# US 2022/0293415 A1 · Method for manufacturing semiconductor structure with reduced nodule defects

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293415 A1
- Document ID: US20220293415A1
- Status: Published application
- Kind: A1
- Application number: 17/199,033
- Filed: 2021-03-11
- Published: 2022-09-15
- Earliest claimed: 2021-03-11
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Che-Yu LIN; Chih-Chiang CHANG; Chien-Hung CHEN; Ming-Hua YU; Tsung-Hsi YANG; Ting-Yi HUANG; Chii-Horng LI; Yee-Chia YEO
- Web page: https://patentgrep.com/patent/US20220293415A1

## CPC

- H10P 50/268: {of silicon-containing layers}
- H10P 70/20: {Cleaning during device manufacture}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/6211: {having fin-shaped semiconductor bodies integral with the bulk semiconductor substrates}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10W 20/075: {of multilayered thin functional dielectric layers}
- H10W 20/076: {in via holes or trenches}
- H10W 20/081: {by forming openings in the dielectric parts}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/121: {oriented parallel to substrates}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method for removing nodule defects is disclosed. The nodule defects may be formed on a non-selected portion of a semiconductor structure during formation of a semiconductor region on a selected portion of the semiconductor structure. A plasma having a higher selectivity to etch the nodule defects relative to the semiconductor region may be used to selectively remove the nodule defects on the non-selected portion.

## Claims

### Claim 1

A method for eliminating nodule defects which are formed on a non-selected portion of a semiconductor structure during formation of a semiconductor region on a selected portion of the semiconductor structure, the method comprising
applying to the semiconductor structure a plasma which has a higher selectivity to etch the nodule defects relative to the semiconductor region, to thereby eliminate the nodule defects.

### Claim 2 (depends on 1)

The method of claim 1, wherein the plasma is generated from a gas source including hydrogen.

### Claim 3 (depends on 2)

The method of claim 2, wherein a flow rate of the hydrogen is controlled in a range from 10 sccm to 2000 sccm.

### Claim 4 (depends on 2)

The method of claim 2, wherein the gas source further includes a carrier gas selected from helium, argon, and a combination thereof.

### Claim 5 (depends on 4)

The method of claim 4, wherein a flow rate of the carrier gas is controlled in a range from 50 sccm to 6000 sccm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plasma is operated under a temperature ranging from 90° C. to 600° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the plasma is operated under a pressure ranging from 0.05 torr to 6 torr.

### Claim 8 (depends on 1)

The method of claim 1, wherein the plasma is generated by a plasma generation source selected from a transformer-coupled plasma generator, an inductively coupled plasma system, a magnetically enhanced reactive ion etching system, an electron cyclotron resonance system, or a remote plasma generator.

### Claim 9

A method for manufacturing a semiconductor structure, comprising:
forming two first recesses in two first regions of a first semiconductor portion;
forming first source-drain regions in the first recesses; and
applying a plasma to eliminate nodule defects formed on a dielectric portion, the plasma having a higher selectivity to etch the nodule defects relative to the first source-drain regions so as to eliminate the nodule defects.

### Claim 10 (depends on 9)

The method of claim 9, after the step of forming the first source-drain regions, further comprising:
forming two second recesses in two second regions of a second semiconductor portion; and
forming second source-drain regions in the second recesses of the second semiconductor portion.

### Claim 11 (depends on 10)

The method of claim 10, wherein the nodule defects are formed in at least one of the step of forming the first source-drain regions and the step of forming the second source-drain regions, and the plasma has a higher selectivity to etch the nodule defects relative to the first source-drain regions and the second source-drain regions.

### Claim 12 (depends on 10)

The method of claim 10, wherein the nodule defects have an amorphous phase, and the first source-drain regions and the second source-drain regions have a crystalline phase.

### Claim 13 (depends on 12)

The method of claim 12, wherein the plasma has a high selectivity to etch the amorphous phase relative to the crystalline phase.

### Claim 14 (depends on 11)

The method of claim 11, wherein the step of applying the plasma is implemented before the step of forming the two second recesses and after the step of forming the first source-drain regions.

### Claim 15 (depends on 11)

The method of claim 11, wherein the step of applying the plasma is implemented after the step of forming the second source-drain regions.

### Claim 16 (depends on 11)

The method of claim 11, wherein the step of applying the plasma is implemented after each of the step of forming the first source-drain regions and the step of forming the second source-drain regions.

### Claim 17 (depends on 9)

The method of claim 9, wherein the plasma is generated from a gas source including hydrogen.

### Claim 18 (depends on 9)

The method of claim 9,
wherein the first semiconductor portion is located on a semiconductor substrate;
wherein, after the step of forming the first source-drain regions, each of the first source-drain regions has an outermost sacrificial layer which includes a first region distal from the semiconductor substrate, and a second region proximate to the semiconductor substrate; and
wherein, after the step of applying the plasma, a thickness of the first region is smaller than a thickness of the second region.

### Claim 19

A semiconductor structure comprising:
a semiconductor substrate; and
a semiconductor portion formed on the semiconductor substrate, and having a channel region and two source-drain regions at two opposite sides of the channel region, each of the source-drain regions having an outermost sacrificial layer, the outermost sacrificial layer including a first region distal from the semiconductor substrate, and a second region proximate to the semiconductor substrate, a thickness of the first region being smaller than a thickness of the second region.

### Claim 20 (depends on 19)

The semiconductor structure of claim 19, wherein each of the source-drain regions has a diamond-like shape structure with a rounded corner.