# US 2022/0293914 A1 · Method for the fabrication of an electroless-metal-plated sulfur nanocomposite, an electroless-metal-plated sulfur cathode which is made from the nanocomposite, and a battery that uses the cathode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293914 A1
- Document ID: US20220293914A1
- Status: Published application
- Kind: A1
- Application number: 17/329,356
- Filed: 2021-05-25
- Published: 2022-09-15
- Earliest claimed: 2021-03-12
- Assignees: National Cheng Kung University
- Applicants: National Cheng Kung University
- Inventors: SHENG HENG CHUNG
- Web page: https://patentgrep.com/patent/US20220293914A1

## CPC

- H01M 4/366: {as layered products}
- C23C 18/1639: {Substrates other than metallic, e.g. inorganic or organic or non-conductive}
- C23C 18/1889: {with use of metal first}
- C23C 18/36: using hypophosphites
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/049: {Manufacturing of an active layer by chemical means}
- H01M 4/139: Processes of manufacture
- H01M 4/38: of elements or alloys
- H01M 4/626: {Metals}
- H01M 10/052: Li-accumulators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for the fabrication of an electroless-metal-plated sulfur nanocomposite, an electroless-metal-plated sulfur cathode which is made from the nanocomposite, and a battery that uses the cathode, where the method includes chemically plating a conductive metal nanoshell onto the surface of the insulating sulfur powder to improve the conductivity of the sulfur cathode material, where through enhancing the electrochemical reaction kinetics with metal catalysis capabilities, and performing physical and chemical adsorption of liquid polysulfides with metal activity, the electroless-metal-plated sulfur nanocomposite enables the battery to exhibit high electrochemical utilization and stable cyclability, such that the nanocomposite can achieve a high sulfur content and high metal content, and the cathode demonstrates a high sulfur loading with a low electrolyte-to-sulfur ratio, the lithium-sulfur battery with the cathode exhibiting a high discharge capacity along with high energy density, and maintaining stable and high reversible capacity after 200 cycles within a wide range of cycling rates.

## Claims

### Claim 1

A method for fabrication of an electroless-metal-plated sulfur nanocomposite, comprising the steps of:
a. a sensitization step, wherein a sensitization solution is prepared by adding SnCl2 to HCl, sulfur powder is added to the sensitization solution and stirred, and the sensitization solution is filtered to collect a sensitized powder;
b. an activation step, wherein an activation solution is prepared by adding PdCl2 to HCl, the sensitized powder is added to the activation solution and stirred, and the activation solution is filtered to collect a pre-treated powder;
c. an acidic chemically plating step, wherein a solution 1 containing metal ions is prepared by dissolving sodium acetate and metallic salt in deionized water; a solution 2 is prepared by dissolving NaH2PO2.H2O in deionized water; solution 1 and solution 2 are preheated to the same temperature and mixed to form a mixture solution, the pre-treated powder is added to the mixture solution and stirred until the metal ions are reduced to metal atoms and form a resulting product, then the resulting product is filtered, dried and ground to form an electroless-metal-plated sulfur nanocomposite.

### Claim 2 (depends on 1)

The method of claim 1, wherein the metallic salt is at least a substance selected from the group consisting of AuCl3, AgCl, CuCl2, SnCl4, NiCl2, CoCl2, and FeCl3.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sensitization solution with the sulfur powder is stirred for 10 to 180 minutes in the sensitization step, wherein the activation solution with the sensitized powder is stirred for 10 to 180 minutes in the activation step, and wherein the mixture solution with the pre-treated powder is stirred for 10 to 180 minutes in the acidic chemically plating step.

### Claim 4 (depends on 1)

The method of claim 1, wherein the same temperature is 70 to 90° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the electroless-metal-plated sulfur nanocomposite has a sulfur content of 60 to 95 wt %.

### Claim 6 (depends on 1)

The method of claim 1, wherein the electroless-metal-plated sulfur nanocomposite has a metal content of 5 to 40 wt %.

### Claim 7 (depends on 1)

An electroless-metal-plated sulfur cathode fabricated by drop-casting, comprising the steps of:
dissolving the electroless-metal-plated sulfur nanocomposite fabricated by the method of claim 1 in an electrolyte, and drop-casting the dissolved electroless-metal-plated sulfur nanocomposite on a current collector to form an electroless-metal-plated sulfur cathode which contains sulfur loading.

### Claim 8 (depends on 7)

The electroless-metal-plated sulfur cathode of claim 7, wherein the electrolyte has an electrolyte-to-sulfur ratio that is 7 to 20 μL/mg.

### Claim 9 (depends on 7)

The electroless-metal-plated sulfur cathode of claim 7, wherein the sulfur loading is 2 to 14 mg/cm2.

### Claim 10 (depends on 7)

A battery that utilizes the electroless-metal-plated sulfur cathode of claim 7.