# US 2022/0293814 A1 · Preparation process and led application of copper nanoclusters fluorescent nanoflowers with high quantum yield

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293814 A1
- Document ID: US20220293814A1
- Status: Published application
- Kind: A1
- Application number: 17/456,558
- Filed: 2021-11-24
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: Shandong University
- Applicants: Shandong University
- Inventors: Xia Xin; Shujin Zhou; Di Sun; Shanshan Zhang; Ning Feng
- Web page: https://patentgrep.com/patent/US20220293814A1

## CPC

- H10H 20/01: Manufacture or treatment
- H10H 20/8513: {having two or more wavelength conversion materials}
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/8512: {Wavelength conversion materials}
- H10H 20/0361: {of wavelength conversion means}
- H10H 20/8511: {characterised by their material, e.g. binder}
- H10H 20/8514: {characterised by their shape, e.g. plate or foil}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A preparation process and LED application of copper nanoclusters (Cu NCs) fluorescent nanoflowers with high quantum yield by dissolving Cu4I4 into dimethyl sulfoxide (DMSO) and then adding glycerol, it self-assembles into Cu NCs s fluorescent nanoflowers. The Cu4I4 fluorescent nanoflowers prepared by the invention have outstanding optical properties, a quantum yield up to 64.5%, and can be made into a series of different luminous colors and excellent stability LED only with commercial blue phosphor, such as yellow-green, sky blue, white, wherein according to the mass ratio of 4:5 ratio mix can be prepared white light emission LED. Fluorescent Cu NCs can successfully replace traditional light conversion materials and prepare environmentally friendly LEDs.

## Claims

### Claim 1

A process for preparing LED comprising the following steps: a Cu NCs fluorescent nanoflowers are ground evenly, then mixed evenly with phosphor of different colors, and then deposited on a LED chip by glue, curing, to obtain different light-emitting color LED.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the Cu NCs fluorescent nanoflowers comprising flakes with a chemical composition of Cu4I4, which is quad-core Cu NCs with Cu as nucleus and triphenylphosphine as a ligand.

### Claim 3 (depends on 2)

The process according to claim 2, wherein each of the Cu NCs fluorescent nanoflowers has a diameter of 30-50 μm, each of the flakes has a length of 15-20 μm and a width of 5-8 μm.

### Claim 4 (depends on 2)

The process according to claim 2, wherein a fluorescent spectra of the Cu NCs fluorescent nanoflowers shows excitation wavelength between 290-400 nm and emission wavelength between 450-620 nm.

### Claim 5 (depends on 2)

The process according to claim 2, wherein the Cu NCs fluorescent nanoflowers are prepared by the following steps: the Cu4I4 are dissolved into DMSO with ultrasound, add glycerol, vortex, static, centrifugal, and dry after washing; wherein with the ratio of the DMSO and glycerol is 1:(1-3) by volume.

### Claim 6 (depends on 5)

The process according to claim 5, wherein Cu4I4 has a molar concentration of 0.12-0.14 mmol·L−1 in DMSO; add glycerol and mix, and final molar concentration of Cu4I4 is 0.06-0.07 mmol·L−1; vortex for 20-30 seconds and incubate for 5-48 hours; then, centrifuge at 6000-8000 r/min for 10-20 min.

### Claim 7 (depends on 4)

The process according to claim 4, wherein the Cu4I4 is prepared by dispersing CuI in dichloromethane solution, stirring evenly, then adding triphenylphosphine, stirring fully at room temperature, filtering to obtain a white powdered solid; then, adding the white powdered solids to an acetylene solution, performing ultrasound, filtrating, washing with acetylene to obtain a pure white powdered solid; dissolving the pure white solid powder in DMSO solution, adding to a diffusion glass tube, a upper layer is diffused by methanol solution, and yielding Cu4I4 powders in three days.

### Claim 8 (depends on 1)

The process according to claim 1, wherein the Cu NCs fluorescent nanoflowers and blue phosphor are mixed by a mass ratio of 1:(0.7-0.8);
high-fold LED patch silicone A and B glue are utilized for deposition, with a quality ratio of 1:4 for A glue and B glue; the LED chip has an excitation wavelength of 365 nm and a light effect of 0.9 lm/W;
curing at temperature of 60° C. for 3 hours.