# US 2022/0293924 A1 · Tin Alloy Sheets as Negative Electrodes for Non-Aqueous Li and Na-ion Batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293924 A1
- Document ID: US20220293924A1
- Status: Published application
- Kind: A1
- Application number: 17/677,738
- Filed: 2022-02-22
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: Nanode Battery Technologies Ltd.
- Applicants: Nanode Battery Technologies Ltd.
- Inventors: Willem Peter Kalisvaart; Sayed Youssef Sayed Nagy; Jillian Mary Buriak; Bing Cao
- Web page: https://patentgrep.com/patent/US20220293924A1

## CPC

- H01M 4/387: {Tin or alloys based on tin}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0492: {Chemical attack of the support material}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

This invention relates to materials for the negative electrode in non-aqueous rechargeable alkali-ion batteries in free-standing form. In particular, this invention relates to the use of metal ribbon that is produced by melt spinning directly as a battery electrode. The invention also relates to a method producing a highly dispersed, multiphase composite material in a single step, as well as a way to generate porosity while maintaining the ‘binder-free’ and ‘additive-free’ characterization of the electrode.

## Claims

### Claim 1

An electrode comprised of a composite ribbon of Sn.

### Claim 2 (depends on 1)

An electrode as claimed in claim 1 comprising Sn phase with Cu6Sn5 inclusions below 1 micron or Al inclusions below 250 nm.

### Claim 3 (depends on 1)

An electrode as claimed in claim 1 further comprising an element selected from the group consisting of Cu and Al.

### Claim 4 (depends on 2)

An electrode according to claim 2 wherein the electrode is free of binder and conductive additives.

### Claim 5 (depends on 2)

An electrode as claimed in claim 2 comprising an alkali metal ion battery anode.

### Claim 6 (depends on 5)

An electrode as claimed in claim 5 wherein the Al inclusions is up to 50 atomic %.

### Claim 7 (depends on 6)

An electrode as claimed in claim 6 wherein the porosity is equal to the volume fraction of Al in the original alloy ribbon.

### Claim 8 (depends on 7)

An electrode as claimed in claim 7 wherein the porosity is between 0 and 38% for 0 and 50 at % Al, respectively.

### Claim 9

An alkali metal ion battery comprising a porous ribbon of Sn subjected to leaching of a second element selected from the group consisting of Cu and Al.

### Claim 10

A method of producing a battery electrode comprising the steps of:
a) spinning a metal ribbon on a melt spinning apparatus;
to produce a ribbon between 20 and 45 micrometer thickness.

### Claim 11 (depends on 10)

The method as claimed in claim 10 further comprising:
a) setting the spin speed between a surface velocity of between 20 to 50 m/s;
b) selecting a rotating copper wheel with a crucible;
c) selecting Sn and Cu or Sn and Al as metal in the crucible;
d) melting the mixture of c) in the crucible;
e) setting the gap between a bottom of the crucible and the copper rotating wheel between 0.1 and 0.5 mm when the molten material is ejected;
f) selecting the overpressure on top of the melt used to expel the molten material from the crucible onto the copper wheel between 0.2 and 0.4 atmospheres;

### Claim 12 (depends on 10)

The method of claim 10 wherein a composite from the group comprising Sn—Al and Sn—Cu is produced.

### Claim 13 (depends on 10)

The method as claimed in claim 10 followed by a cooling step to ambient temperatures.

### Claim 14 (depends on 10)

The method as claimed in claim 10 further including
dissolving Al in 1 M (aq) KOH solution resulting in a porous Sn structure

### Claim 15 (depends on 10)

The method as claimed in claim 10 wherein;
a) the spin speed is selected between a surface velocity of between of 28.27 to 42.4 m/s;
b) the gap between a bottom of the crucible and the copper rotating wheel is selected between 0.25 and 0.4 mm when the molten material is ejected; and
c) the overpressure on top of the melt used to expel the molten material from the crucible onto the copper wheel between 0.2 and 0.4 atmospheres;

### Claim 16 (depends on 11)

The method as claimed in claim 11 comprising:
a) cold rolling the Sn—Al ribbon to densify the Sn—Al ribbon.

### Claim 17 (depends on 13)

The method as claimed in claim 13 comprising
a) alkaline etching of the Al using potassium hydroxide solution to introduce pores into the Sn ribbon.

### Claim 18 (depends on 17)

The method as claimed in claim 17 wherein the ribbon is used as a battery anode in the form of a sheet, rather than powder.