# US 2022/0293904 A1 · Method of producing electrode for secondary battery, electrode, and secondary battery including electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293904 A1
- Document ID: US20220293904A1
- Status: Published application
- Kind: A1
- Application number: 17/692,186
- Filed: 2022-03-11
- Published: 2022-09-15
- Earliest claimed: 2021-03-12
- Assignees: Prime Planet Energy & Solutions, Inc.
- Applicants: Prime Planet Energy & Solutions, Inc.
- Inventors: Naohiro MASHIMO; Katsushi ENOKIHARA; Haruka SHIONOYA; Masanori KITAYOSHI
- Web page: https://patentgrep.com/patent/US20220293904A1

## CPC

- H01M 4/0435: {Rolling or calendering}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/139: Processes of manufacture
- H01M 10/0431: {Cells with wound or folded electrodes (H01M10/045 takes precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of producing an electrode disclosed here includes a step in which a moisture powder formed of agglomerated particles; a step in which a coating film composed of the moisture powder is formed on an electrode current collector by using the moisture powder, with a gas phase of the coating film being remained, so that the average film thickness of the coating film is 50 μm or more; a step in which the coating film on the electrode current collector is transported, concavo-convex transfer is performed by using a roll mold, and thus a plurality of grooves extending in a direction orthogonal to a transport direction are formed on a surface part of the coating film so that a depth of the groove satisfies (9/10×t1)>t2, and a step in which the coating film formed on the electrode current collector is dried to form an electrode active material layer.

## Claims

### Claim 1

A method of producing an electrode for a secondary battery including any electrode current collector of positive and negative electrodes and an electrode active material layer, the method comprising:
a step in which a moisture powder formed of agglomerated particles containing at least an electrode active material, a binder resin, and a solvent is prepared,
with a solid phase, a liquid phase, and a gas phase in at least 50 number % or more of the agglomerated particles forming a pendular state or a funicular state in the moisture powder;
a step in which a coating film composed of the moisture powder is formed on the electrode current collector by using the moisture powder, with a gas phase of the coating film being remained, with an average film thickness t1 (μm) of the coating film being 50 μm or more;
a step in which the coating film on the electrode current collector is transported, concavo-convex transfer is performed by using a roll mold, and thus a plurality of grooves extending in a direction orthogonal to a transport direction are formed on a surface part of the coating film so that a depth t2 (μm) of the groove satisfies (9/10×t1) >t2; and
a step in which the coating film formed on the electrode current collector is dried to form an electrode active material layer.

### Claim 2 (depends on 1)

The method of producing an electrode for a secondary battery according to claim 1,
wherein, in the moisture powder prepared in the step in which the moisture powder is prepared, when a bulk specific gravity measured by putting a moisture powder (g) into a container having a predetermined volume (mL) with leveling and without applying a force is set as a loose bulk specific gravity X (g/mL), and a specific gravity calculated from the composition of the moisture powder assuming that there is no gas phase is set as a true specific gravity Y (g/mL), a ratio: Y/X of the true specific gravity Y to the loose bulk specific gravity X is 1.2 or more.

### Claim 3

An electrode for a secondary battery, which is any electrode of positive and negative electrodes of a secondary battery, the electrode comprising:
a long sheet-shaped electrode current collector; and
an electrode active material layer formed on the electrode current collector, wherein
a surface part of the electrode active material layer has a plurality of grooves extending in a width direction of the electrode current collector,
a region in which the grooves are formed is uniformly divided into three layers, which are an upper layer, an intermediate layer and a lower layer, in a thickness direction from the surface of the electrode active material layer to the electrode current collector, and
when electrode densities (g/cm3) of the upper layer, the intermediate layer and the lower layer of the region in which the grooves are formed are d1, d2, and d3, respectively, a relationship of 0.8<(d1/d3)<1.1 is satisfied.

### Claim 4 (depends on 3)

A secondary battery comprising a wound electrode body in which a positive electrode having a positive electrode active material layer on a long sheet-shaped positive electrode current collector, a negative electrode having a negative electrode active material layer on a long sheet-shaped negative electrode current collector, and a separator are wound around a winding axis, and a non-aqueous electrolyte,
wherein the electrode according to claim 3 is used as at least one of the positive electrode and the negative electrode.