# US 2022/0293422 A1 · Semiconductor structure and preparation method for semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293422 A1
- Document ID: US20220293422A1
- Status: Published application
- Kind: A1
- Application number: 17/401,405
- Filed: 2021-08-13
- Published: 2022-09-15
- Earliest claimed: 2021-03-11
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Zijie WANG; Huan XIA; Jun WEI; Yuanhao GAO
- Web page: https://patentgrep.com/patent/US20220293422A1

## CPC

- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10D 64/01: Manufacture or treatment
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10B 12/485: {Bit line contacts}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor structure and a preparation method for a semiconductor structure are provided. The preparation method includes: a substrate is provided; and a first material layer and a second material layer are formed on the substrate, and thermal treatment is performed on the first material layer and the second material layer to convert the first material layer into an ohmic contact layer and convert the second material layer into an ion barrier layer.

## Claims

### Claim 1

A preparation method for a semiconductor structure, comprising:
providing a substrate; and
forming a first material layer and a second material layer on the substrate, and performing thermal treatment on the first material layer and the second material layer to convert the first material layer into an ohmic contact layer and convert the second material layer into an ion barrier layer.

### Claim 2 (depends on 1)

The preparation method for a semiconductor structure of claim 1, wherein forming the first material layer and the second material layer on the substrate and performing the thermal treatment on the first material layer and the second material layer comprises:
forming the first material layer on the substrate;
forming the second material layer on the first material layer; and
performing the thermal treatment on the first material layer and the second material layer simultaneously to convert the first material layer into the ohmic contact layer and convert the second material layer into the ion barrier layer.

### Claim 3 (depends on 2)

The preparation method for a semiconductor structure of claim 2, wherein the substrate comprises a silicon substrate, and forming the first material layer on the substrate comprises:
forming, on the substrate, a titanium layer as the first material layer by a deposition process.

### Claim 4 (depends on 3)

The preparation method for a semiconductor structure of claim 3, wherein the deposition process comprises a physical vapor deposition process.

### Claim 5 (depends on 3)

The preparation method for a semiconductor structure of claim 3, wherein the titanium layer has a thickness of 1 nm to 5 nm.

### Claim 6 (depends on 3)

The preparation method for a semiconductor structure of claim 3, wherein forming the second material layer on the first material layer comprises:
forming the second material layer on the first material layer by a deposition process, the second material layer comprising a plurality of titanium nitride layers and silicon nitride layers arranged alternately.

### Claim 7 (depends on 6)

The preparation method for a semiconductor structure of claim 6, wherein the deposition process comprises an atomic layer deposition process.

### Claim 8 (depends on 6)

The preparation method for a semiconductor structure of claim 6, wherein performing the thermal treatment on the first material layer and the second material layer simultaneously to convert the first material layer into the ohmic contact layer and convert the second material layer into the ion barrier layer comprises:
performing the thermal treatment on the first material layer and the second material layer simultaneously, reacting the titanium layer with the silicon substrate to form a titanium silicide layer, and reacting the titanium nitride layer with the silicon nitride layer to form a titanium silicon nitride layer.

### Claim 9 (depends on 8)

The preparation method for a semiconductor structure of claim 8, wherein the titanium silicon nitride layer has a thickness of 1 nm to 5 nm.

### Claim 10 (depends on 1)

The preparation method for a semiconductor structure of claim 1, wherein forming the first material layer and the second material layer on the substrate and performing the thermal treatment on the first material layer and the second material layer comprises:
forming the first material layer on the substrate;
performing a first thermal treatment on the first material layer to convert the first material layer into the ohmic contact layer;
forming the second material layer on the ohmic contact layer; and
performing a second thermal treatment on the second material layer to convert the second material layer into the ion barrier layer.

### Claim 11 (depends on 10)

The preparation method for a semiconductor structure of claim 10, wherein the substrate comprises a silicon substrate, and forming the first material layer on the substrate comprises:
forming, on the silicon substrate, a titanium layer as the first material layer by a deposition process.

### Claim 12 (depends on 11)

The preparation method for a semiconductor structure of claim 11, wherein performing the first thermal treatment on the first material layer to convert the first material layer into the ohmic contact layer comprises:
reacting the titanium layer with the silicon substrate by the first thermal treatment to form a titanium silicide layer.

### Claim 13 (depends on 10)

The preparation method for a semiconductor structure of claim 10, wherein forming the second material layer on the ohmic contact layer comprises:
forming the second material layer on the ohmic contact layer by a deposition process, the second material layer comprising a plurality of titanium nitride layers and silicon nitride layers arranged alternately.

### Claim 14 (depends on 13)

The preparation method for a semiconductor structure of claim 13, wherein performing the second thermal treatment on the second material layer to convert the second material layer into the ion barrier layer comprises:
reacting the titanium nitride layer with the silicon nitride layer by the second thermal treatment to form a titanium silicon nitride layer.

### Claim 15 (depends on 1)

The preparation method for a semiconductor structure of claim 1, further comprising: after forming the first material layer and the second material layer on the substrate and performing the thermal treatment the first material layer and the second material layer, forming a conductive layer on the ion barrier layer.

### Claim 16 (depends on 2)

The preparation method for a semiconductor structure of claim 2, further comprising: after forming the first material layer and the second material layer on the substrate and performing the thermal treatment the first material layer and the second material layer,
forming a conductive layer on the ion barrier layer.

### Claim 17 (depends on 3)

The preparation method for a semiconductor structure of claim 3, further comprising: after forming the first material layer and the second material layer on the substrate and performing the thermal treatment the first material layer and the second material layer,
forming a conductive layer on the ion barrier layer.

### Claim 18 (depends on 4)

The preparation method for a semiconductor structure of claim 4, further comprising: after forming the first material layer and the second material layer on the substrate and performing the thermal treatment the first material layer and the second material layer,
forming a conductive layer on the ion barrier layer.

### Claim 19

A semiconductor structure, comprising a silicon substrate and a conductive layer having therebetween sequentially formed with:
a titanium silicide layer, formed on the silicon substrate and configured to form an ohmic contact with the silicon substrate; and
a titanium silicon nitride layer, formed on the titanium silicide layer and configured to block ions in the silicon substrate from diffusing to the conductive layer.

### Claim 20 (depends on 19)

The semiconductor structure of claim 19, wherein the titanium silicon nitride layer has a thickness of 1 nm to 5 nm.