# US 2022/0324065 A1 · Aluminum alloys for fluxless brazing applications, methods of making the same, and uses thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0324065 A1
- Document ID: US20220324065A1
- Status: Published application
- Kind: A1
- Application number: 17/594,957
- Filed: 2020-04-20
- Published: 2022-10-13
- Earliest claimed: 2019-05-19
- Assignees: Novelis Inc.
- Applicants: Novelis Inc.
- Inventors: Jyothi Kadali
- Web page: https://patentgrep.com/patent/US20220324065A1

## CPC

- B23K 35/288: {with Sn or Zn}
- B22D 7/005: {from non-ferrous metals}
- B22D 7/02: Casting compound ingots of two or more different metals in the molten state, i.e. integrally cast
- B22D 11/003: {Aluminium alloys}
- B22D 11/007: {of composite ingots, i.e. two or more molten metals of different compositions being used to integrally cast the ingots (casting of composite ingots in definite lengths B22D7/02)}
- B22D 11/008: {of clad ingots, i.e. the molten metal being cast against a continuous strip forming part of the cast product}
- B22D 11/049: for direct chill casting, e.g. electromagnetic casting
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B23K 1/0012: {Brazing of heat exchangers}
- B23K 35/0238: {layered}
- B23K 35/286: {Al as the principal constituent}
- B32B 15/016: {all layers being formed of aluminium or aluminium alloys}
- C22C 21/00: Alloys based on aluminium
- C22C 21/02: with silicon as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- F28F 21/084: {from aluminium or aluminium alloys}
- F28F 21/089: {Coatings, claddings or bonding layers made from metals or metal alloys (F28F19/06 takes precedence)}
- B23K 2101/14: Heat exchangers
- B23K 2103/10: Aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)

## Abstract

Provided are new aluminum alloys for use as one or more cladding layer(s) in clad aluminum alloy products for brazing applications. The cladding layer(s) include constituents that break and remove the oxide film on metal parts to be joined to produce high-strength brazing joints without the use of corrosive flux. Also provided herein are corrosion-resistant aluminum sheet packages including one or more of the aluminum alloy cladding layer(s) and an aluminum alloy core.

## Claims

### Claim 1

A aluminum alloy comprising 7.0-14.0 wt. % Si, 0.05-1.0 wt. % Fe, 0.01-0.60 wt. % Cu, 0.01-0.30 wt. % Mn, 0.01-0.50 wt. % Mg, 0.0-0.60 wt. % Zn, 0.001-0.50 wt. % Bi, up to 0.30 wt. % Sb, up to 0.20 wt. % Sr, up to 0.20 wt. % Na, up to 0.25 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 2 (depends on 1)

The aluminum alloy of claim 1, comprising 8.0-12.0 wt. % Si, 0.10-0.90 wt. % Fe, 0.01-0.50 wt. % Cu, 0.05-0.20 wt. % Mn, 0.01-0.40 wt. % Mg, 0.05-0.40 wt. % Zn, 0.01-0.40 wt. % Bi, up to 0.25 wt. % Sb, up to 0.15 wt. % Sr, up to 0.10 wt. % Na, up to 0.20 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 3 (depends on 1)

The aluminum alloy of claim 1, comprising 8.5-11.0 wt. % Si, 0.15-0.50 wt. % Fe, 0.01-0.40 wt. % Cu, 0.05-0.15 wt. % Mn, 0.05-0.30 wt. % Mg, 0.10-0.30 wt. % Zn, 0.05-0.30 wt. % Bi, up to 0.20 wt. % Sb, up to 0.10 wt. % Sr, up to 0.06 wt. % Na, up to 0.15 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 4 (depends on 1)

The aluminum alloy of claim 1, comprising 9.0-10.5 wt. % Si, 0.15-0.25 wt. % Fe, 0.30-0.40 wt. % Cu, 0.05-0.15 wt. % Mn, 0.15-0.30 wt. % Mg, 0.15-0.30 wt. % Zn, 0.10-0.35 wt. % Bi, up to 0.15 wt. % Sb, up to 0.05 wt. % Sr, up to 0.05 wt. % Na, up to 0.10 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 5 (depends on 1)

The aluminum alloy of claim 1, comprising 9.5-10.5 wt. % Si, 0.30-0.50 wt. % Fe, 0.01-0.05 wt. % Cu, 0.05-0.15 wt. % Mn, 0.01-0.05 wt. % Mg, 0.20-0.25 wt. % Zn, 0.10-0.20 wt. % Bi, 0.01-0.05 wt. % Sb, 0.001-0.02 wt. % Sr, up to 0.01 wt. % Na, up to 0.10 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 6 (depends on 1)

The aluminum alloy of claim 1 any of claims 1, wherein the aluminum alloy is produced by direct chill casting, followed by hot rolling and cold rolling.

### Claim 7 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy comprises a corrosion potential of 660-720 mV or less, measured after brazing.

### Claim 8 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy withstands at least 28 days without perforation during airside corrosion testing after brazing.

### Claim 9

A clad aluminum alloy product, comprising:
a core layer; and
at least one cladding layer comprising the aluminum alloy of claim.

### Claim 10 (depends on 9)

The clad aluminum alloy product of claim 9, wherein the core layer comprises an aluminum alloy comprising up to 0.25 wt. % Si, up to 0.35 wt. % Fe, 0.50 wt. % to 0.60 wt. % Cu, 1.4 wt. % to 1.6 wt. % Mn, 0.06 wt. % to 0.62 wt. % Mg, up to 0.05 wt. % Cr, up to 0.04 wt. % Zn, 0.10 wt. % to 0.20 wt. % Ti, up to 0.05 wt. % Sr, up to 0.15 wt. % of impurities, and Al.

### Claim 11

A clad aluminum alloy product, comprising:
a core layer, wherein the core layer has a first side and a second side;
at least one cladding layer on the first side or the second side;
wherein the at least one cladding layer comprises 7.0-14.0 wt. % Si, 0.05-1.0 wt. % Fe, 0.01-0.60 wt. % Cu, 0.01-0.30 wt. % Mn, 0.01-0.50 wt. % Mg, 0.0-0.60 wt. % Zn, 0.001-0.50 wt. % Bi, up to 0.30 wt. % Sb, up to 0.20 wt. % Sr, up to 0.20 wt. % Na, up to 0.25 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 12 (depends on 11)

The clad aluminum alloy product of claim 11, wherein the core layer comprises an aluminum alloy comprising up to 0.25 wt. % Si, up to 0.35 wt. % Fe, 0.50 wt. % to 0.60 wt. % Cu, 1.4 wt. % to 1.6 wt. % Mn, 0.06 wt. % to 0.62 wt. % Mg, up to 0.05 wt. % Cr, up to 0.04 wt. % Zn, 0.10 wt. % to 0.20 wt. % Ti, up to 0.05 wt. % Sr, up to 0.15 wt. % of impurities, and Al.

### Claim 13 (depends on 11)

A corrosion resistant brazing sheet comprising the clad aluminum alloy product of claim 11.

### Claim 14 (depends on 11)

A heat exchanger comprising the clad aluminum alloy product of claim 11.

### Claim 15

A method of forming a brazing joint, comprising the steps of:
providing one or more metal parts;
providing a clad aluminum alloy product on or between the one or more metal parts to form an assembly, wherein the clad aluminum alloy product comprises at least one cladding layer;
brazing the assembly without applying flux to join the clad aluminum alloy product and the one or more metal parts to produce a brazed assembly; and
cooling the brazed assembly, wherein the at least one cladding layer comprises 7.0-14.0 wt. % Si, 0.05-1.0 wt. % Fe, 0.01-0.60 wt. % Cu, 0.01-0.30 wt. % Mn, 0.01-0.50 wt. % Mg, 0.0-0.60 wt. % Zn, 0.001-0.50 wt. % Bi, up to 0.30 wt. % Sb, up to 0.20 wt. % Sr, up to 0.20 wt. % Na, up to 0.25 wt. % Ti, up to 0.15 wt. % of impurities, and Al.

### Claim 16 (depends on 15)

The method of claim 15, wherein brazing occurs in a controlled atmosphere brazing furnace comprising an inert gas, wherein the controlled atmosphere brazing furnace comprises less than 100 ppm oxygen.

### Claim 17 (depends on 16)

The method of claim 16, wherein the controlled atmosphere brazing furnace has a dew point of less than —40° C.

### Claim 18 (depends on 16)

The method of claim 16, wherein the assembly is brazed at a brazing temperature from 590° C. to 610° C., wherein the controlled atmosphere brazing furnace is heated to the brazing temperature in less than five minutes.

### Claim 19 (depends on 16)

The method of claim 16, wherein the assembly is brazed for 3 minutes at 600° C. in the controlled atmosphere brazing furnace having an oxygen concentration less than 50 ppm and a dew point less than —40° C. in a nitrogen atmosphere.

### Claim 20 (depends on 15)

The method of claim 15, wherein the at least one cladding layer comprises 8.0-12.0 wt. % Si, 0.10-0.90 wt. % Fe, 0.01-0.50 wt. % Cu, 0.05-0.20 wt. % Mn, 0.01-0.40 wt. % Mg, 0.10- 0.40 wt. % Zn, 0.01-0.40 wt. % Bi, up to 0.25 wt. % Sb, up to 0.15 wt. % Sr, up to 0.06 wt. % Na, up to 0.15 wt. % Ti, and up to 0.15 wt. % of impurities, and Al.