- Number: US 2022/0319740 A1
- Document ID: US20220319740A1
- Status: Published application
- Kind: A1
- Application number: 17/609,362
- Filed: 2019-05-21
- Published: 2022-10-06
- Earliest claimed: 2019-05-21
- Assignees: SuperOx Japan LLC
- Applicants: SuperOx Japan LLC
- Inventors: Valery PETRYKIN; Sergey LI
- Web page: https://patentgrep.com/patent/US20220319740A1

## CPC

- H01B 12/06: Films or wires on bases or cores
- H10N 60/0632: {Intermediate layers, e.g. for growth control}
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/081: {of aluminium, magnesium or beryllium}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/221: {Ion beam deposition (C23C14/46, C23C14/48 take precedence)}
- C23C 14/351: {using a magnetic field in close vicinity to the substrate}
- C23C 14/544: {using measurement in the gas phase}
- C23C 14/562: {for coating elongated substrates}
- Y02E 40/60: Superconducting electric elements or equipment; Power systems integrating superconducting elements or equipment
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of fabricating a superconducting wire includes forming a buffer layer on the substrate, the buffer layer including an Al2O3 layer, the Al2O3 layer being formed by reactive magnetron sputtering in which first oxygen gas as reactant gas and a sputtering target made of aluminium metal are used, the Al2O3 layer being formed while being supplied the first oxygen gas at a first concentration, the first concentration being a concentration of the first oxygen gas at which an emission intensity of Al in plasma near a surface of the sputtering target is not less than 25% and not more than 80% of a first reference value, the first reference value being the emission intensity of Al at which the concentration of the first oxygen gas is zero; and forming a superconducting layer above the buffer layer.

## Claims

### Claim 1

A method of fabricating a superconducting wire, comprising:
forming a buffer layer on the substrate, the buffer layer comprising an Al2O3 layer, the Al2O3 layer being formed by reactive magnetron sputtering in which first oxygen gas as reactant gas and a sputtering target made of aluminium metal are used, the Al2O3 layer being formed while being supplied the first oxygen gas at a first concentration, the first concentration being a concentration of the first oxygen gas at which an emission intensity of Al in plasma near a surface of the sputtering target is not less than 25% and not more than 80% of a first reference value, the first reference value being the emission intensity of Al at which the concentration of the first oxygen gas is zero; and
forming a superconducting layer above the buffer layer.

### Claim 2 (depends on 1)

The method of fabricating a superconducting wire according to claim 1, wherein
the first concentration is the concentration of the first oxygen gas at which the emission intensity of Al is not less than 30% and not more than 80% of the first reference value.

### Claim 3 (depends on 1)

The method of fabricating a superconducting wire according to claim 1, wherein
the buffer layer comprises an Y2O3 layer on the Al2O3 layer, the Y2O3 layer being formed by reactive magnetron sputtering in which second oxygen gas as reactant gas and a sputtering target made of yttrium metal are used, the Y2O3 layer being formed while being supplied the second oxygen gas at a second concentration, the second concentration being a concentration of the second oxygen gas at which an emission intensity of Y in plasma near a surface of the sputtering target is not less than 15% and not more than 90% of a second reference value, the second reference value being the emission intensity of Y at which the concentration of the second oxygen gas is zero.

### Claim 4 (depends on 3)

The method of fabricating a superconducting wire according to claim 3, wherein
the second concentration is the concentration of the second oxygen gas at which the emission intensity of Y is not less than 30% and not more than 80% of the second reference value.

### Claim 5 (depends on 3)

The method of fabricating a superconducting wire according to claim 3, wherein
the buffer layer comprises an MgO layer having a biaxially textured structure on the Y2O3 layer, the MgO layer being formed by reactive magnetron sputtering in which third oxygen gas as reactant gas and a sputtering target made of magnesium metal are used and assisting Ar ion beam is applied, the MgO layer being formed while being supplied the third oxygen gas at a third concentration, the third concentration being a concentration of the third oxygen gas at which an emission intensity of Mg in plasma near a surface of the sputtering target is less than 50% of a third reference value, the third reference value being the emission intensity of Mg at which the concentration of the third oxygen gas is zero.

### Claim 6 (depends on 3)

The method of fabricating a superconducting wire according to claim 3, wherein
the buffer layer comprises an MgO layer having a biaxially textured structure on the Y2O3 layer, the MgO layer being formed by magnetron sputtering in which a sputtering target made of MgO is used and assisting Ar ion beam is applied.

### Claim 7

A method of fabricating a superconducting wire, comprising:
forming a buffer layer on the substrate, the buffer layer comprising an Y2O3 layer, the Y2O3 layer being formed by reactive magnetron sputtering in which second oxygen gas as reactant gas and a sputtering target made of yttrium metal are used, the Y2O3 layer being formed while being supplied the second oxygen gas at a second concentration, the second concentration being a concentration of the second oxygen gas at which an emission intensity of Y in plasma near a surface of the sputtering target is not less than 15% and not more than 90% of a second reference value, the second reference value being the emission intensity of Y at which the concentration of the second oxygen gas is zero; and
forming a superconducting layer above the buffer layer.

### Claim 8 (depends on 7)

The method of fabricating a superconducting wire according to claim 7, wherein
the second concentration is the concentration of the second oxygen gas at which the emission intensity of Y is not less than 30% and not more than 80% of the second reference value.

### Claim 9 (depends on 7)

The method of fabricating a superconducting wire according to claim 7, wherein
the buffer layer comprises an MgO layer having a biaxially textured structure on the Y2O3 layer, the MgO layer being formed by reactive magnetron sputtering in which third oxygen gas as reactant gas and a sputtering target made of magnesium metal are used and assisting Ar ion beam is applied, the MgO layer being formed while being supplied the third oxygen gas at a third concentration, the third concentration being a concentration of the third oxygen gas at which an emission intensity of Mg in plasma near a surface of the sputtering target is less than 50% of a third reference value, the third reference value being the emission intensity of Mg at which the concentration of the third oxygen gas is zero.

### Claim 10 (depends on 7)

The method of fabricating a superconducting wire according to claim 7, wherein
the buffer layer comprises an MgO layer having a biaxially textured structure on the Y2O3 layer, the MgO layer being formed by magnetron sputtering in which a sputtering target made of MgO is used and assisting Ar ion beam is applied.

### Claim 11

A method of fabricating a superconducting wire, comprising:
forming a buffer layer on the substrate, the buffer layer comprising an MgO layer, the MgO layer being formed by reactive magnetron sputtering in which third oxygen gas as reactant gas and a sputtering target made of magnesium metal are used and to which ion beam assisted deposition is applied, the MgO layer being formed while being supplied the third oxygen gas at a third concentration, the third concentration being a concentration of the third oxygen gas at which an emission intensity of Mg in plasma near a surface of the sputtering target is less than 50% of a third reference value, the third reference value being the emission intensity of Mg at which the concentration of the third oxygen gas is zero; and
forming a superconducting layer above the buffer layer.