# US 2022/0331857 A1 · Iron-based alloy powder containing non-spherical particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0331857 A1
- Document ID: US20220331857A1
- Status: Published application
- Kind: A1
- Application number: 17/640,808
- Filed: 2020-09-03
- Published: 2022-10-20
- Earliest claimed: 2019-09-06
- Assignees: BASF SE; Formetrix, Inc.
- Applicants: BASF SE; Formetrix, Inc.
- Inventors: Rudolf SEILER; Cecile MUELLER-WEITZEL; Matthias Johannes WAGNER; Rene ARBTER; Thorsten MArtin STAUDT; Marie-Claire HERMANT; Harald LEMKE; Jonathan TRENKLE
- Web page: https://patentgrep.com/patent/US20220331857A1

## CPC

- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B33Y 40/10: Pre-treatment
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 33/006: {compositions used for making ferrous alloys}
- C22C 33/04: by melting
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/26: with niobium or tantalum
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- B22F 10/00: Additive manufacturing of workpieces or articles from metallic powder (apparatus or devices therefor B22F12/00)
- B22F 2009/0808: {Mechanical dispersion of melt, e.g. by sieves}
- B22F 2009/0828: {with water}
- B22F 2009/084: {combination of methods}
- B22F 2009/0844: {in controlled atmosphere}
- B22F 2009/088: {Fluid nozzles, e.g. angle, distance}
- B22F 2009/0892: {casting nozzle; controlling metal stream in or after the casting nozzle}
- B22F 2301/35: Iron
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B33Y 10/00: Processes of additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to an iron-based alloy powder containing non-spherical particles wherein the alloy comprises the elements Fe (iron), Cr (chrome) and Mo (molybdenum), and at least 40% of the total amount of particles have a non-spherical shape. In said iron-based alloy powder, Cr is present at 10.0 wt. % to 18.3 wt. %, Mo is present at 0.5 wt. % to 2.5 wt. %, C is present at 0 to 0.30 wt. %, Ni is present at 0 to 4.0 wt. %, Cu is present at 0 to 4.0 wt. %, Nb is present at 0 to 0.7 wt. %, Si is present at 0 to 0.7 wt. % and N is present at 0 to 0.20 wt. %, the balance up to 100 wt. % is Fe.

## Claims

### Claim at position 1

-11. (canceled)

### Claim 12

An iron-based alloy powder containing non-spherical particles wherein the alloy comprises the elements Fe, Cr and Mo, and at least 40% of the total amount of particles have a non-spherical shape, wherein Cr is present at 10.0 wt. % to 18.3 wt. %, Mo is present at 0.5 wt. % to 2.5 wt. %, C is present at 0 to 0.30 wt. %, Ni is present at 0 to 4.0 wt. %, Cu is present at 0 to 4.0 wt. %, Nb is present at 0 to 0.7 wt. %, Si is present at 0 to 0.7 wt. % and N is present at 0 to 0.20 wt. %, the balance up to 100 wt. % is Fe, wherein the sphericity of the particles having a non-spherical shape is not more than 0.9.

### Claim 13 (depends on 12)

The iron-based alloy powder according to claim 12, wherein
(i) at least 50%, of the total amount of particles have a non-spherical shape, or
(ii) the total amount of particles having a non-spherical shape is in the range of at least 40 to 70%,.

### Claim 14 (depends on 12)

The iron-based alloy powder according to claim 12, wherein
(i) at least 70% of the total amount of particles have a non-spherical shape, or
(ii) the total amount of particles having a non-spherical shape is in the range of 45 to 60%

### Claim 15 (depends on 12)

The iron-based alloy powder according to claim 12, wherein
(i) at least 95% of the total amount of particles have a non-spherical shape, or
(ii) the total amount of particles having a non-spherical shape is in the range of 50 to 55%

### Claim 16 (depends on 12)

The iron-based alloy powder according to claim 12, wherein
(i) at least 99% of the total amount of particles have a non-spherical shape, or
(ii) the total amount of particles having a non-spherical shape is in the range of 50 to 55%.

### Claim 17 (depends on 12)

The iron-based alloy powder according to claim 12, wherein the particles have a diameter in the range of 1 to 200 microns.

### Claim 18 (depends on 12)

The iron-based alloy powder according to claim 12, wherein the particles have a diameter in the range of 3 to 70 microns.

### Claim 19 (depends on 12)

The iron-based alloy powder according to claim 12, wherein the particles have a diameter in the range of 15 to 53 microns.

### Claim 20 (depends on 12)

A process for producing an iron-based alloy powder according to claim 12, wherein the iron-based alloy powder is provided in a molten state and an atomization step is carried out with a stream of the molten iron-based alloy powder.

### Claim 21 (depends on 20)

The process according to claim 20, wherein the atomization step is carried out as an ultrahigh pressure liquid atomization by jetting at least one liquid with a pressure of at least 300 bar.

### Claim 22 (depends on 20)

The process according to claim 20, wherein the atomization step is carried out as an ultrahigh pressure liquid atomization by jetting at least one liquid with a pressure of at least 600 bar onto the stream of the molten iron-based alloy powder.

### Claim 23 (depends on 20)

The process according to claim 20, wherein the liquid contains water, and/or the ultrahigh pressure liquid atomization is carried out by an atomization process comprising at least two stages,
preferably, within a first stage of this atomization process, a stream of the molten iron-based alloy powder is fed through a nozzle into a first area located between the nozzle and a choke and a gas stream, which is preferably a nitrogen-containing gas stream and/or an inert gas stream, circulates around the molten iron-based alloy powder within this first area and, within a second stage of this atomization process, the stream of the molten iron-based alloy powder is fed to a second area located beyond the choke, where the stream of the molten iron-based alloy powder is contacted with a water-containing jet stream under a pressure of at least 300 bar, causing a break up and solidification of the stream of the molten iron-based alloy powder into the respective particles, wherein at least 50% of the total amount of the particles have a non-spherical shape.

### Claim 24 (depends on 23)

The process according to claim 23, wherein the liquid is water, and the water-containing jet stream is under a pressure of at least 600 bar.

### Claim 25 (depends on 12)

A use of at least one iron-based alloy powder according to claim 12 within a three-dimensional (3D) printing process.

### Claim 26 (depends on 12)

A process for producing a three-dimensional (3D) object wherein the 3D object is formed layer by layer and within each layer at least one iron-based alloy powder according to claim 12 is employed.

### Claim 27 (depends on 26)

The process according to claim 26, wherein in each layer the employed at least one iron-based alloy powder is molten by applying energy on the surface of the iron-based alloy powder with a laser beam,

### Claim 28 (depends on 26)

The process according to claim 26, wherein in each layer the employed at least one iron-based alloy powder is molten by applying energy on the surface of the iron-based alloy powder with an electron beam.

### Claim 29 (depends on 19)

The process according to claim 19, wherein the 3D object is produced by a selective laser melting (SLM) process,
preferably the selective laser melting (SLM) process comprises the steps (i) to (iv):
(i) applying a first layer of at least one iron-based alloy powder onto a surface,
(ii) scanning the first layer of the at least one iron-based alloy powder with a focused laser beam at a temperature sufficient to melt at least part of the first layer of the at least one iron-based alloy powder throughout its layer thickness to obtain a first molten layer,
(iii) solidifying the first molten layer obtained in step (ii),
(iv) repeating process steps (i), (ii) and (iii) with a pattern of scanning effective to form the respective 3D object or at least a part thereof.

### Claim 30 (depends on 19)

A three-dimensional (3D) object obtainable by a process according to claim 19.