# US 2022/0293464 A1 · Semiconductor manufacturing method and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293464 A1
- Document ID: US20220293464A1
- Status: Published application
- Kind: A1
- Application number: 17/469,291
- Filed: 2021-09-08
- Published: 2022-09-15
- Earliest claimed: 2021-03-15
- Assignees: Kioxia Corporation
- Applicants: Kioxia Corporation
- Inventors: Kenichi IDE
- Web page: https://patentgrep.com/patent/US20220293464A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- H10W 20/055: {by formation methods other than physical vapour deposition [PVD], chemical vapour deposition [CVD] or liquid deposition}
- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10W 20/082: {the openings being tapered via holes}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor manufacturing method includes forming a concave portion in a layer provided above a substrate from a top surface of the layer downwards, the layer including an insulation layer at least partially. The method includes forming a silicon film on an inner surface of the concave portion. The method includes exposing the silicon film to a raw material gas of metal and an inhibitor gas that inhibits growth of the metal at a first temperature, to replace a first portion of the silicon film located in an upper-end side portion of the concave portion with a first conductive film containing the metal. The method includes exposing the silicon film to the raw material gas and the inhibitor gas at a second temperature lower than the first temperature, to replace a second portion of the silicon film with a second conductive film containing the metal.

## Claims

### Claim 1

A semiconductor manufacturing method comprising:
forming a concave portion in a layer provided above a substrate from a top surface of the layer downwards, the layer including an insulation layer at least partially;
forming a silicon film on an inner surface of the concave portion;
exposing the silicon film to a raw material gas of metal and an inhibitor gas that inhibits growth of the metal at a first temperature, to replace a first portion of the silicon film located in an upper-end side portion of the concave portion with a first conductive film containing the metal; and
exposing the silicon film to the raw material gas and the inhibitor gas at a second temperature lower than the first temperature, to replace a second portion of the silicon film different from the first portion with a second conductive film containing the metal.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a conductive layer containing the metal on the first conductive film and the second conductive film.

### Claim 3 (depends on 1)

The method of claim 1, wherein by exposing the silicon film to the raw material gas and the inhibitor gas at the second temperature, the second portion is replaced with the second conductive film and the conductive layer containing the metal is formed on the first conductive film and the second conductive film.

### Claim 4 (depends on 1)

The method of claim 1, wherein a time of exposing the silicon film to the raw material gas and the inhibitor gas at the first temperature is shorter than a time of exposing the silicon film to the raw material gas and the inhibitor gas at the second temperature.

### Claim 5 (depends on 2)

The method of claim 2, wherein a time of exposing the silicon film to the raw material gas and the inhibitor gas at the first temperature is shorter than a time of exposing the silicon film to the raw material gas and the inhibitor gas at the second temperature.

### Claim 6 (depends on 3)

The method of claim 3, wherein a time of exposing the silicon film to the raw material gas and the inhibitor gas at the first temperature is shorter than a time of exposing the silicon film to the raw material gas and the inhibitor gas at the second temperature.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first conductive film is higher in concentration of a component of the inhibitor gas than the second conductive film.

### Claim 8 (depends on 2)

The method of claim 2, wherein the first conductive film is higher in concentration of a component of the inhibitor gas than the second conductive film.

### Claim 9 (depends on 3)

The method of claim 3, wherein the first conductive film is higher in concentration of a component of the inhibitor gas than the second conductive film.

### Claim 10 (depends on 4)

The method of claim 4, wherein the first conductive film is higher in concentration of a component of the inhibitor gas than the second conductive film.

### Claim 11 (depends on 1)

The method of claim 1, further comprising forming a metal film on the inner surface of the concave portion prior to formation of the silicon film.

### Claim 12 (depends on 1)

The method of claim 1, wherein the metal is tungsten.

### Claim 13 (depends on 12)

The method of claim 12, wherein
the raw material gas is tungsten hexafluoride gas and
the inhibitor gas is nitrogen gas.

### Claim 14 (depends on 1)

The method of claim 1, wherein
the first temperature is 400° C. or higher and
the second temperature is lower than 400° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the silicon film is formed to have a thickness of 0.5 to 10 nm.

### Claim 16 (depends on 1)

The method of claim 1, wherein a width of the concave portion is the maximum at a first position between an upper end and a lower end of the concave portion, increases from the upper end toward the first position, and decreases from the first position toward the lower end.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first portion is a portion of the silicon film formed on a range from the upper end of the concave portion to a second position above the first position.

### Claim 18

A semiconductor device comprising:
a layer provided above a substrate, provided with a concave portion from its top surface downwards, and including an insulation layer at least partially;
a first conductive film provided on a first range that is an upper-end side portion of an inner surface of the concave portion, and containing metal and an inhibitor that inhibits growth of the metal;
a second conductive film provided on a second range of the inner surface of the concave portion and containing the metal and the inhibitor, the second range being different from the first range; and
a conductive layer provided on the first conductive film and the second conductive film and containing the metal, wherein
the first conductive film is higher in concentration of the inhibitor than the second conductive film.

### Claim 19 (depends on 18)

The device of claim 18, wherein
the metal is tungsten and
the inhibitor is nitrogen.

### Claim 20 (depends on 18)

The device of claim 18, wherein the layer including the insulation layer is a stack of the insulation layer and a conductive layer.