# US 2022/0295602 A1 · Flexible heating element, fabrication method therefor, flexible heating assembly thereof, and aerosol generator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0295602 A1
- Document ID: US20220295602A1
- Status: Published application
- Kind: A1
- Application number: 17/829,646
- Filed: 2022-06-01
- Published: 2022-09-15
- Earliest claimed: 2019-12-20
- Assignees: Shenzhen Smoore Technology Limited
- Applicants: Shenzhen Smoore Technology Limited
- Inventors: Hongming ZHOU; Zhenqian CHENG; Junjie XIAO
- Web page: https://patentgrep.com/patent/US20220295602A1

## CPC

- H05B 3/36: heating conductor embedded in insulating material
- A24F 40/46: Shape or structure of electric heating means
- A24F 40/70: Manufacture
- H05B 3/10: Heating elements characterised by the composition or nature of the materials or by the arrangement of the conductor
- H05B 3/12: characterised by the composition or nature of the conductive material
- H05B 3/34: flexible, e.g. heating nets or webs
- H05B 3/42: non-flexible
- A24F 40/20: Devices using solid inhalable precursors
- H05B 2203/003: using serpentine layout
- H05B 2203/013: Heaters using resistive films or coatings
- H05B 2203/017: Manufacturing methods or apparatus for heaters
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL
- A24F: SMOKERS' REQUISITES; MATCH BOXES; SIMULATED SMOKING DEVICES (inhaling appliances for medical purposes, shaped like cigars, cigarettes or pipes A61M15/06)

## Abstract

A flexible heating body includes: a sheet-shaped flexible base; at least one heating circuit disposed on the base; a conductive circuit disposed on the base and connected to both ends of the at least one heating circuit; and a flexible protective film covering the at least one heating circuit. In an embodiment, the at least one heating circuit, the conductive circuit, or the protective film are all formed by magnetron sputtering coating.

## Claims

### Claim 1

A flexible heating body, comprising:
a sheet-shaped flexible base;
at least one heating circuit disposed on the base;
a conductive circuit disposed on the base and connected to both ends of the at least one heating circuit; and
a flexible protective film covering the at least one heating circuit.

### Claim 2 (depends on 1)

The heating body of claim 1, wherein the at least one heating circuit, the conductive circuit, or the protective film are all formed by magnetron sputtering coating.

### Claim 3 (depends on 1)

The heating body of claim 1, wherein the base comprises at least one of aluminosilicate fiber paper, a PI film, or a casting ceramic piece.

### Claim 4 (depends on 1)

The heating body of claim 1, wherein the protective film comprises at least one of a casting piece, a nitride ceramic material, or an oxide ceramic material, and
wherein a thermal expansion coefficient of the protective film matches a thermal expansion coefficient of the base.

### Claim 5 (depends on 1)

The heating body of claim 1, wherein the protective film comprises at least one of a ZrO2 composite film, an Al2O3 composite film, a SiO2 composite film, or a Si3N4 composite film prepared through direct current or radio frequency magnetron sputtering, and
wherein a thickness of the protective film is 100 nm to 1000 nm.

### Claim 6 (depends on 1)

The heating body of claim 1, wherein a thickness of the heating circuit is from 1 μm to 3.5 μm, and a thickness of the conductive circuit is from 1 μm to 5 μm.

### Claim 7 (depends on 1)

The heating body of claim 1, further comprising:
an electrode lead connected to the conductive circuit.

### Claim 8 (depends on 1)

The heating body of claim 1, wherein the heating circuit comprises a transition layer disposed on the base and a heating layer disposed on the transition layer.

### Claim 9 (depends on 8)

The heating body of claim 8, wherein the transition layer comprises at least one of Cr, ZrNi, or TiN, and
wherein the heating layer comprises at least one of Pt, AgPd, AuPd, PtRu, PtRh, NiCr, or NiCrAlY.

### Claim 10 (depends on 1)

The heating body of claim 1, wherein the conductive circuit comprises a bottom layer disposed on the base, an intermediate buffer layer disposed on the bottom layer, and a conductive layer disposed on the intermediate buffer layer.

### Claim 11 (depends on 10)

The heating body of claim 10, wherein the bottom layer comprises at least one of pure Ti or pure Ni,
wherein the intermediate buffer layer comprises at least one of pure Ti or pure Ni, and
wherein the conductive layer comprises at least one of Au, Ag, or Cu.

### Claim 12

A manufacturing method for a flexible heating body, comprising:
S1: providing a sheet-shaped flexible base, and putting the base into a coating machine cavity;
S2: performing magnetron sputtering on the base to form at least one heating circuit;
S3: performing magnetron sputtering on the base to form a conductive circuit; and
S4: performing magnetron sputtering on the at least one heating circuit to form a protective film.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein in S 1, after being wiped and cleaned with alcohol, the base is placed in a coating machine cavity, the coating machine cavity is vacuumized and preheated, and a surface of the base is ion-cleaned; and
in S4, argon and oxygen in a ratio of 1:1 are introduced until a working air pressure in the cavity is 0.4 Pa; a SiO2 target power supply, a ZrO2 target power supply, an Al2O3 target power supply, or a Si3N4 target power supply is turned on; and sputtering is performed at a power density of from 2 W/cm2 to 6 W/cm2 and at a range from a room temperature to 500° C. to form the protective film with a thickness of from 100 nm to 1000 nm.

### Claim 14 (depends on 12)

The manufacturing method of claim 12, wherein S2 comprises:
performing magnetron sputtering on the base to form a transition layer; and
performing magnetron sputtering on the transition layer to form a heating layer.

### Claim 15 (depends on 14)

The manufacturing method of claim 14, wherein in S2, argon is introduced until a working air pressure in the cavity is 0.5 Pa; a Cr target power supply, a ZrNi target power supply, or a TiN target power supply is turned on; and a film is coated on the base for 5 minutes to 15 minutes at a power density of from 6 W/cm2 to 8 W/cm2 and at a room temperature to form the transition layer with a thickness of from 10 nm to 200 nm; and
wherein the Cr target power supply, the ZrNi target power supply, or the TiN target power supply is turned off; a NiCr target power supply, a NiCrAlY target power supply, a Pt target power supply, an AgPd target power supply, an AuPd target power supply, a PtRu target power supply, or a PtRh target power supply is turned on; and a film is coated on the transition layer for 60 minutes to 120 minutes at a power density of from 6 W/cm2 to 8 W/cm2 and at a room temperature to form the heating layer with a thickness of from 1 μm to 2.5 μm.

### Claim 16 (depends on 12)

The manufacturing method of claim 12, wherein S3 comprises:
performing magnetron sputtering on the base to form a bottom layer;
performing magnetron sputtering on the bottom layer to form an intermediate buffer layer;
performing magnetron sputtering on the intermediate buffer layer to form a conductive layer; and
soldering an electrode lead on the conductive layer to form a conductive electrode.

### Claim 17 (depends on 16)

The manufacturing method of claim 16, wherein in S2, argon is introduced until a working air pressure in the cavity is 0.5 Pa; a Titanium target or a Nickel target power supply is turned on; and a film is coated on the base for 5 minutes to 10 minutes at a power density of 6 W/cm2 to 8 W/cm2 and at a room temperature to form the bottom layer,
wherein the Titanium target power supply or the Nickel target power supply is turned off, then the Nickel target power supply or the Titanium target power supply is turned on, and a film is coated on the bottom layer for 10 minutes to 30 minutes at the power density of from 6 W/cm2 to 8 W/cm2 and at the room temperature to form the intermediate buffer layer, and
wherein then the Nickel target power supply or the Titanium target power supply is turned off; a silver target power supply, a copper target power supply, or a gold target power supply is turned on; and a film is coated on the intermediate buffer layer for 30 minutes to 120 minutes at a power density of from 4 W/cm2 to 8 W/cm2 at a room temperature to form the conductive layer.

### Claim 18 (depends on 1)

A flexible heating element, comprising:
the heating body of claim 1; and
an aerosol-generating substrate coated on a surface of a side of the heating body on which the at least one heating circuit is disposed,
wherein the heating element is in a shape of a spiral cylinder.

### Claim 19 (depends on 18)

The heating element of claim 18, wherein the aerosol-generating substrate comprises an aerosol-generating substrate to which a viscous substance is added, and
wherein a thickness of the aerosol-generating substrate is 0.5 mm to 1 mm.

### Claim 20 (depends on 1)

An aerosol generator, comprising:
the heating body of claim 1.