# US 2022/0294005 A1 · A process for preparing a composite anode for lithium ion cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0294005 A1
- Document ID: US20220294005A1
- Status: Published application
- Kind: A1
- Application number: 17/636,363
- Filed: 2020-07-07
- Published: 2022-09-15
- Earliest claimed: 2019-08-20
- Assignees: Indian Space Research Organisation
- Applicants: Indian Space Research Organisation
- Inventors: Aravamuthan S; TD MERCY; John BIBIN
- Web page: https://patentgrep.com/patent/US20220294005A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/364: {as mixtures}
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/623: {fluorinated polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application provides a process for preparing a composite anode for a lithium ion cell comprising the steps of: (i) forming an anode slurry in a planetary mixing machine by mixing active materials, a binder and a solvent; (ii) coating the slurry over a copper foil substrate in a coating machine at a speed of 0.3-1.0 m/min; and (iii) calendering of the anode in a calendering machine at a temperature of 50-150° C. The lithium ion cell with the anode disclosed in this invention and a cathode exhibited a capacity retention of >80% at 100% depth-of-discharge at C/2-1C charge-discharge rate when tested for 2000 cycles.

## Claims

### Claim 1

A process for preparing a composite anode for a lithium ion cell comprising the steps of:
i. forming an anode slurry in a planetary mixing machine by mixing active materials, a binder and a solvent;
ii. coating the slurry over a copper foil substrate in a coating machine at a speed of 0.3-1.0 m/min; and
iii. calendering of the anode in a calendering machine at a temperature of 50-150° C.

### Claim 2 (depends on 1)

The process as claimed in claim 1, comprises drying the ingredients prior to mixing in the planetary mixing machine.

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein step (i) is performed by dry mixing the active materials, followed by the addition of binder solution and then the solvent.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the active material is a mixture of spherical graphite and flaky graphite.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the binder is selected from polyvinylidene fluoride, poly (vinylidene fluoride-co-hexafluoropropylene).

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein the solvent is selected from 1-methyl-2-pyrrolidinone, dimethyl acetamide (DMAC), dimethyl formamide (DMF).

### Claim 7 (depends on 1)

The process as claimed in claim 1, wherein the amount of spherical graphite is in the range of 30 to 40 wt % based on the total weight of the anode slurry.

### Claim 8 (depends on 1)

The process as claimed in claim 1, wherein the amount of flaky graphite is in the range of 5 to 15 wt % based on the total weight of the anode slurry.

### Claim 9 (depends on 1)

The process as claimed in claim 1, wherein the amount of binder is in the range of 1 to 15 wt % based on the total weight of the anode slurry.

### Claim 10 (depends on 1)

The process as claimed in claim 1, wherein the amount of solvent is in the range of 45 to 55 wt % based on the total weight of the anode slurry.

### Claim 11 (depends on 1)

The process as claimed in claim 1, wherein the copper foil substrate has a thickness in the range of 8 to 15 μm.

### Claim 12 (depends on 1)

The process as claimed in claim 1, wherein the thickness of the anode after coating is in the range of 200 to 300 μm.

### Claim 13 (depends on 1)

The process as claimed in claim 1, wherein the final thickness of the anode after calendering is in the range of 100 to 200 μm.

### Claim 14 (depends on 1)

The process as claimed in claim 1, wherein the relative humidity of the process environment in which the electrode processing is carried out is in the range of 2 to 15%.

### Claim 15 (depends on 1)

The process as claimed in claim 1, comprises drying the anode in a drying zone after coating at a temperature in the range of 50 to 150° C.

### Claim 16 (depends on 1)

The process as claimed in claim 1, wherein the calendering of the anode is performed at a speed of 0.5 to 3 m/min, and at a temperature in the range of 50-150° C.