# US 2022/0293989 A1 · Highly reinforced ionomer membranes for high selectivity and high strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293989 A1
- Document ID: US20220293989A1
- Status: Published application
- Kind: A1
- Application number: 17/829,597
- Filed: 2022-06-01
- Published: 2022-09-15
- Earliest claimed: 2017-06-15
- Assignees: W. L. Gore & Associates, Inc.; W. L. Gore & Associates G.K.
- Applicants: W. L. Gore & Associates, Inc.; W. L. Gore & Associates G.K.
- Inventors: Takeyuki Suzuki; Alexander Agapov; Mark Edmundson
- Web page: https://patentgrep.com/patent/US20220293989A1

## CPC

- H01M 8/1039: halogenated, e.g. sulfonated polyvinylidene fluorides
- B01D 69/106: {Membranes in the pores of a support, e.g. polymerized in the pores or voids}
- B01D 69/1071: {Woven, non-woven or net mesh}
- B01D 69/1213: {Laminated layers}
- B01D 71/32: containing fluorine atoms
- B01D 71/82: characterised by the presence of specified groups, e.g. introduced by chemical after-treatment
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- H01M 8/1053: consisting of layers of polymers with at least one layer being ionically conductive
- H01M 8/1062: characterised by the physical properties of the porous support, e.g. its porosity or thickness
- H01M 8/1067: characterised by their physical properties, e.g. porosity, ionic conductivity or thickness
- B01D 2323/46: Impregnation
- B01D 2325/04: Characteristic thickness
- B01D 2325/14: Membrane materials having negatively charged functional groups
- B01D 2325/42: Ion-exchange membranes
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Embodiments are directed to composite membranes having: increased volume of the microporous polymer structure relative to the total volume of the PEM; decreased permeance and thus increased selectivity; and lower ionomer content. An increased amount of polymers of the microporous polymer structure is mixed with a low equivalent weight ionomer (e.g., <460 cc/mole eq) to obtain a composite material having at least two distinct materials. Various embodiments provide a composite membrane comprising a microporous polymer structure that occupies from 13 vol % to 65 vol % of a total volume of the composite membrane, and an ionomer impregnated in the microporous polymer structure. The acid content of the composite membrane is 1.2 meq/cc to 3.5 meq/cc, and/or the thickness of the composite membrane is less than 17 microns. The selectivity of the composite membrane is greater than 0.05 MPa/mV, based on proton conductance and hydrogen permeance.

## Claims

### Claim 1

A composite membrane, comprising:
a) a microporous polymer structure present in an amount from 13 vol % to 65 vol % based on the total volume of the composite membrane; and
b) an ion exchange material at least partially embedded within the microporous polymer structure and rendering the microporous polymer structure occlusive;
wherein a thickness of the composite membrane is below 17 micrometers while an acid content of the composite membrane is between 1.2 meq/cm3 to 3.5 meq/cm3, wherein the composite membrane has an acid content and a thickness determined at 0% relative humidity.

### Claim 2 (depends on 1)

The composite membrane of claim 1, wherein the ion exchange material has an equivalent volume equal to or less than 460 cm3/mole eq at 0% relative humidity.

### Claim 3 (depends on 1)

The composite membrane of claim 1, wherein the ion exchange material has an equivalent volume greater than 460 cm3/mole eq at 0% relative humidity.

### Claim 4 (depends on 1)

The composite membrane as in claim 1, wherein the composite membrane has a selectivity of greater than 0.05 MPa/mV.

### Claim 5 (depends on 1)

The composite membrane as in claim 1, wherein the ion exchange material may be selected from the group comprising perfluorosulfonic acid polymers, perfluorocarboxylic acid polymers, perfluorophosphonic acid polymers, styrenic ion exchange polymers, fluorostyrenic ion exchange polymers, polyarylether ketone ion exchange polymers, polysulfone ion exchange polymers, bis(fluoroalkylsulfonyl)imides, (fluoroalkylsulfonyl)(fluorosulfonyl)imides, polyvinyl alcohol, polyethylene oxides, divinyl benzene, metal salts with or without a polymer, and mixtures thereof

### Claim 6 (depends on 1)

A method for forming a composite membrane as in claim 1, wherein the microporous polymer structure is fully imbibed with ion exchange material and the composite membrane further comprises two additional layers of ion exchange material, the method comprising:
providing a support structure;
applying a first ionomer solution as a layer of controlled thickness to the support structure in a single or multiple pass ionomer coating technique, in which the first ionomer solution comprises an ion exchange material dissolved in a solvent;
laminating an untreated microporous polymer structure over at least a portion of the first ionomer solution to provide a treated microporous polymer structure;
drying the treated microporous polymer structure to provide a dried composite material in which the ion exchange material is securely adhered to the internal membrane surfaces of the microporous polymer structure;
coating a second ionomer solution over the dried composite material as a layer of controlled thickness in a single or multipass ionomer coating technique to provide a structure, in which the second ionomer solution comprises an ion exchange material dissolved in a solvent;
drying the structure to provide the composite membrane.

### Claim 7 (depends on 6)

The method as in claim 6 wherein the support structure is:
a woven material selected from scrims made of woven fibers of expanded porous polytetrafluoroethylene, webs made of extruded or oriented polypropylene or polypropylene netting, and woven materials of polypropylene and polyester; or
a non-woven material selected from a spun-bonded polypropylene; or
a web of polyethylene (“PE”), polystyrene (“PS”), cyclic olefin copolymer (“COC”), cyclic olefin polymer (“COP”), fluorinated ethylene propylene (“FEP”), perfluoroalkoxy alkanes (“PFAs”), ethylene tetrafluoroethylene (“ETFE”), polyvinylidene fluoride (“PVDF”), polyetherimide (“PEI”), polysulfone (“PSU”), polyethersulfone (“PES”), polyphenylene oxide (“PPO”), polyphenyl ether (“PPE”), polymethylpentene (“PMP”), polyethyleneterephthalate (“PET”), or polycarbonate (“PC”).

### Claim 8 (depends on 6)

The method as in claim 6 wherein the support structure further comprises a protective layer selected from polyethylene (PE), polystyrene (“PS”), cyclic olefin copolymer (“COC”), cyclic olefin polymer (“COP”), fluorinated ethylene propylene (“FEP”), perfluoroalkoxy alkanes (“PFAs”), ethylene tetrafluoroethylene (“ETFE”), polyvinylidene fluoride (“PVDF”), polyetherimide (“PEI”), polysulfone (“PSU”), polyethersulfone (“PES”), polyphenylene oxide (“PPO”), polyphenyl ether (“PPE”), polymethylpentene (“PMP”), polyethyleneterephthalate (“PET”), or polycarbonate (“PC”).

### Claim 9 (depends on 6)

The method as in claim 6 wherein the support structure further includes a reflective layer including a metal substrate.

### Claim 10 (depends on 6)

The method as in claim 6 wherein the single or multipass ionomer coating technique is selected from forward roll coating, reverse roll coating, gravure coating, doctor coating, kiss coating, slot die coating, slide die coating, dipping, brushing, painting, and spraying.

### Claim 11 (depends on 6)

The method as in claim 6 wherein the drying comprises heating in an oven at a temperature greater than 60° C.

### Claim 12 (depends on 6)

The method as in claim 6, wherein:
the second ionomer solution is the same as the first ionomer solution; or
the second ionomer solution is different than the first ionomer solution.

### Claim 13 (depends on 6)

The method as in claim 6, wherein the mass per unit area of the composite membrane is greater than 0.2 g/m2 at 0% relative humidity.

### Claim 14 (depends on 1)

A method for forming a composite membrane as in claim 1, wherein two microporous polymer structures are in contact with each other and are fully imbibed with ion exchange material and the composite membrane further comprises two additional layers of ion exchange material, the method comprising:
providing a support structure;
applying a first ionomer solution as a layer of controlled thickness to the support structure in a single or multiple pass ionomer coating technique, in which the first ionomer solution comprises an ion exchange material dissolved in a solvent;
laminating a first untreated microporous polymer structure over a first a portion of the first ionomer solution and a second untreated microporous polymer structure over the same portion of the first ionomer solution on top of the first untreated microporous polymer structure to provide a treated microporous polymer structure;
drying the treated microporous polymer structure to provide a dried composite material in which the ion exchange material is securely adhered to the internal membrane surfaces of the microporous polymer structures;
coating a second ionomer solution over the dried composite material as a layer of controlled thickness in a single or multipass ionomer coating technique to provide a coated structure, in which the second ionomer solution comprises an ion exchange material dissolved in a solvent;
drying the coated structure to provide the composite membrane.

### Claim 15 (depends on 14)

The method as in claim 14, wherein the first and second untreated porous polymer structures comprise ePTFE having a microporous polymer structure.

### Claim 16 (depends on 14)

The method as in claim 14, wherein:
the second untreated polymer structure is the same as the first untreated polymer structure; or
the second untreated polymer structure is different from the first untreated polymer structure.

### Claim 17 (depends on 1)

A method for forming a composite membrane as in claim 1, the composite membrane having two microporous polymer structures each fully imbibed with ion exchange material that are separated from each other by a layer of ion exchange material, the composite membrane further comprising two additional layers of ion exchange material, the method comprising:
providing a support structure;
applying a first ionomer solution as a layer of controlled thickness to the support structure in a single or multiple pass ionomer coating technique, in which the first ionomer solution comprises an ion exchange material dissolved in a solvent;
laminating a first untreated microporous polymer structure over at least a portion of the first ionomer solution to provide a first treated microporous polymer structure;
drying the first treated microporous polymer structure to provide a first dried composite material in which the ion exchange material is securely adhered to the internal membrane surfaces of the microporous polymer structure;
coating a second ionomer solution over the first dried composite material as a layer of controlled thickness in a single or multipass ionomer coating technique, in which the second ionomer solution comprises an ion exchange material dissolved in a solvent;
laminating a second untreated microporous polymer structure over at least a portion of the second ionomer solution to provide a second treated microporous polymer structure;
drying the second treated microporous polymer structure to provide a second dried composite material in which the ion exchange material is securely adhered to the internal membrane surfaces of the second microporous polymer structure;
coating a third ionomer solution over the dried second microporous polymer structure as a layer of controlled thickness in a single or multipass ionomer coating technique to provide a third treated microporous polymer structure, in which the third ionomer solution comprises an ion exchange material dissolved in a solvent;
drying the third treated microporous polymer structure to provide the composite membrane.

### Claim 18 (depends on 17)

The method as in claim 17, wherein the second untreated porous polymer structure comprises ePTFE having a microporous polymer structure.

### Claim 19 (depends on 17)

The method as in claim 17, wherein:
the second untreated polymer structure is the same as the first untreated polymer structure; or
the second untreated polymer structure is different from the first untreated polymer structure.

### Claim 20 (depends on 17)

The method as in claim 17, wherein:
the third ionomer solution is the same as the first and/or second ionomer solutions; or