# US 2022/0294004 A1 · Method of manufacturing composite anode for lithium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0294004 A1
- Document ID: US20220294004A1
- Status: Published application
- Kind: A1
- Application number: 17/480,241
- Filed: 2021-09-21
- Published: 2022-09-15
- Earliest claimed: 2021-03-11
- Assignees: Hyundai Motor Company; Kia Corporation; Ulsan National Institute of Science and Technology
- Applicants: Hyundai Motor Company; Kia Corporation; Ulsan National Institute of Science and Technology
- Inventors: Jong Chan Song; Won Keun Kim; Jae Wook Shin; Sung Hee Shin; Kyoung Han Ryu; Seong Min Ha; Seok Ju Kang; Kyung Eun Baek
- Web page: https://patentgrep.com/patent/US20220294004A1

## CPC

- H01M 10/058: Construction or manufacture
- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed are a method of manufacturing a composite anode for a lithium ion battery and a composite anode for a lithium ion battery manufactured thereby. According to the method provide herein, since a metal catalyst precursor is reduced using Joule heating to obtain a carbon-metal catalyst composite layer, composite anode for a lithium ion battery having a large area in a short period of time can be provided, which is excellent in terms of economic feasibility. Further, since it is possible to manufacture a composite anode for a lithium ion battery with the improved lithium electrodeposition density and reversibility of lithium ions, a composite anode for a lithium ion battery having high capacity and improved life stability can be obtained.

## Claims

### Claim 1

A method of manufacturing a composite anode for a lithium ion battery, comprising:
heat treating a carbon-supplying layer so that a surface of the carbon-supplying layer is modified to obtain a carbon-modified layer;
adding a metal catalyst precursor solution to the carbon-modified layer;
heating the carbon-modified layer to which the metal catalyst precursor solution is added, to obtain a carbon-metal catalyst composite layer; and
impregnating lithium metal on one surface of the carbon-metal catalyst composite layer to form an impregnation layer having a predetermined thickness.

### Claim 2 (depends on 1)

The method of claim 1, wherein the carbon-supplying layer comprises one or more selected from the group consisting of carbon paper, carbon cloth, carbon felt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the heat treating is performed at a temperature of 400 to 500° C. for 4 to 6 hours.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal catalyst precursor solution comprises one or more selected from the group consisting of silver nitrate (AgNO3), platinum chloride (PtCl2), iron chloride (FeCl3), palladium chloride (PdCl2), ruthenium chloride (RuCl2), nickel chloride (NiCl2), and copper chloride (CuCl2).

### Claim 5 (depends on 1)

The method of claim 1, wherein the second heating is performed on the carbon-modified layer to which the metal catalyst precursor solution is added in an inert gas atmosphere at a current of 25 A to 35 A for 1 to 5 seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carbon-metal catalyst composite layer comprises an amount of 85 to 95 wt % of the carbon-modified layer and an amount of 5 to 15 wt % of a metal catalyst based on 100 wt % of the carbon-metal catalyst composite layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the impregnation layer has a thickness of 100 to 200 um.

### Claim 8

A composite anode for a lithium ion battery comprising:
a carbon-metal catalyst composite layer in which a metal catalyst is carried in a carbon-modified layer; and
an impregnation layer on one surface of the carbon-metal catalyst composite layer, wherein the impregnation layer has a predetermined thickness and which is impregnated with lithium metal.

### Claim 9 (depends on 8)

The composite anode of claim 8, wherein the carbon-metal catalyst composite layer comprises an amount of 85 to 95 wt % of the carbon-modified layer and an amount of 5 to 15 wt % of the metal catalyst based on 100 wt % of carbon-metal catalyst composite layer.

### Claim 10 (depends on 8)

The composite anode of claim 8, wherein the impregnation layer has a thickness of 100 to 200 um.

### Claim 11 (depends on 8)

A lithium ion battery comprising:
a composite anode for the lithium ion battery of claim 8;
an electrolyte membrane located on the composite anode for the lithium ion battery; and
a cathode located on the electrolyte membrane.

### Claim 12 (depends on 11)

The lithium ion battery of claim 11, wherein an impregnation layer is located in the composite anode for the lithium ion battery so as to come into contact with the electrolyte membrane.