# US 2022/0293793 A1 · Process to reduce plasma induced damage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293793 A1
- Document ID: US20220293793A1
- Status: Published application
- Kind: A1
- Application number: 17/805,161
- Filed: 2022-06-02
- Published: 2022-09-15
- Earliest claimed: 2017-10-12
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Jianheng LI; Lai ZHAO; Yujia ZHAI; Soo Young CHOI
- Web page: https://patentgrep.com/patent/US20220293793A1

## CPC

- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- H10K 10/462: {Insulated gate field-effect transistors [IGFETs]}
- H10K 10/472: {the gate dielectric comprising only inorganic materials}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D 30/0312: {characterised by the gate electrodes}
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10K 59/12: Active-matrix OLED [AMOLED] displays
- H10K 59/1201: {Manufacture or treatment}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

Embodiments described herein provide thin film transistors (TFTs) and processes to reduce plasma induced damage in TFTs. In one embodiment, a buffer layer is disposed over a substrate and a semiconductor layer is disposed over the buffer layer. A gate dielectric layer is disposed over the semiconductor layer. The gate dielectric layer contacts the semiconductor layer at an interface. The gate electrode 204 is disposed over the gate dielectric layer. The gate dielectric layer has a Dit of about 5e10 cm−2eV−1 to about 5e11 cm−2eV−1 and a hysteresis of about 0.10 V to about 0.30 V improve performance capability of the TFT while having a breakdown field between about 6 MV/cm and about 10 MV/cm.

## Claims

### Claim 1

A method of fabricating a thin film transistor (TFT), comprising:
flowing a deposition gas at a deposition gas flow rate into a process volume of a chamber;
applying a radio frequency (RF) power to the deposition gas for an initial interval at an initial power level forming an intermediate layer of a gate dielectric layer, the intermediate layer having a first surface contacting a semiconductor layer at an interface with the first surface; and
applying the RF power for a final interval at a final power level different than the first power level forming a bulk layer of the gate dielectric layer having a second surface to contact a gate electrode and an ILD layer to be formed, the gate electrode having:
a thickness consisting essentially of the intermediate layer and the bulk layer, the intermediate layer is not greater than about 20% of the thickness and has a density not greater than the density of the bulk layer; and
a breakdown field between about 6 MV/cm and about 10 MV/cm, an interface trap density (Dit) of about 5e10 cm−2 eV−1 to about 5e11 cm−2eV−1, and a hysteresis of about 0.10 V to about 0.30 V.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming initial layers of the TFT on a substrate before flowing the deposition gas at the deposition gas flow rate.

### Claim 3 (depends on 1)

The method of claim 1, further comprising forming a remaining structure of the TFT after the RF power is applied for the final interval at the final power level.

### Claim 4 (depends on 1)

The method of claim 1, wherein the RF power is about 2000 Watts (W) to about 16000 W.

### Claim 5 (depends on 1)

The method of claim 1, wherein the initial power level is about 2000 W to about 5000 W.

### Claim 6 (depends on 1)

The method of claim 1, wherein the final power level is about 12000 W to about 16000 W.

### Claim 7 (depends on 1)

The method of claim 1, wherein the thickness is about 500 Angstroms to about 1500 Angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein the semiconductor layer includes at least one of a silicon, a polysilicon, a low temperature polysilicon, an amorphous silicon, an indium-gallium-zinc oxide (IGZO), or an zinc oxynitride (ZnON) containing material.

### Claim 9 (depends on 1)

The method of claim 1, wherein the gate dielectric layer comprises at least one of a SiN, a silicon nitride (Si3N4), a silicon monoxide (SiO), a silicon dioxide SiO2, or a silicon oxynitride Si2N2O containing material.

### Claim 10

A method of fabricating a thin film transistor (TFT), comprising:
forming initial layers including a semiconductor layer over a substrate;
flowing a deposition gas at a deposition gas flow rate into a process volume of a chamber;
applying a radio frequency (RF) power to the deposition gas for an initial interval at an initial power level forming an intermediate layer of a gate dielectric layer, the intermediate layer having a first surface contacting the semiconductor layer at an interface with the first surface; and
applying the RF power for a final interval at a final power level different than the first power level forming a bulk layer of the gate dielectric layer having a second surface to contact a gate electrode and an ILD layer to be formed, the gate electrode having:
a thickness consisting essentially of the intermediate layer and the bulk layer, the intermediate layer is not greater than about 20% of the thickness and has a density not greater than the density of the bulk layer; and
a breakdown field between about 6 MV/cm and about 10 MV/cm, an interface trap density (Dit) of about 5e10 cm−2 eV−1 to about 5e11 cm−2eV−1, and a hysteresis of about 0.10 V to about 0.30 V.

### Claim 11 (depends on 10)

The method of claim 10, further comprising forming a remaining structure of the TFT after the RF power is applied for the final interval at the final power level.

### Claim 12 (depends on 10)

The method of claim 10, wherein the RF power is about 2000 Watts (W) to about 16000 W.

### Claim 13 (depends on 10)

The method of claim 10, wherein the initial power level is about 2000 W to about 5000 W.

### Claim 14 (depends on 10)

The method of claim 10, wherein the final power level is about 12000 W to about 16000 W.

### Claim 15 (depends on 10)

The method of claim 10, wherein the thickness is about 500 Angstroms to about 1500 Angstroms.

### Claim 16 (depends on 10)

The method of claim 10, wherein the semiconductor layer includes at least one of a silicon, a polysilicon, a low temperature polysilicon, an amorphous silicon, an indium-gallium-zinc oxide (IGZO), or an zinc oxynitride (ZnON) containing material.

### Claim 17 (depends on 10)

The method of claim 10, wherein the gate dielectric layer comprises at least one of a SiN, a silicon nitride (Si3N4), a silicon monoxide (SiO), a silicon dioxide SiO2, or a silicon oxynitride Si2N2O containing material.

### Claim 18

A method of fabricating a thin film transistor (TFT), comprising:
forming a buffer layer on a substrate;
forming a semiconductor layer on the buffer layer;
flowing a deposition gas at a deposition gas flow rate into a process volume of a chamber;
applying a radio frequency (RF) power to the deposition gas for an initial interval at an initial power level forming an intermediate layer of a gate dielectric layer, the intermediate layer having a first surface contacting the semiconductor layer at an interface with the first surface; and
applying the RF power for a final interval at a final power level different than the first power level forming a bulk layer of the gate dielectric layer having a second surface to contact a gate electrode and an ILD layer to be formed, the gate electrode having:
a thickness consisting essentially of the intermediate layer and the bulk layer, the intermediate layer is not greater than about 20% of the thickness and has a density not greater than the density of the bulk layer; and
a breakdown field between about 6 MV/cm and about 10 MV/cm, an interface trap density (Dit) of about 5e10 cm−2eV−1 to about 5e11 cm−2eV−1, and a hysteresis of about 0.10 V to about 0.30 V.

### Claim 19 (depends on 18)

The method of claim 18, wherein the initial power level is about 2000 W to about 5000 W.

### Claim 20 (depends on 18)

The method of claim 18, wherein the final power level is about 12000 W to about 16000 W.