# US 2022/0293897 A1 · Negative electrode for secondary battery, method for manufacturing the same, and lithium metal secondary battery comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293897 A1
- Document ID: US20220293897A1
- Status: Published application
- Kind: A1
- Application number: 17/639,007
- Filed: 2020-10-21
- Published: 2022-09-15
- Earliest claimed: 2019-12-20
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Jiyong SOON
- Web page: https://patentgrep.com/patent/US20220293897A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/052: Li-accumulators
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 10/0568: characterised by the solutes
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A negative electrode for a secondary battery, including a negative electrode protective layer which can be formed by a simplified method and can effectively suppress the growth of acicular dendrites generated in the negative electrode of a lithium metal secondary battery. The negative electrode for the secondary battery includes a negative electrode current collector; a lithium metal film on the negative electrode current collector; and a negative electrode protective layer including a diazonium ion bonded to the lithium metal film.

## Claims

### Claim 1

A negative electrode for a secondary battery comprising:
a negative electrode current collector;
a lithium metal film present on at least one surface of the negative electrode current collector; and
a negative electrode protective layer comprising a diazonium ion chemically bonded to the lithium metal film.

### Claim 2 (depends on 1)

The negative electrode for the secondary battery according to claim 1, wherein the negative electrode protective layer comprises the diazonium ion having Chemical Formula 1, or comprises a salt of the diazonium ion:
A-N+≡N Chemical Formula 1
in Chemical Formula 1, A is a substituted or unsubstituted alkyl group having 1 to 20 carbon atoms, or a substituted or unsubstituted aryl group having 6 to 40 carbon atoms.

### Claim 3 (depends on 2)

The negative electrode for the secondary battery according to claim 2, wherein the group A present in the diazonium ion is graft bonded to the surface of the lithium metal film.

### Claim 4 (depends on 1)

The negative electrode for the secondary battery according to claim 1, wherein the negative electrode protective layer has a thickness of 1 nm to 1 μm.

### Claim 5 (depends on 1)

The negative electrode for the secondary battery according to claim 1, wherein the negative electrode current collector comprises a copper.

### Claim 6 (depends on 1)

A method for forming the negative electrode of claim 1 comprising:
forming the diazonium ion or a diazonium salt by reacting a nitrite compound and an amine compound on the lithium metal film.

### Claim 7 (depends on 6)

The method for forming the negative electrode according to claim 6, further comprising:
reacting the diazonium ion or diazonium salt with the lithium metal film.

### Claim 8 (depends on 7)

The method for forming theft negative electrode according to claim 7, wherein the step of forming the diazonium ion or the diazonium salt, and the step of reacting the diazonium ion or diazonium salt with the lithium metal film are performed in a single solvent system.

### Claim 9 (depends on 6)

The method for forming the negative electrode according to claim 6, wherein the amine compound is represented by the following Chemical Formula 2:
A-NH2 Chemical Formula 2
in Chemical Formula 2, A is a substituted or unsubstituted alkyl group having 1 to 20 carbon atoms, or a substituted or unsubstituted aryl group having 6 to 40 carbon atoms.

### Claim 10 (depends on 6)

The method for forming the negative electrode according to claim 6, wherein the nitrite compound comprises tert-butyl nitrite or sodium nitrite.

### Claim 11 (depends on 8)

The method for forming the negative electrode according to claim 8, wherein the step of forming the diazonium ion or the diazonium salt, and the step of reacting the diazonium ion or the diazonium salt with the lithium metal film are performed in an organic solvent of acetonitrile or tetrahydrofuran.

### Claim 12 (depends on 1)

A lithium metal secondary battery comprising:
the negative electrode of claim 1,
a positive electrode, and
an electrolyte disposed between the negative electrode and the positive electrode.

### Claim 13 (depends on 12)

The lithium metal secondary battery according to claim 12, wherein the positive electrode active material comprises one or more complex oxides of cobalt, manganese, nickel, or iron; and lithium.

### Claim 14 (depends on 12)

The lithium metal secondary battery according to claim 12, wherein
the electrolyte comprises at least one lithium salt selected from lithium bis(fluorosulfonyl)imide (LiFSI), LiPF6, LiBF4, LiSbF6, LiAsF6, LiC4F9SO3, LiClO4, LiAlO2, LiAlCl4, LiN(CxF2x+1SO2)(CyF2y+1SO2) (where, x and y are a natural number), LiCl, LiI, or LiB(C2O4)2 (lithium bis(oxalato)borate; LiBOB) or a combination thereof; and a non-aqueous organic solvent.

### Claim 15 (depends on 1)

The negative electrode for the secondary battery according to claim 1, wherein the lithium metal film has a thickness of 1 μm to 100 μm.