# US 2022/0293625 A1 · Methods of forming microelectronic devices with nitrogen-rich insulative structures, and related microelectronic devices, memory devices, and electronic systems

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293625 A1
- Document ID: US20220293625A1
- Status: Published application
- Kind: A1
- Application number: 17/200,169
- Filed: 2021-03-12
- Published: 2022-09-15
- Earliest claimed: 2021-03-12
- Assignees: Mcron Technology, Inc.
- Applicants: Mcron Technology, Inc.
- Inventors: Swapnil Lengade; Jeremy Adams; Naiming Liu; Jeslin J. Wu; Kadir Abdul; Carlo Mendoza Orofeo
- Web page: https://patentgrep.com/patent/US20220293625A1

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 41/10: characterised by the top-view layout
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 43/10: characterised by the top-view layout
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a microelectronic device comprises forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures, at least some of the additional insulative structures comprising silicon nitride having a ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00, forming openings through the stack structure, and forming cell pillar structures within the openings, the cell pillar structures individually comprising a semiconductor channel material vertically extending through the stack structure. Related methods, microelectronic devices, memory devices, and electronic systems are also described.

## Claims

### Claim 1

A method of forming a microelectronic device, the method comprising:
forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures, at least some of the additional insulative structures comprising silicon nitride having a ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00;
forming openings through the stack structure; and
forming cell pillar structures within the openings, the cell pillar structures individually comprising a semiconductor channel material vertically extending through the stack structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming a majority of the additional insulative structures to have the ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming all of the additional insulative structures to comprise the ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00.

### Claim 4 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming vertically uppermost of the additional insulative structures and vertically lowermost of the additional insulative structures to each comprise a higher ratio of nitrogen atoms to silicon atoms than other of the additional insulative structures.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming the at least some of the additional insulative structures to have greater than 1.70 nitrogen atoms per 1.00 silicon atoms.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming the additional insulative structures by plasma enhanced physical vapor deposition at a pressure greater than about 7 torr.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming a stack structure comprising a vertically alternating sequence of insulative structures and additional insulative structures comprises forming the additional insulative structures by plasma enhanced chemical vapor deposition using silane and ammonia, a flowrate of the silane within a range from about 300 sccm to about 700 sccm and a flowrate of ammonia within a range from about 15,000 sccm to about 22,000 sccm.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming openings through the stack structure comprises:
forming initial openings partially vertically extending through the stack structure;
forming a polymer material on sidewalls of the stack structure defining the initial openings; and
after forming the polymer material, removing additional portions of the stack structure vertically underlying and within horizontal boundaries of the initial openings to form the openings from the initial openings.

### Claim 9 (depends on 8)

The method of claim 8, further comprising removing the polymer material after forming the openings.

### Claim 10 (depends on 9)

The method of claim 9, wherein removing the polymer material comprises exposing the polymer material to oxygen.

### Claim 11 (depends on 1)

The method of claim 1, further comprising:
forming slots vertically extending through the stack structure in an array region thereof;
removing portions of the additional insulative structures within the array region through the slots while maintaining additional portions of the additional insulative structures in a peripheral region of the stack structure; and
replacing the removed portions of the additional insulative structures with conductive structures.

### Claim 12

A microelectronic device, comprising:
a stack structure comprising:
first levels comprising insulative structures; and
second levels vertically interleaved with the first levels and each comprising an additional insulative structure and a conductive structure horizontally neighboring the additional insulative structure, the additional insulative structure of at least some of the second levels comprising silicon nitride having a ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00; and
strings of memory cells vertically extending through the stack structure and each within horizontal boundaries of the conductive structures of each of the second levels.

### Claim 13 (depends on 12)

The microelectronic device of claim 12, wherein the ratio of the nitrogen atoms to silicon atoms increases with an increasing vertical distance from a center of the stack structure.

### Claim 14 (depends on 12)

The microelectronic device of claim 12, wherein the stack structure is divided into block structures having the strings of memory cells within horizontal areas thereof, the additional insulative structures external to the block structures.

### Claim 15 (depends on 12)

The microelectronic device of claim 12, further comprising a staircase structure laterally neighboring the strings of memory cells and the additional insulative structures.

### Claim 16 (depends on 12)

The microelectronic device of claim 12, wherein the ratio of nitrogen atoms to silicon atoms is greater than about 1.60:1.00.

### Claim 17 (depends on 12)

The microelectronic device of claim 12, wherein the additional insulative structures of some of the second levels comprise a different ratio of nitrogen atoms to silicon atoms than the additional insulative structures of some other of the second levels.

### Claim 18 (depends on 12)

The microelectronic device of claim 12, wherein the additional insulative structures of vertically uppermost of the second levels and vertically lowermost of the second levels have a higher ratio of nitrogen atoms to silicon atoms than the additional insulative structures of other of the second levels.

### Claim 19

A method of forming a microelectronic device, the method comprising:
forming a stack structure comprising vertically alternating insulative structures and additional insulative structures arranged in tiers, the additional insulative structures horizontally extending through an array region of the stack structure to a peripheral region of the stack structure and individually having a ratio of nitrogen atoms to silicon atoms greater than about 1.58:1.00;
forming strings of memory cell vertically extending through the stack structure and within horizontal boundaries of the array region of the stack structure;
forming slots vertically extending through the stack structure and within the horizontal boundaries of the array region of the stack structure; and
replacing portions of the additional insulative structures within the array region of the stack structure with conductive structures while maintaining additional portions of the additional insulative structures within the peripheral region of the stack structure.

### Claim 20 (depends on 19)

The method of claim 19, wherein forming the additional insulative structures comprises forming the additional insulative structures to have a density within a range from about 2.45 g/cm3 to about 2.55 g/cm3.

### Claim 21 (depends on 19)

The method of claim 19, wherein forming the stack structure comprises forming some of the additional insulative structures to have a different ratio of nitrogen atoms to silicon atoms than at least some other of the additional insulative structures.

### Claim 22 (depends on 19)

The method of claim 19, further comprising selecting the ratio of nitrogen atoms to silicon atoms of the additional insulative structures to be within a range from about 1.60:1.00 to about 1.65:1.00.

### Claim 23 (depends on 19)

The method of claim 19, wherein forming strings of memory cells vertically extending through the stack structure comprises:
removing portions of the insulative structures and the additional insulative structures to form openings horizontally within and partially vertically extending through the array region of the stack structure;
forming a protective material on sidewalls defining the openings;
removing additional portions of the insulative structures and the additional insulative structures to increase a vertical dimension of the openings; and
forming a channel material within the openings after increasing the vertical dimension thereof.

### Claim 24 (depends on 19)

The method of claim 19, wherein forming a stack structure comprises forming a vertically uppermost of the additional insulative structures and a vertically lowermost of the additional insulative structures to have a lower refractive index than other of the additional insulative structures more proximate a vertical center of the stack structure.

### Claim 25

A memory device, comprising:
a stack structure comprising:
an array region comprising a vertically alternating sequence of insulative structures and conductive structures arranged in tiers; and
a peripheral region comprising a vertically alternating sequence of the insulative structures and additional insulative structures arranged in additional tiers horizontally neighboring the tiers of the array region, at least some of the additional insulative structures comprising silicon nitride comprising greater than or equal to about 1.60 silicon atoms for every about 1.00 nitrogen atom; and
strings of memory cells in the array region of the stack structure and comprising a channel material vertically extending through the stack structure.

### Claim 26 (depends on 25)

The memory device of claim 25, wherein the array region is substantially free of the additional insulative structures.

### Claim 27 (depends on 25)

The memory device of claim 25, wherein each of the additional insulative structures horizontally neighbors and is positioned at substantially the same vertical elevated as one of conductive structures.

### Claim 28 (depends on 25)

The memory device of claim 25, wherein the strings of memory cells further comprise a memory material comprising silicon nitride.

### Claim 29 (depends on 25)

The memory device of claim 25, wherein a ratio of nitrogen atoms to silicon atoms of the at least some of the additional insulative structures is greater than about 1.62:1.00.

### Claim 30

An electronic system, comprising:
an input device;
an output device;
a processor device operably coupled to the input device and the output device; and
a memory device operably coupled to the processor device and comprising at least one microelectronic device structure, the at least one microelectronic device structure comprising:
an array region comprising strings of memory cells vertically extending through a vertically alternating sequence of insulative structures and conductive structures; and
a peripheral region comprising a vertically alternating sequence of the insulative structures and additional insulative structures, the additional insulative structures of the peripheral region vertically aligned with the conductive structures of the array region, and at least some of the additional insulative structures comprising a ratio of silicon atoms to nitrogen atoms greater than about 1.58:1.00.