# US 2022/0294037 A1 · Method for manufacturing secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0294037 A1
- Document ID: US20220294037A1
- Status: Published application
- Kind: A1
- Application number: 17/637,703
- Filed: 2020-09-22
- Published: 2022-09-15
- Earliest claimed: 2019-09-23
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Young Jae KIM; Jung Woo YOO; Ye Lin KIM
- Web page: https://patentgrep.com/patent/US20220294037A1

## CPC

- H01M 10/446: {Initial charging measures}
- H01M 4/0447: {of complete cells or cells stacks}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 10/052: Li-accumulators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- H01M 10/52: Removing gases inside the secondary cell, e.g. by absorption (vent plugs or other mechanical arrangements for facilitating escape of gases H01M50/30)
- H01M 50/30: Arrangements for facilitating escape of gases
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/624: {Electric conductive fillers}
- H01M 10/058: Construction or manufacture
- H01M 50/317: Re-sealable arrangements
- H01M 2004/027: {Negative electrodes}
- H01M 2010/4292: {Aspects relating to capacity ratio of electrodes/electrolyte or anode/cathode}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for manufacturing a secondary battery including: forming an electrode assembly including a negative electrode including a silicon-based active material, a positive electrode facing the negative electrode, and a separator between the negative electrode and the positive electrode; impregnating the electrode assembly by injecting an electrolytic solution into the electrode assembly to form an impregnated electrode assembly; performing activation through first charging/discharging in at least one cycle while pressurizing the impregnated electrode assembly to form an activated electrode assembly; allowing the activated electrode assembly to stand at 40° C. to 80° C. in a state of being charged to a SOC of 70% or more; removing a gas generated from the electrode assembly after allowing the activated electrode assembly to stand; and subjecting the electrode assembly to a second charging/discharging in at least one cycle at 15° C. to 30° C. after the removing of gas generated from the electrode assembly.

## Claims

### Claim 1

A method for manufacturing a secondary battery, the method comprising:
forming an electrode assembly comprising a negative electrode comprising a silicon-based active material, a positive electrode facing the negative electrode, and a separator interposed between the negative electrode and the positive electrode;
impregnating the electrode assembly by injecting an electrolyte solution into the electrode assembly to form an impregnated electrode assembly;
activating the impregnated electrode assembly by performing a first charging/discharging in at least one cycle while pressurizing the impregnated electrode assembly to form an activated electrode assembly;
allowing the activated electrode assembly to stand at a temperature ranging from 40° C. to 80° C. in a state of being charged to a SOC of 70% or higher;
removing a gas generated from the electrode assembly after allowing the activated electrode assembly to stand; and
performing a second charging/discharging on the electrode assembly at a temperature ranging from 15° C. to 30° C. in at least one cycle after the removing of gas generated from the electrode assembly.

### Claim 2 (depends on 1)

The method of claim 1, wherein the impregnating of the electrode assembly is performed at a temperature ranging from 15° C. to 30° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the impregnating of the electrode assembly is performed for a time range of 12 hours to 48 hours.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first charging/discharging is performed in two or more cycles.

### Claim 5 (depends on 1)

The method of claim 1, wherein the pressurization in the first charging/discharging is performed in a range of 1.5 MPa to 3.5 MPa.

### Claim 6 (depends on 1)

The method of claim 1, wherein the second charging/discharging is performed while pressurizing the electrode assembly.

### Claim 7 (depends on 1)

The method of claim 1, wherein the standing is performed for a time range of 12 hours to 36 hours.

### Claim 8 (depends on 1)

The method of claim 1, wherein the silicon-based active material is Si.

### Claim 9 (depends on 1)

The method of claim 1, wherein the negative electrode comprises a negative electrode current collector, and a negative electrode active material layer on a surface of the negative electrode current collector, and the negative electrode active material layer comprises the silicon-based active material, a binder, and a conductive material.

### Claim 10 (depends on 9)

The method of claim 9, wherein the silicon-based active material is present in an amount of 60 wt % to 90 wt % in the negative electrode active material layer,
the binder is present in an amount of 5 wt % to 30 wt % in the negative electrode active material layer, and
the conductive material is present in an amount of 5 wt % to 20 wt % in the negative electrode active material layer.

### Claim 11 (depends on 9)

The method of claim 9, wherein the negative electrode active material layer has a thickness of 35 μm to 50 μm.

### Claim 12 (depends on 1)

The method of claim 1, wherein an N/P ratio of the electrode assembly calculated by the following Equation 1 is 1.5 to 3.5:
N/P ratio=Discharge capacity per unit area of the negative electrode/Discharge capacity per unit area of the positive electrode. [Equation 1]