvinylalcohol-based hydrogel contact lens,
(3) sealing the lens package with the contact lens and the in-package-coating solution having the pH of from about 1.0 to about 4.0,
(4) autoclaving said package with the contact lens and the in-package-coating solution therein, thereby inducing crosslinking reaction between azetidinium groups of the water-soluble polymeric material and the carboxyl groups of the polyanionic polymer to form a crosslinked hydrophilic coating on the surface of the polyvinylalcohol-based hydrogel contact lens immersed in the in-package-coating solution, wherein the decomposable-at-autoclave material is hydrolyzed to increase the pH to 6.5 to 7.5, wherein the polyvinylalcohol-based hydrogel contact lens with the crosslinked hydrophilic coating thereon has a surface having improved lubricity as compared to uncoated lenses.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polyvinylalcohol-based hydrogel contact lens is composed of a polymer comprising at least 50% by mole of repeating units of vinyl alcohol,

### Claim 3 (depends on 1)

The method of claim 1, wherein the decomposable-at-autoclave material is urea, ammonium carbamate, or combination thereof.

### Claim 4 (depends on 1, 2)

The method of claims 1 and 2, wherein the water-soluble and thermally-crosslinkable polymeric material comprises (i) from about 20% to about 95% by weight of first polymer chains derived from an epichlorohydrin-functionalized polyamine or polyamidoamine, (ii) from about 5% to about 80% by weight of hydrophilic moieties or second polymer chains derived from at least one hydrophilicity-enhancing agent having at least one reactive functional group selected from the group consisting of amino group, carboxyl group, and combination thereof.

### Claim 5 (depends on 4)

The method of claim 4, wherein the hydrophilic polymer as the hydrophilicity-enhancing agent is a copolymer which is a polymerization product of a composition comprising (1) about 60% by weight or less by weight of at least one reactive vinylic monomer and (2) at least one non-reactive hydrophilic vinylic monomer and/or at least one phosphorylcholine-containing vinylic monomer; or combinations thereof;
wherein the reactive vinylic monomer is selected from the group consisting of amino-C1-C6 alkyl (meth)acrylate, C1-C6 alkylamino-C1-C6 alkyl (meth)acrylate, allylamine, vinylamine, amino-C1-C6 alkyl (meth)acrylamide, C1-C6 alkylamino-C1-C6 alkyl (meth)acrylamide, acrylic acid, C1-C12 alkylacrylic acid, N,N-2-acrylamidoglycolic acid, beta-methyl-acrylic acid, alpha-phenyl acrylic acid, beta-acryloxy propionic acid, sorbic acid, angelic acid, cinnamic acid, 1-carobxy-4-phenyl butadiene-1,3, itaconic acid, citraconic acid, mesaconic acid, glutaconic acid, aconitic acid, maleic acid, fumaric acid, tricarboxy ethylene, and combinations thereof;
wherein the non-reactive hydrophilic vinylic monomer is selected from the group consisting of acrylamide, methacrylamide, N,N-dimethylacrylamide, N,N-dimethylmethacrylamide, N-vinylpyrrolidone, N,N,-dimethylaminoethylmethacrylate, N,N-dimethylaminoethylacrylate, N,N-dimethylaminopropylmethacrylamide, N,N-dimethylaminopropylacrylamide, glycerol methacrylate, 3-acryloylamino-1-propanol, N-hydroxyethyl acrylamide, N-[tris(hydroxymethyl)methyl]-acrylamide, N-methyl-3-methylene-2-pyrrolidone, 1-ethyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 1-ethyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, 5-ethyl-3-methylene-2-pyrrolidone, 2-hydroxyethyl (meth)acrylate, hydroxypropyl (meth)acrylate, C1-C4-alkoxy polyethylene glycol (meth)acrylate having a weight average molecular weight of up to 1500 Daltons, N-vinyl formamide, N-vinyl acetamide, N-vinyl isopropylamide, N-vinyl-N-methyl acetamide, allyl alcohol, vinyl alcohol (hydrolyzed form of vinyl acetate in the copolymer), and combinations thereof.

### Claim 6 (depends on 4)

The method of claim 4, wherein the weight average molecular weight Mw of the hydrophilic polymer as the hydrophilicity-enhancing agent is from about 500 to about 1,000,000.

### Claim 7 (depends on 1)

The method of claim 1, wherein the step of autoclaving is performed by heating the polyvinylalcohol-based hydrogel contact lens immersed in a packaging solution in a sealed lens package at a temperature of from about 118° C. to about 125° C. for approximately 20-90 minutes to form the crosslinked hydrophilic coating on the polyvinylalcohol-based hydrogel contact lens, wherein the packaging solution comprises at least one buffering agent in an amount sufficient to maintain a pH of from about 6.0 to about 8.5 and has a tonicity of from about 200 to about 450 milliosmol (mOsm) and a viscosity of from about 1 centipoise to about 20 centipoises at 25° C.

### Claim 8 (depends on 4)

The method of claim 4, wherein the molar charge ratio of the polyanionic material to the water soluble and thermal-crosslinkable hydrophilic polymeric material azetidinium groups is from 1:20 to 20:1.

### Claim 9

A method for applying an ophthalmic product having a lubricious surface, comprising the steps of:
(1) obtaining a polyvinylalcohol-based hydrogel contact lens,
(2) placing the polyvinylalcohol-based hydrogel contact lens in a lens package containing an polyanionic polymer solution for more than 10 seconds to form a layer of the polyanionic polymer coating on the hydrogel contact lens, wherein the polyanionic polymer having carboxyl groups and the solution having a pH of 1.0 to 4.0, and then
(3) adding a water-soluble and thermal-crosslinkable polymeric material comprising azetidinium groups to the lens package of the step (2) containing the polyanionic polymer solution to form an in-package-coating solution, provided that the molar charge ratio of the polyanionic polymer and the water-soluble and thermal-crosslinkable polymeric material comprising azetidinium groups is from 1:100 to 100:1 and no precipitation is formed after mixing, wherein the in-package-coating solution having a pH higher than 6,
(4) sealing the lens package with the contact lens and the in-package-coating solution,
(5) autoclaving said package with the contact lens and the in-package-coating solution therein, thereby inducing crosslinking reaction between azetidinium groups of the water-soluble and thermal-crosslinkable polymeric material and the carboxyl groups of the polyanionic polymer to form an in-package crosslinked hydrophilic coating on the surface of the polyvinylalcohol-based hydrogel contact lens, wherein the polyvinylalcohol-based hydrogel contact lens with the crosslinked hydrophilic coating thereon has a surface having improved lubricity as compared to uncoated lenses.

### Claim 10 (depends on 9)

The method of claim 9, wherein the polyvinylalcohol-based hydrogel contact lens is composed of a polymer comprising at least 50% by mole of repeating units of vinyl alcohol.

### Claim 11 (depends on 9, 10)

The method of claims 9 and 10, wherein the water-soluble and thermally-crosslinkable polymeric material comprises (i) from about 20% to about 95% by weight of first polymer chains derived from an epichlorohydrin-functionalized polyamine or polyamidoamine, (ii) from about 5% to about 80% by weight of hydrophilic moieties or second polymer chains derived from at least one hydrophilicity-enhancing agent having at least one reactive functional group selected from the group consisting of amino group, carboxyl group, and combination thereof.

### Claim 12 (depends on 11)

The method of claim 11, wherein the hydrophilic polymer as the hydrophilicity-enhancing agent is a copolymer which is a polymerization product of a composition comprising (1) about 60% by weight or less by weight of at least one reactive vinylic monomer and (2) at least one non-reactive hydrophilic vinylic monomer and/or at least one phosphorylcholine-containing vinylic monomer; or combinations thereof;
wherein the reactive vinylic monomer is selected from the group consisting of amino-C1-C6 alkyl (meth)acrylate, C1-C6 alkylamino-C1-C6 alkyl (meth)acrylate, allylamine, vinylamine, amino-C1-C6 alkyl (meth)acrylamide, C1-C6 alkylamino-C1-C6 alkyl (meth)acrylamide, acrylic acid, C1-C12 alkylacrylic acid, N,N-2-acrylamidoglycolic acid, beta-methyl-acrylic acid, alpha-phenyl acrylic acid, beta-acryloxy propionic acid, sorbic acid, angelic acid, cinnamic acid, 1-carobxy-4-phenyl butadiene-1,3, itaconic acid, citraconic acid, mesaconic acid, glutaconic acid, aconitic acid, maleic acid, fumaric acid, tricarboxy ethylene, and combinations thereof;
wherein the non-reactive hydrophilic vinylic monomer is selected from the group consisting of acrylamide, methacrylamide, N,N-dimethylacrylamide, N,N-dimethylmethacrylamide, N-vinylpyrrolidone, N,N,-dimethylaminoethylmethacrylate, N,N-dimethylaminoethylacrylate, N,N-dimethylaminopropylmethacrylamide, N,N-dimethylaminopropylacrylamide, glycerol methacrylate, 3-acryloylamino-1-propanol, N-hydroxyethyl acrylamide, N-[tris(hydroxymethyl)methyl]-acrylamide, N-methyl-3-methylene-2-pyrrolidone, 1-ethyl-3-methylene-2-pyrrolidone, 1-methyl-5-methylene-2-pyrrolidone, 1-ethyl-5-methylene-2-pyrrolidone, 5-methyl-3-methylene-2-pyrrolidone, 5-ethyl-3-methylene-2-pyrrolidone, 2-hydroxyethyl (meth)acrylate, hydroxypropyl (meth)acrylate, C1-C4-alkoxy polyethylene glycol (meth)acrylate having a weight average molecular weight of up to 1500 Daltons, N-vinyl formamide, N-vinyl acetamide, N-vinyl isopropylamide, N-vinyl-N-methyl acetamide, allyl alcohol, vinyl alcohol (hydrolyzed form of vinyl acetate in the copolymer), and combinations thereof.

### Claim 13 (depends on 11)

The method of claim 11, wherein the weight average molecular weight Mw of the hydrophilic polymer as the hydrophilicity-enhancing agent is from about 500 to about 1,000,000.

### Claim 14 (depends on 9)

The method of claim 9, wherein the step of autoclaving is performed by heating the polyvinylalcohol-based hydrogel contact lens immersed in a packaging solution in a sealed lens package at a temperature of from about 118° C. to about 125° C. for approximately 20-90 minutes to form the crosslinked hydrophilic coating on the polyvinylalcohol-based hydrogel contact lens, wherein the packaging solution comprises at least one buffering agent in an amount sufficient to maintain a pH of from about 6.0 to about 8.5 and has a tonicity of from about 200 to about 450 milliosmol (mOsm) and a viscosity of from about 1 centipoise to about 20 centipoises at 25° C.

### Claim 15 (depends on 11)

The method of claim 11, wherein the molar charge ratio of the polyanionic material to the water soluble and thermal-crosslinkable hydrophilic polymeric material azetidinium groups is from 1:20 to 20:1.