# US 2022/0293948 A1 · A nonaqueous electrolyte secondary battery and a method for manufacturing the nonaqueous electrolyte secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293948 A1
- Document ID: US20220293948A1
- Status: Published application
- Kind: A1
- Application number: 17/770,572
- Filed: 2018-10-30
- Published: 2022-09-15
- Earliest claimed: 2018-10-30
- Applicants: ATTACCATO Limited Liability Company; The Japan Steel Works, Ltd.
- Inventors: Takashi MUKAI; Yuta IKEUCHI; Taichi SAKAMOTO; Naoto YAMASHITA; Ryou ISHIGURO; Satoru NAKAMURA
- Web page: https://patentgrep.com/patent/US20220293948A1

## CPC

- H01M 4/622: {being polymers}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/381: {Alkaline or alkaline earth metals elements (H01M4/40 takes precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/058: Construction or manufacture
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

Characteristics of a battery are improved. The nonaqueous electrolyte secondary battery of the present application includes a positive electrode, a negative electrode, a separator disposed between the positive electrode and the negative electrode, and an electrolyte solution. The positive electrode has a positive electrode active material and a binder for positive electrode. Then, the positive electrode active material has at least an alkali metal element as a constituent element, and the binder for positive electrode has cellulose and a solvent, and carbon dioxide gas is dissolved in the solvent. Further, a part or all of the surface of the positive electrode active material is coated with the cellulose, and a carbonate compound of the alkali metal element is coated on a part or all of the surface of the cellulose. According to such a configuration, it is possible to improve the characteristics of the battery, such as suppression of decrease in carbonic acid concentration due to carbonic acid vaporization, suppression of decrease in battery characteristics, suppression of oxidative decomposition of cellulose fibers, suppression of swelling of active material layer, and active decomposition of alkali metal carbonate.

## Claims

### Claim 1

A nonaqueous electrolyte secondary battery having a positive electrode, a negative electrode, a separator disposed between the positive electrode and the negative electrode, and an electrolytic solution, wherein
the positive electrode includes a positive electrode active material and a binder for positive electrode,
the positive electrode active material, at least, has an alkali metal element as a constituent element,
the binder for positive electrode has a cellulose, and a solvent,
carbon dioxide is dissolved in the solvent,
a part or all of the surface of the positive electrode active material is coated with the cellulose, and
a carbonic acid compound of alkali metal element is coated on a part or all of a surface of the cellulose.

### Claim 2 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
the binder for positive electrodes further has a thermoplastic resin.

### Claim 3 (depends on 2)

The nonaqueous electrolyte secondary battery according to claim 2, wherein
the thermoplastic resin has a polymer gel absorbed the electrolytic solution.

### Claim 4 (depends on 3)

The nonaqueous electrolyte secondary battery according to claim 3, wherein
in the binder for positive electrode, cellulose is 5% by mass or more and 80% by mass or less, and the thermoplastic resin is 20% by mass or more and 95% by mass or less.

### Claim 5 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
the carbon dioxide gas is dissolved in a binder solvent containing the cellulose and the solvent at a concentration of 50 mg/L or more and 9000 mg/L or less.

### Claim 6 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
the cellulose has a fiber diameter of 0.002 μm or more and 1 μm or less, a fiber length of 0.5 μm or more and 10 mm or less, and an aspect ratio of fiber length/fiber diameter of 2 or more and 100000 or less.

### Claim 7 (depends on 5)

The nonaqueous electrolyte secondary battery according to claim 5, wherein
the cellulose includes cellulose in which a hydrophilic group of cellulose is substituted with a hydrophobic group by reaction of cellulose and an additive.

### Claim 8 (depends on 7)

The nonaqueous electrolyte secondary battery according to claim 7, wherein
the cellulose comprises cellulose hydrophobized by a part of a hydroxyl group being replaced with a carboxyl group.

### Claim 9 (depends on 8)

The nonaqueous electrolyte secondary battery according to claim 8, wherein
the cellulose comprises cellulose subjected to ethylene oxide addition treatment or propylene oxide addition treatment.

### Claim 10 (depends on 6)

The nonaqueous electrolyte secondary battery according to claim 6, wherein
the cellulose is subjected to a defibration treatment, and
the defibration treatment is a chemical treatment or a physical treatment.

### Claim 11 (depends on 10)

The nonaqueous electrolyte secondary battery according to claim 10, wherein
the chemical treatment is performed by adding one or more kinds of reagents having a pH value of 0.1 or more and 13 or less and a melting point of −20° C. to 200° C.

### Claim 12 (depends on 10)

The nonaqueous electrolyte secondary battery according to claim 10, wherein
the physical treatment is performed using a grinder, a bead mill, an opposed collision treatment device, a high pressure homogenizer or a water jet.

### Claim 13 (depends on 1)

The nonaqueous electrolyte secondary battery according to claim 1, wherein
the solvent is N-methylpyrrolidone.

### Claim 14

A method of manufacturing a nonaqueous electrolyte secondary battery, comprising
(a) a step of preparing a positive electrode, a negative electrode, a separator disposed between the positive electrode and the negative electrode, and an electrolyte;
(b) a step of laminating the positive electrode, the negative electrode, and the separator and immersing them in an electrolytic solution, and
(c) a step of preparing the positive electrode,
the step (c) includes
(c1) a step of forming a binder for positive electrode having cellulose and a solvent and having carbon dioxide gas dissolved therein,
(c2) a step of forming a slurry having a positive electrode active material and the binder for positive electrode,
(c3) a step of forming the positive electrode by applying the slurry to a current collector,
the positive electrode active material, at least, has an alkali metal element as a constituent element,
in the step (b),
a part or all of the surface of the positive electrode active material is coated with the cellulose, and
a carbonic acid compound of the alkali metal element is coated on a part or all of a surface of the cellulose.

### Claim 15 (depends on 14)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 14, wherein
the binder for positive electrodes further has thermoplastic resin.

### Claim 16 (depends on 15)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 15, wherein
in the step (b),
a polymer gel in which the thermoplastic resin absorbs the electrolytic solution is formed.

### Claim 17 (depends on 15)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 15, wherein
in the binder for positive electrode, cellulose is 5% by mass or more and 80% by mass or less, and the thermoplastic resin is 20% by mass or more and 95% by mass or less.

### Claim 18 (depends on 14)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 14, wherein
the carbon dioxide gas is dissolved in a binder solvent containing the cellulose and the solvent at a concentration of 50 mg/L or more and 9000 mg/L or less.

### Claim 19 (depends on 14)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 14, wherein
the cellulose has a fiber diameter of 0.002 μm or more and 1 μm or less, a fiber length of 0.5 μm or more and 10 mm or less, and an aspect ratio of fiber length/fiber diameter of 2 or more and 100000 or less.

### Claim 20 (depends on 14)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 14, wherein
a hydrophilic group of cellulose comprises cellulose substituted with a hydrophobic group.

### Claim 21 (depends on 20)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 20, wherein
the cellulose comprises cellulose hydrophobized by a part of a hydroxyl group being replaced with a carboxyl group.

### Claim 22 (depends on 21)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 21, wherein
the cellulose comprises cellulose subjected to an ethylene oxide addition treatment or a propylene oxide addition treatment.

### Claim 23 (depends on 19)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 19, wherein
the cellulose is subjected to a defibration treatment, and
the defibration treatment is a chemical treatment or a physical treatment.

### Claim 24 (depends on 23)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 23, wherein
the chemical treatment is performed by adding one or more kinds of reagents having pH value of 0.1 or more and 13 or less, and having melting point of −20° C. to 200° C.

### Claim 25 (depends on 23)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 23, wherein
the physical treatment is performed using a grinder, a bead mill, an opposed collision treatment apparatus, a high pressure homogenizer or a water jet.

### Claim 26 (depends on 14)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 14, wherein
the solvent is a N-methylpyrrolidone.

### Claim 27 (depends on 19)

The method of manufacturing a nonaqueous electrolyte secondary battery according to claim 19, wherein
in the step (c1) comprising
a step of obtaining a mixed solvent liquid comprising the cellulose and a liquid medium and the N-methyl-2-pyrrolidone, and
a step of evaporating the liquid medium in the mixed solvent liquid to increase the concentration of N-methyl-2-pyrrolidone.