# US 2022/0293587 A1 · Methods for reduction of photoresist defect

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293587 A1
- Document ID: US20220293587A1
- Status: Published application
- Kind: A1
- Application number: 17/199,123
- Filed: 2021-03-11
- Published: 2022-09-15
- Earliest claimed: 2021-03-11
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chun-Wei LIAO; Hui-Chun LEE
- Web page: https://patentgrep.com/patent/US20220293587A1

## CPC

- H10D 89/814: {involving a parasitic bipolar transistor triggered by the electrical biasing of the gate electrode of the FET, e.g. gate coupled transistors}
- G03F 7/0035: {Multiple processes, e.g. applying a further resist layer on an already in a previously step, processed pattern or textured surface}
- G03F 7/0043: {Chalcogenides; Silicon, germanium, arsenic or derivatives thereof; Metals, oxides or alloys thereof (G03F7/0044 takes precedence)}
- G03F 7/2004: {characterised by the use of a particular light source, e.g. fluorescent lamps or deep UV light}
- G03F 7/40: Treatment after imagewise removal, e.g. baking
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The present disclosure in various embodiments provides a hardened resist layer that can reduce resist scum defects in a resist layer. In one embodiment, a lithography method is provided. The method includes forming a resist layer over a substrate, performing an exposure process on the resist layer, performing a developing process on the resist layer to form a patterned resist layer having a plurality resist segments, exposing the patterned resist layer to a vacuum ultraviolet (VUV) radiation, and subjecting the resist pattern a de-scum process.

## Claims

### Claim 1

A lithography method, comprising:
forming a resist layer over a substrate;
performing an exposure process on the resist layer;
performing a developing process on the resist layer to form a patterned resist layer having a plurality resist segments;
exposing the patterned resist layer to a vacuum ultraviolet (VUV) radiation; and
subjecting the resist pattern a de-scum process.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
after exposing the patterned resist layer to VUV radiation, heating the patterned resist layer from a first temperature to a second temperature that is greater than the first temperature.

### Claim 3 (depends on 1)

The method of claim 1, wherein the VUV radiation is emitted at an exposure energy directed to reduce a critical dimension of each resist segment.

### Claim 4 (depends on 1)

The method of claim 1, wherein exposing the patterned resist layer to a VUV radiation is performed under vacuum condition.

### Claim 5 (depends on 1)

The method of claim 1, wherein the de-scum process further comprises:
performing an ion bombardment process on the patterned resist layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the de-scum process further comprises:
after the ion bombardment process, performing an etching process on the patterned resist layer to remove a resist scum extending from the patterned resist layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the de-scum process is an etching process directed to remove a resist scum extending from the patterned resist layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the de-scum process is an etching process directed to remove a material layer disposed below the patterned resist layer.

### Claim 9 (depends on 1)

The method of claim 1, wherein the resist layer is a metal-containing photoresist.

### Claim 10 (depends on 1)

The method of claim 1, wherein the resist layer is a tri-layer photoresist.

### Claim 11 (depends on 1)

The method of claim 1, wherein the VUV radiation is emitted at a plurality of pulses.

### Claim 12

A lithography method, comprising:
performing a developing process on a resist layer to form a patterned resist layer having a plurality resist segments, wherein each resist segment has a first critical dimension after the developing process;
exposing the patterned resist layer to a photon radiation having a wavelength of 400 nm or below, wherein each resist segment has a second critical dimension after exposing the patterned resist layer to the photon radiation, and the second critical dimension is smaller than the first critical dimension;
bombarding the patterned resist layer with energetic particles directed to remove a resist scum extending from the patterned resist layer, wherein each resist segment has a third critical dimension after the bombardment process, and the third critical dimension is smaller than the second critical dimension; and
performing an etching process on the patterned resist layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the photon radiation is generated by striking a plasma formed from a gas mixture comprising an inert gas.

### Claim 14 (depends on 13)

The method of claim 13, wherein exposing the patterned resist layer to a photon radiation is performed under vacuum condition.

### Claim 15 (depends on 12)

The method of claim 12, further comprising:
after exposing the patterned resist layer to the photon radiation, heating the patterned resist layer from a first temperature to a second temperature that is greater than the first temperature.

### Claim 16 (depends on 12)

The method of claim 12, wherein the resist layer is a metal oxide based photoresist.

### Claim 17

A lithography method, comprising:
forming a patterned resist layer over a substrate, wherein the patterned resist layer has a plurality resist segments;
hardening the patterned resist layer in a vacuum chamber by exposing the patterned resist layer to a vacuum ultraviolet (VUV) light, wherein the patterned resist layer has a reduced critical dimension after the VUV exposure; and
performing an etching process directed to remove a material layer disposed below the patterned resist layer, wherein the material layer is etched using the patterned resist layer as a mask.

### Claim 18 (depends on 17)

The method of claim 17, further comprising:
after hardening the patterned resist layer, performing a baking process on the patterned resist layer to heat the patterned resist layer from a first temperature to a second temperature that is greater than the first temperature.

### Claim 19 (depends on 18)

The method of claim 18, further comprising:
after the baking process, performing an ion bombardment process on the patterned resist layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the resist layer is a metal-containing photoresist.