# US 2022/0293884 A1 · Encapsulated Electronic Device with Improved Protective Barrier Layer and Method of Manufacture Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293884 A1
- Document ID: US20220293884A1
- Status: Published application
- Kind: A1
- Application number: 17/202,242
- Filed: 2021-03-15
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: SDK New Materials, Inc.
- Applicants: SDK New Materials, Inc.
- Inventors: Wenming Li; Jiaming Hua; Xingbao Zhou; Qiujun Pan; Chuang Jin
- Web page: https://patentgrep.com/patent/US20220293884A1

## CPC

- H10K 50/844: Encapsulations
- H10K 77/111: {Flexible substrates}
- H10K 2102/311: {Flexible OLED}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

Embodiments of a thin film protective barrier for an encapsulated electronic device is disclosed. The barrier is applied as a thin film coating onto a moisture-sensitive microelectronic device, such as an OLED. A density of the barrier is varied during fabrication, allowing the barrier to flex in applications that demand that the encapsulated electronic device be flexible, while providing a highly-resistant barrier to moisture, oxygen and other contaminants.

## Claims

### Claim 1

An encapsulated electronic device, comprising:
a flexible substrate;
a microelectronic device fabricated onto a first surface of the flexible substrate; and
a protective barrier layer fabricated onto the microelectronic device for preventing contamination of the microelectronic device, the protective barrier layer comprising a density that varies as a function of a thickness of the protective barrier layer.

### Claim 2 (depends on 1)

The encapsulated microelectronic device of claim 1, further comprising:
a second protective barrier layer fabricated onto a second, opposing surface of the flexible substrate for preventing contamination of the microelectronic device through the flexible substrate, the second barrier layer comprising a second density that varies as a function of a thickness of the second protective barrier layer.

### Claim 3 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the density of the protective barrier layer varies continuously from a low density in a lower portion of the protective barrier layer adjacent to the microelectronic device, to a high density in a middle portion of the protective barrier layer, to a second low density in a top portion of the protective barrier layer exposed to ambient air.

### Claim 4 (depends on 3)

The encapsulated microelectronic device of claim 3, wherein the low density comprises a density from about X to Y.

### Claim 5 (depends on 3)

The encapsulated microelectronic device of claim 3, wherein the high density comprises a density from about X to Y.

### Claim 6 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the density of the protective barrier layer varies as a series of low-to-high-to-low transitions.

### Claim 7 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the density of the protective barrier layer varies linearly as a gradient.

### Claim 8 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the protective barrier layer comprises an inorganic, transparent material, selected from the group consisting of Al2O3, SiO2, Si2N4, and Nb2O5.

### Claim 9 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the protective barrier layer comprises a refractive index that varies as a function of the density of the protective barrier layer.

### Claim 10 (depends on 1)

The encapsulated microelectronic device of claim 1, wherein the protective barrier layer comprises a thickness of about between 20 nanometers and 200 nanometers.

### Claim 11

A method for fabricating an encapsulated microelectronic device, comprising:
fabricating the microelectronic device onto a flexible substrate; and
fabricating a protective barrier layer onto the microelectronic device, comprising:
varying a deposition power density delivered by a deposition power generator over a deposition time while maintaining a constant deposition pressure of a deposition chamber, resulting in the protective barrier layer having a density that varies as a function of its thickness.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
fabricating a second protective barrier layer onto the flexible substrate, comprising:
varying the deposition power density delivered by the deposition power generator over a second deposition time while maintaining the constant deposition pressure of the deposition chamber, resulting in the second protective barrier layer having a density that varies as a function of its thickness.

### Claim 13 (depends on 11)

The method of claim 11, wherein varying a deposition power density of the deposition power generator over a deposition time comprises:
varying a power density delivered by the deposition power generator continuously from a low power density to a high power density then down to a second low power density during the deposition time.

### Claim 14 (depends on 13)

The method of claim 13, wherein the high power density comprises a power density of about 20 w/cm2.

### Claim 15 (depends on 11)

The method of claim 11, wherein varying a deposition power density delivered by the deposition power generator over a deposition time comprises:
varying a power density delivered by the thin film power generator from about 0.5 w/cm2 to about 20 w/cm2.

### Claim 16 (depends on 11)

The method of claim 11, wherein varying a deposition power density over a deposition time comprises:
repeatedly varying a power density delivered by the deposition power generator continuously from a low power density to a high power density then down to second low power density during the deposition time.

### Claim 17

A method for fabricating an encapsulated microelectronic device, comprising:
fabricating the microelectronic device onto a flexible substrate; and
fabricating a protective barrier layer onto the microelectronic device, comprising:
varying a deposition pressure of a deposition chamber over a deposition time while maintaining a constant deposition power density delivered by a deposition power generator, resulting in the protective barrier layer having a density that varies as a function of its thickness.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
fabricating a second protective barrier layer onto the flexible substrate, comprising:
varying the deposition pressure of the deposition chamber over a second deposition time while maintaining the constant deposition power density delivered by the deposition power generator, resulting in the second protective barrier layer having a density that varies as a function of its thickness.

### Claim 19 (depends on 17)

The method of claim 17, wherein varying a deposition pressure of a deposition chamber over a deposition time comprises:
varying the deposition pressure of the deposition chamber continuously from a low pressure to a high pressure then down to a second low pressure during the deposition time.

### Claim 20 (depends on 17)

The method of claim 17, wherein varying a deposition pressure of a deposition chamber over a deposition time comprises:
repeatedly varying the deposition pressure of the deposition chamber continuously from a low pressure to a high pressure then down to a second low pressure during the deposition time.