# US 2022/0293427 A1 · System and method for fabricating photonic device elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293427 A1
- Document ID: US20220293427A1
- Status: Published application
- Kind: A1
- Application number: 17/635,081
- Filed: 2020-07-28
- Published: 2022-09-15
- Earliest claimed: 2019-08-14
- Assignees: Paul Scherrer Institut
- Applicants: Paul Scherrer Institut
- Inventors: Lucia Romano; Konstantins Jefimovs; Matias Kagias; Joan Vila Comamala; Marco Stampanoni
- Web page: https://patentgrep.com/patent/US20220293427A1

## CPC

- H10P 50/642: {Chemical etching}
- B81C 1/00619: {Forming high aspect ratio structures having deep steep walls}
- G02B 5/1857: {using exposure or etching means, e.g. holography, photolithography, exposure to electron or ion beams}
- H10F 77/122: comprising only Group IV materials
- H10P 50/691: {for Group IV materials or Group III-V materials}
- H10P 50/694: {characterised by their behaviour during the process, e.g. soluble masks or redeposited masks}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- B82Y 40/00: Manufacture or treatment of nanostructures
- C09K 13/08: containing a fluorine compound
- G02B 5/1838: {for use with ultraviolet radiation or X-rays}
- H10F 71/121: {The active layers comprising only Group IV materials}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Elements of photonic devices with high aspect ratio patterns are fabricated. A stabilizing catalyst that forms a stable metal-semiconductor alloy allows to etch a substrate in vertical direction even at very low oxidant concentration without external bias or magnetic field. A metal layer on the substrate reacts with the oxidant contained in air and catalyzes the semiconductor etching by the etchant. Air in continuous flow at the metal layer allows to maintain constant the oxidant concentration in proximity of the metal layer. The process can continue for a long time in order to form very high aspect ratio structures in the order of 10,000:1. Once the etched semiconductor structure is formed, the continuous air flow supports the reactant species diffusing through the etched semiconductor structure to maintain a uniform etching rate. The continuous air flow supports the diffusion of reaction by-products to avoid poisoning of the etching reaction.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method for fabricating photonic device elements by means of metal assisted chemical etching in gas phase, the method comprising the following steps:
(a) providing a semiconductor substrate and a patterned metal layer on the semiconductor substrate;
(b) exposing the semiconductor substrate and the patterned metal layer to reactants in gas phase, the reactants including an oxidant gas and an etchant gas;
the oxidant gas comprising air and the etchant gas comprising hydrofluoric acid;
supplying the reactants in a continuous or pulsed flow to the semiconductor substrate and the patterned metal layer on the semiconductor substrate;
locally increasing a concentration of oxygen in the oxidant gas by decomposing H2O2 on a platinum surface, being a solid piece containing platinum immersed in a liquid solution containing H2O2, with a decomposition of H2O2 in the liquid phase on the platinum surface producing O2 in gas phase; and
wherein the liquid solution is placed in a container and the liquid is not in contact with the semiconductor substrate and the patterned metal on the semiconductor substrate.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the etchant comprises hydrofluoric acid (HF) in vapor phase as evaporated from a liquid solution containing water diluted HF.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the semiconductor substrate contains a semiconductor selected from the group consisting of: Si, Ge, or an alloy containing elements from groups III and V in the periodic table and wherein the final metal layer contains a metal selected from the group consisting of: Au, Ag, Pt, Pd, Cu, Ni, Rh.

### Claim 20 (depends on 17)

The method according to claim 17, which comprises heating the semiconductor substrate and the metal patterned layer thereon to a temperature in a range from 30° C. to 90° C. during the step of exposing to the oxidant gas and the etchant.

### Claim 21 (depends on 17)

The method according to claim 17, which comprises carrying out the method in presence of an inert gas selected from the group consisting of nitrogen, argon, and helium.

### Claim 22 (depends on 17)

The method according to claim 17, which comprises carrying out the method in the presence of an alcohol selected from the group consisting of isopropanol, methanol, and ethanol.

### Claim 23 (depends on 17)

The method according to claim 17, which comprises supplying the etchant gas to an enclosed etching chamber by way of a dedicated gas line.

### Claim 24 (depends on 17)

The method according to claim 17, wherein the patterned metal layer comprises a continuous mesh pattern, and the etched semiconductor structure comprises an array of nanowires with an aspect ratio of at least 10:1.

### Claim 25 (depends on 17)

The method according to claim 17, wherein the patterned metal layer comprises an X-ray diffractive grating pattern with periodic features, and the etched semiconductor structure comprises an X-ray diffractive grating with periodic features.

### Claim 26

A method of fabricating photonic device elements by metal assisted chemical etching with reactants in liquid or gas phase, to form a semiconductor substrate and a patterned metal layer thereon, the method comprising the steps of:
(a) forming a semiconductor oxide on the semiconductor substrate;
(b) forming a plurality of different metal layers in the patterned metal layer, wherein a first metal layer is in contact with the semiconductor oxide of the substrate, a final metal layer is in contact with an etching reactant, with the first metal layer containing metals that form a stable metal-semiconductor alloy of a compound selected from the group consisting of silicides and germanides of one or more metals selected from the group containing Pt, Pd, Cu, Ni and Rh;
(c) heating the substrate and the metal layer thereon in order to realize, at the same time, a formation of the metal-semiconductor alloy and a metal dewetting, the metal dewetting forming an interconnected metal pattern having features, with the features of the interconnected metal pattern being holes in the metal layer, and the holes having a feature size of at least 1 nm.

### Claim 27 (depends on 26)

The method according to claim 26, which comprises providing the semiconductor substrate having a semiconductor selected from the group consisting of Si, Ge, and an alloy containing elements from groups III and V in the periodic table, and wherein the final metal layer contains a metal selected from the group consisting of Au, Ag, Pt, Pd, Cu, Ni, and Rh.

### Claim 28 (depends on 26)

The method according to claim 26, wherein the reactant gas comprises air.

### Claim 29 (depends on 26)

The method according to claim 26, wherein the reactant gas comprises as etching reactant HF in vapor phase as evaporated from a liquid solution containing water diluted HF.

### Claim 30 (depends on 26)

The method according to claim 26, which comprises heating the semiconductor substrate and the metal patterned layer thereon to a temperature in a range from 30° C. to 90° C. during the step of exposing to the reactant gas.

### Claim 31 (depends on 26)

The method according to claim 26, wherein the patterned metal layer comprises a continuous mesh pattern, and the etched semiconductor structure comprises an array of nanowires with an aspect ratio of at least 10:1.

### Claim 32 (depends on 26)

The method according to claim 26, wherein the patterned metal layer comprises an X-ray diffractive grating pattern with periodic features, and the etched semiconductor structure comprises an X-ray diffractive grating with periodic features.