# US 2022/0293801 A1 · Uv-curing of light-receiving surfaces of solar cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293801 A1
- Document ID: US20220293801A1
- Status: Published application
- Kind: A1
- Application number: 17/829,152
- Filed: 2022-05-31
- Published: 2022-09-15
- Earliest claimed: 2016-11-11
- Assignees: SunPower Corporation; Total Marketing Services
- Applicants: Sunpower Corporation; Total Marketing Services
- Inventors: Yu-Chen Shen; Perine Jaffrennou; Gilles Olav Tanguy Sylvain Poulain; Michael C. Johnson; Seung Bum Rim
- Web page: https://patentgrep.com/patent/US20220293801A1

## CPC

- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 10/166: the Group IV-IV heterojunctions being heterojunctions of crystalline and amorphous materials, e.g. silicon heterojunction [SHJ] photovoltaic cells
- H10F 71/128: {Annealing}
- H10F 71/129: {Passivating}
- H10F 77/311: {for photovoltaic cells}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/546: Polycrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods of fabricating solar cells using UV-curing of light-receiving surfaces of the solar cells, and the resulting solar cells, are described herein. In an example, a method of fabricating a solar cell includes forming a passivating dielectric layer on a light-receiving surface of a silicon substrate. The method also includes forming an anti-reflective coating (ARC) layer below the passivating dielectric layer. The method also includes exposing the ARC layer to ultra-violet (UV) radiation. The method also includes, subsequent to exposing the ARC layer to ultra-violet (UV) radiation, thermally annealing the ARC layer.

## Claims

### Claim 1

A solar cell fabricated according to a method, the method comprising:
forming a passivating dielectric layer on a light-receiving surface of a silicon substrate;
forming an anti-reflective coating (ARC) layer below the passivating dielectric layer;
exposing the ARC layer to ultra-violet (UV) radiation;
subsequent to forming the ARC layer and prior to exposing the ARC layer to UV radiation, heating at a temperature approximately in the range of 200-500 degrees Celsius; and
subsequent to exposing the ARC layer to ultra-violet (UV) radiation, thermally annealing the ARC layer.

### Claim 2 (depends on 1)

The solar cell of claim 1, wherein exposing the ARC layer to UV radiation comprises exposing the ARC layer to light having a wavelength approximately in the range of 250-450 nanometers.

### Claim 3 (depends on 1)

The solar cell of claim 1, wherein exposing the ARC layer to UV radiation comprises exposing for a duration approximately in the range of 1 second-1 day.

### Claim 4 (depends on 1)

The solar cell of claim 1, wherein thermally annealing the ARC layer comprises heating at a temperature approximately in the range of 200-500 degrees Celsius.

### Claim 5 (depends on 4)

The solar cell of claim 4, wherein the heating comprises using a process selected from the group consisting of a forming gas anneal (FGA) process, a rapid thermal anneal (RTA) process, an intra-red (IR) heating process, a furnace heating process, and a laser annealing process.

### Claim 6 (depends on 1)

The solar cell of claim 1, wherein forming the passivating dielectric layer comprises forming a thermal silicon oxide layer on a light-receiving surface of the silicon substrate, and wherein the silicon substrate is an N-type monocrystalline silicon substrate.

### Claim 7 (depends on 1)

The solar cell of claim 1, wherein forming the passivating dielectric layer comprises forming the passivating dielectric layer by atomic layer deposition (ALD), the passivating dielectric layer selected from the group consisting of silicon oxide.

### Claim 8 (depends on 1)

The solar cell of claim 1, wherein forming the ARC layer comprises forming a silicon nitride layer.

### Claim 9 (depends on 1)

The solar cell of claim 1, the method further comprising:
subsequent to forming the passivating dielectric layer, forming an N-type micro- or poly-crystalline silicon layer on the passivating dielectric layer, wherein the ARC layer is formed on the N-type micro- or poly-crystalline silicon layer.

### Claim 10 (depends on 1)

The solar cell of claim 1, the method further comprising:
subsequent to forming the passivating dielectric layer, forming an intermediate material layer on the passivating dielectric layer, the intermediate material layer selected from the group consisting of an amorphous silicon (a-Si) layer, a silicon-rich silicon nitride layer, and a Group III-V material layer, wherein the ARC layer is formed on the intermediate material layer.

### Claim 11 (depends on 1)

The solar cell of claim 1, wherein forming the ARC layer comprises forming the ARC layer having an amount of hydrogen therein, the method further comprising:
removing at least a portion of the amount of hydrogen from the ARC layer.

### Claim 12 (depends on 11)

The solar cell of claim 11, wherein removing the portion of the amount of hydrogen from the ARC layer is performed during the thermal annealing of the ARC layer.

### Claim 13 (depends on 1)

The solar cell of claim 1, wherein the ARC layer includes hydrogen.

### Claim 14 (depends on 1)

The solar cell of claim 1, wherein the exposing the ARC layer to UV radiation and the thermally annealing the ARC layer reduce hydrogen bonds at the interface between the ARC layer and the passivating dielectric layer.

### Claim 15 (depends on 1)

The solar cell of claim 1, wherein the ARC layer that is exposed to UV radiation includes silicon nitride, aluminum oxide or indium tin oxide.

### Claim 16 (depends on 1)

The solar cell of claim 1, wherein the passivating dielectric layer includes an oxide.

### Claim 17

A solar cell fabricated according to a method, the method comprising:
forming a passivating dielectric layer on a light-receiving surface of a silicon substrate;
forming an anti-reflective coating (ARC) layer below the passivating dielectric layer;
increasing the saturation current density (J0) at an interface at the light-receiving surface of the silicon substrate, wherein increasing the saturation current density at the interface comprises exposing the ARC layer to UV radiation having a wavelength approximately in the range of 250-450 nanometers for a duration approximately in the range of 1 second-1 day;
subsequent to forming the ARC layer and prior to exposing the ARC layer to UV radiation, heating at a temperature approximately in the range of 200-500 degrees Celsius; and
subsequent to increasing the saturation current density, thermally annealing the ARC layer.

### Claim 18 (depends on 17)

The solar cell of claim 17, wherein thermally annealing the ARC layer comprises heating at a temperature approximately in the range of 200-500 degrees Celsius using a process selected from the group consisting of a forming gas anneal (FGA) process, a rapid thermal anneal (RTA) process, an intra-red (IR) heating process, a furnace heating process, and a laser annealing process.

### Claim 19

A solar cell fabricated according to a method, the method comprising:
forming a thermal silicon oxide layer on a light-receiving surface of an N-type monocrystalline silicon substrate;
forming an anti-reflective coating (ARC) layer below the thermal silicon oxide layer;
increasing the saturation current density (J0) at an interface at the light-receiving surface of the silicon substrate, wherein increasing the saturation current density at the interface comprises exposing the ARC layer to UV radiation having a wavelength approximately in the range of 250-450 nanometers for a duration approximately in the range of 1 second-1 day;
subsequent to forming the ARC layer and prior to exposing the ARC layer to UV radiation, heating at a temperature approximately in the range of 200-500 degrees Celsius; and
subsequent to increasing the saturation current density, thermally annealing the ARC layer.