# US 2022/0294087 A1 · Method for producing secondary battery, and secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0294087 A1
- Document ID: US20220294087A1
- Status: Published application
- Kind: A1
- Application number: 17/635,887
- Filed: 2020-07-01
- Published: 2022-09-15
- Earliest claimed: 2019-09-30
- Assignees: Sanyo Electric Co., Ltd.
- Applicants: SANYO Electric Co., Ltd.
- Inventors: Tomoharu ARAI; Shinichirou YOSHIDA; Tetsuya OKADO; Masashi MURAOKA; Atsushi MIYAZAKI
- Web page: https://patentgrep.com/patent/US20220294087A1

## CPC

- B23K 11/115: {by means of two electrodes placed opposite one another on both sides of the welded parts}
- H01M 50/536: characterised by the method of fixing the leads to the electrodes, e.g. by welding
- B23K 11/14: Projection welding
- B23K 11/18: of non-ferrous metals (B23K11/20 takes precedence)
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/04: Construction or manufacture in general (H01M10/058, H01M10/12, H01M10/28, H01M10/38 take precedence)
- B23K 11/002: {specially adapted for particular articles or work}
- B23K 2101/36: Electric or electronic devices
- B23K 2101/38: Conductors
- B23K 2103/12: Copper or alloys thereof
- B23K 2103/166: {Multilayered materials}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a secondary battery according to the present invention comprises a step wherein a negative electrode collector, which has a projection having a height of from 0.36 mm to 0.45 mm on at least one of a first member and a second member, said members constituting the negative electrode collector, is resistance-welded with a core multilayer part in such a manner that the core multilayer part is sandwiched between the first member and the second member, while having the projection in contact with the core multilayer part.

## Claims

### Claim 1

A method for manufacturing a secondary battery including an electrode assembly and a negative electrode current collector, the electrode assembly including a positive electrode, a negative electrode, and a separator, and formed by stacking the positive electrode and the negative electrode with the separator interposed therebetween,
the negative electrode including a negative electrode core made of a copper foil having a surface roughness of from 0 μm to 2.0 μm and a glossiness of from 50 to 350, and a negative electrode mixture layer formed on a surface of the negative electrode core except for an exposure region where a surface of the negative electrode core is exposed,
the electrode assembly including a core stacked portion formed by stacking a plurality of the exposure regions of the negative electrode,
the negative electrode current collector including a projection having a height of from 0.36 mm to 0.45 mm on at least one of a first member and a second member constituting the negative electrode current collector,
the method for manufacturing the secondary battery, comprising:
resistance-welding the negative electrode current collector and the core stacked portion in a state where the core stacked portion is sandwiched between the first member and the second member from both sides and the projection is in contact with the core stacked portion.

### Claim 2 (depends on 1)

The method for manufacturing the secondary battery according to claim 1, wherein
the core stacked portion is formed by stacking at least forty layers of the negative electrode core.

### Claim 3 (depends on 1)

The method for manufacturing the secondary battery according to claim 1, wherein
the projection is formed in a rounded-hill shape having a diameter of from 1.41 mm to 1.49 mm.

### Claim 4 (depends on 1)

The method for manufacturing the secondary battery according to claim 1, wherein
a recess portion having a diameter of from 1.10 mm to 1.30 mm is formed on at least one of the first member and the second member at a position overlapping the projection on a surface opposite to a surface on which the projection is formed.

### Claim 5 (depends on 1)

The method for manufacturing the secondary battery according to claim 1, further comprising:
disposing an insulating sheet including a hole having a diameter of from 4.1 mm to 4.3 mm between the core stacked portion and the negative electrode current collector; and
resistance-welding the core stacked portion and the negative electrode current collector through the hole of the insulating sheet.

### Claim 6

A secondary battery including an electrode assembly and a negative electrode current collector, the electrode assembly including a positive electrode, a negative electrode, and a separator, and formed by stacking the positive electrode and the negative electrode with the separator interposed therebetween, wherein
the negative electrode includes a negative electrode core made of a copper foil having a surface roughness of 2.0 μm or less and a glossiness of from 50 to 350, and a negative electrode mixture layer formed on a surface of the negative electrode core except for an exposure region where a surface of the negative electrode core is exposed,
the electrode assembly includes a core stacked portion formed by stacking a plurality of the exposure regions of the negative electrode,
the core stacked portion is sandwiched between a first member and a second member, which constitute the negative electrode current collector, from both sides, and welded with the first member and the second member to obtain a nugget formed by the welding, and
no void having a length of at least 1.0 mm is present at an interface between the core stacked portion and the negative electrode current collector, while a maximum diameter of the nugget is at least 1.6 mm.

### Claim 7 (depends on 6)

The secondary battery according to claim 6, wherein
a ratio of a contact length between the negative electrode current collector and the nugget relative to the maximum length of the nugget is at least 40%.