# US 2022/0293772 A1 · Method for Manufacturing Semiconductor Structure and Semiconductor Structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293772 A1
- Document ID: US20220293772A1
- Status: Published application
- Kind: A1
- Application number: 17/452,454
- Filed: 2021-10-27
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Shuai Guo
- Web page: https://patentgrep.com/patent/US20220293772A1

## CPC

- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10B 12/00: Dynamic random access memory [DRAM] devices
- H10B 12/053: {the transistor being at least partially in a trench in the substrate (vertical transistor in combination with a capacitor formed in a substrate trench H10B12/0383)}
- H10B 12/34: {the transistor being at least partially in a trench in the substrate}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10D 64/027: {by etching at gate locations}
- H10D 64/27: Electrodes not carrying the current to be rectified, amplified, oscillated or switched, e.g. gates
- H10D 64/513: {within recesses in the substrate, e.g. trench gates, groove gates or buried gates}
- H10D 64/516: {the thicknesses being non-uniform}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D 84/0135: {Manufacturing their gate conductors}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10B 12/488: {Word lines}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/683: {being parallel to the channel plane}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The present application relates to the technical field of semiconductors, and provides a method for manufacturing a semiconductor structure and a semiconductor structure. The manufacturing method includes: providing a substrate with trench structures; forming a source region and a drain region respectively on both sides of each of the trench structures; forming an oxide layer, the oxide layer including a first oxide portion covering side walls of each of the trench structured and a second oxide portion covering a bottom wall of each of the trench structures, and a thickness of the second oxide portion being less than a thickness of the first oxide portion; and nitriding the oxide layer, so that a concentration of nitrogen ions in the first oxide portion is less than a concentration of nitrogen ions in the second oxide portion.

## Claims

### Claim 1

A method for manufacturing a semiconductor structure, comprising:
providing a substrate, the substrate comprising trench structures distributed at intervals;
forming a source region and a drain region respectively on both sides of each of the trench structures;
forming an oxide layer, the oxide layer comprising a first oxide portion and a second oxide portion, wherein the first oxide portion covers side walls of each of the trench structures, the second oxide portion covers a bottom wall of each of the trench structures, and a thickness of the second oxide portion is less than a thickness of the first oxide portion;
nitriding the oxide layer, so that a concentration of nitrogen ions in the first oxide portion is less than a concentration of nitrogen ions in the second oxide portion; and
forming a gate structure in each of the trench structures.

### Claim 2 (depends on 1)

The method for manufacturing the semiconductor structure according to claim 1, wherein a ratio of the concentration of the nitrogen ions in the first oxide portion to the concentration of the nitrogen ions in the second oxide portion is between 0.1 and 0.5.

### Claim 3 (depends on 2)

The method for manufacturing the semiconductor structure according to claim 2, wherein nitriding the oxide layer comprises:
at 400° C.-850° C., introducing ammonia gas or nitrogen gas to a surface of the oxide layer, and then nitriding the oxide layer by plasma treatment.

### Claim 4 (depends on 1)

The method for manufacturing the semiconductor structure according to claim 1, wherein forming the oxide layer comprises:
forming a silicon oxide layer on the side walls and the bottom wall of each of the trench structures by an atomic layer deposition process, wherein the silicon oxide layer covering the side walls of each of the trench structures forms the first oxide portion, and the silicon oxide layer covering the bottom wall of each of the trench structures forms the second oxide portion; and
performing high temperature treatment on the first oxide portion and the second oxide portion, so as to increase compactness of the first oxide portion and compactness of the second oxide portion.

### Claim 5 (depends on 4)

The method for manufacturing the semiconductor structure according to claim 4, wherein performing the high temperature treatment on the first oxide portion and the second oxide portion comprises: performing a thermal annealing treatment process on the first oxide portion and the second oxide portion, wherein a reaction temperature in the thermal annealing treatment process is 600° C.-650° C.

### Claim 6 (depends on 5)

The method for manufacturing the semiconductor structure according to claim 5, wherein a ratio of the thickness of the second oxide portion to the thickness of the first oxide portion is 75%-95%.

### Claim 7 (depends on 1)

The method for manufacturing the semiconductor structure according to claim 1, wherein after nitriding the oxide layer and before forming the gate structure in each of the trench structures, the method further comprises:
forming an initial barrier layer on the oxide layer; and
nitriding the initial barrier layer.

### Claim 8 (depends on 7)

The method for manufacturing the semiconductor structure according to claim 7, wherein nitriding the initial barrier layer comprises:
at 400° C.-850° C., introducing ammonia gas or nitrogen gas to a surface of the initial barrier layer, and then nitriding the initial barrier layer by plasma treatment.

### Claim 9 (depends on 8)

The method for manufacturing the semiconductor structure according to claim 8, wherein forming the gate structure in each of the trench structures comprises:
forming an initial conductive layer on the initial barrier layer, the initial conductive layer covering the surface of the initial barrier layer;
removing a portion of the initial barrier layer and a portion of the initial conductive layer, a remaining initial barrier layer forming a barrier layer, and a remaining initial conductive layer forming the gate structure; and
wherein an upper surface of the barrier layer is flush with an upper surface of the gate structure, and the upper surface of the gate structure is lower than an upper surface of the substrate.

### Claim 10 (depends on 9)

The method for manufacturing the semiconductor structure according to claim 9, wherein after forming the gate structure in each of the trench structures, the method further comprises:
forming a gate protection layer, the gate protection layer covering the surface of the substrate and filling each of the trench structures.

### Claim 11 (depends on 10)

The method for manufacturing the semiconductor structure according to claim 10, wherein after forming the gate structure in each of the trench structures and before forming the gate protection layer, the method further comprises:
introducing hydrogen gas or ammonia gas to a surface of the gate structure, and performing the plasma treatment on the gate structure at 600° C.-760° C.

### Claim 12

A semiconductor structure, comprising:
a substrate, the substrate having trench structures;
an oxide layer, the oxide layer comprising a first oxide portion and a second oxide portion, the first oxide portion covers side walls of each of the trench structures, the second oxide portion covers a bottom wall of each of the trench structures, a thickness of the second oxide portion is less than a thickness of the first oxide portion, and a concentration of nitrogen ions in the first oxide portion is less than a concentration of nitrogen ions in the second oxide portion; and
a gate structure, the gate structure being provided in each of the trench structures, and a top surface of the gate structure being lower than a top surface of the substrate.

### Claim 13 (depends on 12)

The semiconductor structure according to claim 12, wherein a ratio of the concentration of nitrogen ions in the first oxide portion to the concentration of nitrogen ions in the second oxide portion is between 0.1 and 0.5.

### Claim 14 (depends on 13)

The semiconductor structure according to claim 13, wherein the semiconductor structure further comprises a barrier layer, the barrier layer is located between the oxide layer and the gate structure.

### Claim 15 (depends on 14)

The semiconductor structure according to claim 14, wherein the semiconductor structure further comprises a gate protection layer, the gate protection layer is provided on a surface of the barrier layer and a surface of the gate structure, and fills the trench structure.
