# US 2022/0295644 A1 · Bonded body, ceramic copper circuit board, method for manufacturing bonded body, and method for manufacturing ceramic copper circuit board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0295644 A1
- Document ID: US20220295644A1
- Status: Published application
- Kind: A1
- Application number: 17/826,464
- Filed: 2022-05-27
- Published: 2022-09-15
- Earliest claimed: 2020-03-18
- Assignees: Kabushiki Kaisha Toshiba; Toshiba Materials Co., Ltd.
- Applicants: Kabushiki Kaisha Toshiba; Toshiba Materials Co., Ltd.
- Inventors: Maki YONETSU; Seiichi SUENAGA; Sachiko FUJISAWA; Takashi SANO
- Web page: https://patentgrep.com/patent/US20220295644A1

## CPC

- H05K 3/388: {by the use of a metallic or inorganic thin film adhesion layer}
- H05K 1/0306: {Inorganic insulating substrates, e.g. ceramic, glass}
- H05K 1/09: Use of materials for the {conductive, e.g. } metallic pattern
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W 40/258: {Metallic materials (H10W40/254, H10W40/257, H10W40/255, H10W40/251, H10W40/253 take precedence)}
- H05K 1/0271: {Arrangements for reducing stress or warp in rigid printed circuit boards, e.g. caused by loads, vibrations or differences in thermal expansion}
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- H05K 2201/0266: Size distribution
- H05K 2203/04: Soldering or other types of metallurgic bonding
- H10W 70/635: {Through-vias}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A bonded body includes a ceramic substrate and a copper plate, in which the copper plate is bonded to the ceramic substrate via a bonding layer, the copper plate includes a surface perpendicular to a direction in which the ceramic substrate and the copper plate are bonded, and a number percentage of copper crystal grains having major diameters greater than 400 μm in three 5 mm×5 mm regions included in the surface is not less than 0% and not more than 5%. The bonding temperature is favorably not more than 800° C. The number percentage of the copper crystal grains having major diameters greater than 400 μm is favorably not more than 1%.

## Claims

### Claim 1

A bonded body, comprising:
a ceramic substrate; and
a copper plate bonded to the ceramic substrate via a bonding layer,
the copper plate including a surface perpendicular to a direction in which the ceramic substrate and the copper plate are bonded,
a number percentage of copper crystal grains having major diameters greater than 400 μm in three 5 mm×5 mm regions included in the surface being not less than 0% and not more than 5%.

### Claim 2 (depends on 1)

The body according to claim 1, wherein
the number percentage is not more than 1%.

### Claim 3 (depends on 1)

The body according to claim 1, wherein
an average value of the major diameters of the copper crystal grains in the three regions is not less than 30 μm and not more than 300 μm.

### Claim 4 (depends on 1)

The body according to claim 1, wherein
an average value of the major diameters of the copper crystal grains in the three regions is not less than 50 μm and not more than 150 μm.

### Claim 5 (depends on 1)

The body according to claim 1, wherein
a number percentage of the copper crystal grains having major diameters within an average range in the three regions is not less than 80%, and
the average range is not less than 0.5 times and not more than 2 times an average value of the major diameters of the copper crystal grains in the three regions.

### Claim 6 (depends on 1)

The body according to claim 1, wherein
an arithmetic average height Wa of a waviness curve of the ceramic substrate is not more than 2 μm, and
a maximum cross-sectional height Wt of the waviness curve is not more than 10 μm.

### Claim 7 (depends on 1)

The body according to claim 1, wherein
the bonding layer includes Ag, Cu, and Ti.

### Claim 8 (depends on 1)

The body according to claim 1, wherein
the ceramic substrate is one of a silicon nitride substrate or an aluminum nitride substrate.

### Claim 9 (depends on 1)

The body according to claim 1, wherein
an average value of the major diameters of the copper crystal grains in the three regions is not less than 30 μm and not more than 300 μm,
a number percentage of the copper crystal grains having major diameters within an average range in the three regions is not less than 80%, and
the average range is not less than 0.5 times and not more than 2 times an average value of the major diameters of the copper crystal grains in the three regions.

### Claim 10 (depends on 9)

The body according to claim 9, wherein
an arithmetic average height Wa of a waviness curve of the ceramic substrate is not more than 2 μm, and
a maximum cross-sectional height Wt of the waviness curve is not more than 10 μm.

### Claim 11 (depends on 10)

The body according to claim 10, wherein
the bonding layer includes Ag, Cu, and Ti.

### Claim 12 (depends on 11)

The body according to claim 11, wherein
the ceramic substrate is one of a silicon nitride substrate or an aluminum nitride substrate.

### Claim 13 (depends on 1)

A ceramic copper circuit board using the bonded body according to claim 1.

### Claim 14 (depends on 1)

A method for manufacturing the bonded body according to claim 1, the method comprising:
a process of disposing a brazing material used as the bonding layer between the ceramic substrate and the copper plate; and
a bonding process including a bonding temperature of not more than 800° C.

### Claim 15 (depends on 14)

The method according to claim 14, wherein
the bonding temperature is not more than 700° C.

### Claim 16 (depends on 14)

The method according to claim 14, wherein
B/A≤10 is satisfied,
A (μm) is an average grain size of the copper plate before bonding, and
B (μm) is an average grain size of the copper plate after bonding.

### Claim 17 (depends on 16)

The method according to claim 16, wherein
1.1≤B/A≤5 is satisfied.

### Claim 18 (depends on 14)

The method according to claim 14, wherein
a largest endothermic peak of a DSC curve of the brazing material is at not more than 700° C.

### Claim 19 (depends on 1)

A method for manufacturing a ceramic copper circuit board, the method comprising:
a method for manufacturing the bonded body according to claim 1; and
a process of providing a circuit structure in the bonded copper plate.