# US 2022/0325056 A1 · Member for composite material, composite material, mobile body, and method for manufacturing film for composite material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0325056 A1
- Document ID: US20220325056A1
- Status: Published application
- Kind: A1
- Application number: 17/848,601
- Filed: 2022-06-24
- Published: 2022-10-13
- Earliest claimed: 2019-12-27
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Masayasu Hasuike; Hikari Wakita
- Web page: https://patentgrep.com/patent/US20220325056A1

## CPC

- C08J 5/24: Impregnating materials with prepolymers which can be polymerised in situ, e.g. manufacture of prepregs
- C08J 5/243: {using carbon fibres}
- C08J 5/042: {with carbon fibres}
- C08J 2329/12: Homopolymers or copolymers of unsaturated ketones
- C08J 2361/16: of ketones with phenols
- C08J 2365/00: Characterised by the use of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08J2307/00 - C08J2357/00, C08J2361/00 take precedence); Derivatives of such polymers
- C08J 2371/00: Characterised by the use of polyethers obtained by reactions forming an ether link in the main chain; Derivatives of such polymers
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The following is provided as a member for a composite material that has excellent stiffness, heat resistance, and productivity. A member for a composite material containing resin component that contains polyaryletherketone as a main component. The resin component has a molecular weight distribution of 3.8 or more and 8 or less and a mass average molecular weight of 86000 or less. The member for a composite material has a thickness more than 15 μm. The composite material contains a resin and reinforcing fibers having a number average fiber length of 5 mm or more.

## Claims

### Claim 1

A multilayer body, comprising
a first layer comprising a resin containing polyaryletherketone as a main component, and
a second layer comprising reinforcing fibers having a number average fiber length of 5 mm or more,
wherein the resin has a molecular weight distribution of 3.8 or more and 8 or less and a mass average molecular weight of 86000 or less,
wherein the first layer has a thickness more than 15 μm.

### Claim 2 (depends on 1)

The multilayer body according to claim 1,
wherein the polyaryletherketone comprises polyetheretherketone.

### Claim 3 (depends on 1)

The multilayer body according to claim 1,
wherein a percentage of a content of the polyaryletherketone in the resin is more than 90 mass %.

### Claim 4 (depends on 1)

The multilayer body according to claim 1,
wherein the polyaryletherketone has the molecular weight distribution of 3.8 or more and 8 or less and the mass average molecular weight of 86000 or less.

### Claim 5 (depends on 1)

The multilayer body according to claim 1,
wherein the first layer has a crystal heat of fusion of 43 J/g or more and 60 J/g or less.

### Claim 6 (depends on 1)

The multilayer body according to claim 1,
wherein the first layer has a crystallization temperature of 299° C. or more and 320° C. or less.

### Claim 7 (depends on 1)

The multilayer body according to claim 1,
wherein a tensile modulus of the first layer measured at a tension rate of 5 mm/minute is 3450 MPa or more and 5000 MPa or less.

### Claim 8 (depends on 1)

The multilayer body according to claim 1,
wherein the first layer has a thickness accuracy of 7% or less.

### Claim 9 (depends on 1)

The multilayer body according to claim 1,
wherein at least one surface of the first layer has an arithmetic mean height of 0.001 to 1 μm.

### Claim 10 (depends on 1)

The multilayer body according to claim 1,
wherein at least one surface of the first layer has a maximum height of 0.1 to 10 μm.

### Claim 11 (depends on 1)

The multilayer body according to claim 1,
wherein at least one surface of the first layer has an arithmetic mean roughness of 0.005 to 1 μm.

### Claim 12 (depends on 1)

The multilayer body according to claim 1,
wherein at least one surface of the first layer has a maximum height roughness of 0.05 to 5 μm.

### Claim 13 (depends on 1)

The multilayer body according to claim 1,
wherein the first layer has a relative crystallinity of 50% or more.

### Claim 14 (depends on 1)

The multilayer body according to claim 1,
wherein the first layer is a film.

### Claim 15 (depends on 1)

A composite material obtained by molding the multilayer body according to claim 1.

### Claim 16 (depends on 15)

The composite material according to claim 15,
wherein the composite material is a prepreg.

### Claim 17 (depends on 15)

A mobile body comprising the composite material according to claim 15,
wherein the mobile body is an airplane, an automobile, a ship, or a railroad vehicle.

### Claim 18

A multilayer body comprising
a first layer comprising a resin comprising polyaryletherketone as a main component, and
a second layer comprising reinforcing fibers having a number average fiber length of 5 mm or more,
wherein the resin has a molecular weight distribution of 3.8 or more and 8 or less and a mass average molecular weight of 86000 or less,
wherein the first layer is a plate-shaped member, and
wherein the plate-shaped member has a thickness more than 15 μm.

### Claim 19 (depends on 18)

The multilayer body according to claim 18,
wherein the polyaryletherketone comprises polyetheretherketone.

### Claim 20 (depends on 18)

The multilayer body according to claim 18,
wherein the plate-shaped member is a film.

### Claim 21

A method for manufacturing a multilayer body comprising a first layer containing a resin comprising polyaryletherketone as a main component and a second layer comprising reinforcing fibers having a number average fiber length of 5 mm or more, the method comprising:
preparing the resin having a molecular weight distribution of 3.8 or more and 8 or less and a mass average molecular weight of 86000 or less;
melt kneading the resin using an extruder;
extruding the melted resin from a mouthpiece; and cooling the melted resin using a casting roller to form the melted resin into a film,
wherein a crystallization temperature of the film is 299° C. or more and 320° C. or less, and a tensile modulus of the cooled film measured at a tension rate of 5 mm/minute is 3450 MPa or more and 5000 MPa or less.

### Claim 22 (depends on 21)

The method for manufacturing a multilayer body according to claim 21,
wherein the polyaryletherketone has the molecular weight distribution of 3.8 or more and 8 or less and the mass average molecular weight of 86000 or less.