# US 2022/0294024 A1 · Method for manufacturing secondary battery and equipment for manufacturing the secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0294024 A1
- Document ID: US20220294024A1
- Status: Published application
- Kind: A1
- Application number: 17/770,581
- Filed: 2020-07-01
- Published: 2022-09-15
- Earliest claimed: 2019-11-19
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Hyun Jun CHOI; Soon Ju CHOI; Seok Koo KIM; Young Deok KIM; Dae Soo KIM
- Web page: https://patentgrep.com/patent/US20220294024A1

## CPC

- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 10/0404: {Machines for assembling batteries}
- H01M 10/0463: {Cells or batteries with horizontal or inclined electrodes}
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/44: Methods for charging or discharging (circuits for charging H02J7/00)
- H01M 10/446: {Initial charging measures}
- H01M 10/52: Removing gases inside the secondary cell, e.g. by absorption (vent plugs or other mechanical arrangements for facilitating escape of gases H01M50/30)
- H01M 10/052: Li-accumulators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Discussed is a method for manufacturing a secondary battery, the method including an operation (a) of alternately stacking an electrode and a separator to manufacture an electrode assembly; an operation (b) of laminating the electrode assembly at a pressure of 5 kgf/cm2 or more to bond the electrode and the separator, which are provided in the electrode assembly, to each other; an operation (c) of accommodating the electrode assembly in a battery case and injecting an electrolyte into the battery case to seal the battery case, thereby manufacturing a preliminary battery; an operation (d) of charging and discharging the preliminary battery to activate the preliminary battery; and an operation (e) of aging the preliminary battery at a high temperature of 60° C. to 100° C. for 1 hour to 6 hours to thermally treat the preliminary battery.

## Claims

### Claim 1

A method for manufacturing a secondary battery, the method comprising:
an operation (a) of alternately stacking an electrode and a separator to manufacture an electrode assembly;
an operation (b) of laminating the electrode assembly at a pressure of 5 kgf/cm2 or more to bond the electrode and the separator, which are provided in the electrode assembly, to each other;
an operation (c) of accommodating the electrode assembly in a battery case and injecting an electrolyte into the battery case to seal the battery case, thereby manufacturing a preliminary battery;
an operation (d) of charging and discharging the preliminary battery to activate the preliminary battery; and
an operation (e) of aging the preliminary battery at a temperature of 60° C. to 100° C. for 1 hour to 6 hours to thermally treat the preliminary battery.

### Claim 2 (depends on 1)

The method of claim 1, wherein, in operation (e), the temperature aging is performed for 1 hour to 3 hours.

### Claim 3 (depends on 1)

The method of claim 1, wherein, in operation (e), the temperature aging is performed at a temperature of 75° C. to 90° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein operation (d) comprises a process of charging and discharging the preliminary battery one or more times and a degassing process.

### Claim 5 (depends on 4)

The method of claim 4, wherein the degassing process is further performed by the temperature aging.

### Claim 6 (depends on 1)

The method of claim 1, wherein operation (d) comprises:
a process (d1) of primarily charging the preliminary battery;
a process (d2) of primarily aging the primarily charged preliminary battery at room temperature of 23° C. to 27° C.;
a process (d3) of primarily aging the preliminary battery at a temperature of 50° C. to 80° C. after the process (d2);
a process (d4) of secondarily aging the preliminary battery at room temperature of 23° C. to 27° C. after the process (d3); and
a process (d5) of primarily discharging the preliminary battery after the process (d4).

### Claim 7 (depends on 6)

The method of claim 6, further comprising an additional degassing process between the process (d4) and the process (d5).

### Claim 8 (depends on 7)

The method of claim 7, wherein the additional degassing process comprises a process of opening the battery case of the preliminary battery and a process of sealing the battery case again.

### Claim 9 (depends on 6)

The method of claim 6, wherein the process (d1) is performed from SOC 10 to SOC 100.

### Claim 10 (depends on 6)

The method of claim 6, wherein the process (d2) is performed for 1 day to 5 days.

### Claim 11 (depends on 6)

The method of claim 6, wherein the process (d3) is performed for 10 hours to 30 hours.

### Claim 12 (depends on 6)

The method of claim 6, wherein the process (d4) is performed for 10 hours to 30 days.

### Claim 13 (depends on 6)

The method of claim 6, wherein the process (d5) is performed to be discharged to 6.5 C for 1 minute at SOC 90.

### Claim 14

An equipment for manufacturing a secondary battery, the equipment comprising:
an electrode assembly manufacturing device configured to manufacture an electrode assembly by alternately stacking an electrode and a separator;
a lamination device configured to laminate the electrode assembly at a pressure of 5 kgf/cm2 or more so as to bond the electrode and the separator to each other;
a preliminary battery manufacturing device configured to accommodate the electrode assembly and an electrolyte in a battery case so as to manufacture a preliminary battery;
an activation device configured to charge and discharge the preliminary battery so as to activate the preliminary battery; and
a heat treatment device configured to age the preliminary battery at a temperature of 60° C. to 100° C. for 1 hour to 6 hours so as to manufacture the secondary battery.