# US 2022/0349080 A1 · Method and system for depositing a zinc-nickel alloy on a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0349080 A1
- Document ID: US20220349080A1
- Status: Published application
- Kind: A1
- Application number: 17/778,104
- Filed: 2020-12-18
- Published: 2022-11-03
- Earliest claimed: 2019-12-20
- Assignees: Atotech Deutschland GmbH
- Applicants: Atotech Deutschland GmbH & Co. KG
- Inventors: Steven LEONHARD; Thomas FREESE
- Web page: https://patentgrep.com/patent/US20220349080A1

## CPC

- C25D 3/22: of zinc
- C25D 21/18: of electrolytes (C25D21/22 takes precedence)
- C25D 3/562: {containing more than 50% by weight of iron or nickel or cobalt}
- C25D 3/565: {containing more than 50% by weight of zinc}
- C25D 5/34: Pretreatment of metallic surfaces to be electroplated
- C25D 21/20: of rinse-solutions (C25D21/22 takes precedence)
- C25D 21/22: by ion-exchange
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method for depositing a zinc-nickel alloy on a substrate, including: (a) providing the substrate, (b) providing an aqueous zinc-nickel deposition bath as catholyte in a compartment, wherein the compartment includes an anode and anolyte, the anolyte being separated from catholyte by a membrane, and the catholyte includes nickel ions, complexing agent, zinc ions, (c) depositing zinc-nickel alloy onto the substrate, wherein after step (c) nickel ions have lower concentration than before step (c), (d) rinsing the zinc-nickel coated substrate in water, obtaining a rinsed zinc-nickel coated substrate and rinse water including a portion of the complexing agent and nickel ions, wherein (i) a portion of rinse water and/or a portion of catholyte is treated in a first treatment compartment to separate water from the complexing agent and the nickel ions, (ii) returning the separated complexing agent to the catholyte, and (iii) adding nickel ion to the catholyte.

## Claims

### Claim 1

A method for depositing a zinc-nickel alloy on a substrate, the method comprising the steps:
(a) providing the substrate,
(b) providing an aqueous zinc-nickel deposition bath as a catholyte in a deposition compartment, wherein
the deposition compartment comprises at least one anode with an anolyte, and
the anolyte is separated from the catholyte by at least one membrane, and
the catholyte comprises
(i) nickel ions,
(ii) at least one complexing agent for nickel ions, and
(iii) zinc ions,
(c) contacting the substrate with the catholyte in the deposition compartment such that the zinc-nickel alloy is electrolytically deposited onto the substrate and thereby obtaining a zinc-nickel coated substrate, wherein
after step (c) the nickel ions in the catholyte have a lower concentration than before step (c),
(d) rinsing the zinc-nickel coated substrate in a rinsing compartment comprising water, such that a rinsed zinc-nickel coated substrate and rinse water is obtained, wherein
the rinse water comprises a portion of the at least one complexing agent for nickel ions and a portion of the nickel ions,
characterized in that
(i) at least a portion of the rinse water and/or at least a portion of the catholyte is treated in a first treatment compartment such that water is separated from the at least one complexing agent for nickel ions and the nickel ions,
(ii) at least a portion of the at least one complexing agent separated from water is returned into the catholyte, and
(iii) a nickel ion source is added to the catholyte, with the proviso that the nickel ion source does not comprise said at least one complexing agent for nickel ions or any other complexing agent for nickel ions.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the at least one complexing agent for nickel ions is not in contact with the at least one anode.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the nickel ion source is an aqueous solution comprising water and a nickel salt dissolved therein.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the nickel ion source is essentially free of or does not comprise tetraethylenepentaamine.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in the catholyte the at least one complexing agent for nickel ions comprises an amine.

### Claim 6 (depends on 1)

The method according to claim 1, wherein step (a), prior to step (c), further comprises step
(a-1) pre-rinsing the substrate in a pre-rinsing compartment comprising water, such that a pre-rinsed substrate and pre-rinse water is obtained.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the at least one anode has a distance to the at least one membrane in a range from 0.5 mm to 5.0 mm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first treatment compartment comprises an evaporator.

### Claim 9 (depends on 1)

The method according to claim 1, wherein at least a portion of the separated water obtained in the first treatment compartment is returned into the pre-rinsing compartment and/or the rinsing compartment.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising step
(e) treating at least a portion of the catholyte in a second treatment compartment such that dissolved anions are separated from the catholyte.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the precipitation is carried out at a temperature in a range from −5° C. to 11.0° C.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the dissolved anions comprise at least sulfate anions.

### Claim 13 (depends on 1)

The method according to claim 1, wherein in the catholyte the zinc ions are present as hydroxo complexes.

### Claim 14 (depends on 1)

The method according to claim 1, wherein at least a portion of the separated water obtained in the first treatment compartment is disposed, wherein the disposed water comprises nickel ions in a concentration range from 0 mg/L to 1.0 mg/L, based on the total volume of the disposed water.

### Claim 15

A system (1) for depositing a zinc-nickel alloy on a substrate, the system (1) comprising:
(I) optionally, a pre-rinsing compartment (2) for pre-rinsing the substrate,
(II) a deposition compartment (3) for electrolytically depositing in a catholyte (3-1) the zinc-nickel alloy on the substrate such that a zinc-nickel coated substrate is obtained, wherein the deposition compartment (3) comprises at least one anode with at least one membrane (3-2),
(III) a rinsing compartment (4) for rinsing the zinc-nickel coated substrate such that a rinsed zinc-nickel coated substrate and rinse water is obtained,
(IV) a first treatment compartment (5) for treating the rinse water and a portion of the catholyte (3-1) such that water is separated from nickel ions and complexing agents for nickel ions, and
(V) optionally, a second treatment compartment (8) for treating the catholyte such that dissolved anions are separated from the catholyte,
wherein
the first treatment compartment (5) is adapted such that
the separated water is returned into the pre-rinsing compartment (2) and/or the rinsing compartment (4), and
the separated nickel ions and the separated complexing agents for nickel ions are returned into the deposition compartment (3).