# US 2022/0293413 A1 · Pattern Formation Through Mask Stress Management and Resulting Structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293413 A1
- Document ID: US20220293413A1
- Status: Published application
- Kind: A1
- Application number: 17/341,332
- Filed: 2021-06-07
- Published: 2022-09-15
- Earliest claimed: 2021-03-10
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Chun-Yi Chang; Chunyao Wang
- Web page: https://patentgrep.com/patent/US20220293413A1

## CPC

- H10P 50/71: {using masks for conductive or resistive materials}
- H10P 76/00: Manufacture or treatment of masks on semiconductor bodies, e.g. by lithography or photolithography
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/019: {of FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 30/501: {FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 62/121: {oriented parallel to substrates}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

As deposited, hard mask thin films have internal stress components which are an artifact of the material, thickness, deposition process of the mask layer as well as of the underlying materials and topography. This internal stress can cause distortion and twisting of the mask layer when it is patterned, especially when sub-micron critical dimensions are being patterned. A stress-compensating process is employed to reduce the impact of this internal stress. Heat treatment can be employed to relax the stress, as an example. In another example, a second mask layer with an opposite internal stress component is employed to offset the internal stress component in the hard mask layer.

## Claims

### Claim 1

A method for forming a semiconductor device, comprising:
forming a material layer over a substrate;
forming a mask layer over the material layer, the mask layer having an internal stress; and
performing a stress-compensating process on the mask layer to adjust the internal stress of the mask layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of performing a stress-compensating process on the mask layer includes performing a thermal process on the mask layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the thermal process is a rapid thermal anneal process.

### Claim 4 (depends on 2)

The method of claim 2, wherein the thermal process is a furnace anneal process.

### Claim 5 (depends on 1)

The method of claim 1, wherein the stress-compensating process includes forming a second mask layer on the mask layer, the second mask layer having a compensating internal stress relative to the mask layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the mask layer has a tensile internal stress and the second mask layer has a compressive internal stress.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
patterning the mask layer after performing the stress-compensating process on the mask layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein patterning the mask layer includes forming a photoresist layer on the mask layer, patterning the photoresist layer, and etching the mask layer using the patterned photoresist layer as an etch mask.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
using the mask layer as a hard mask to pattern the material layer.

### Claim 10

A method for forming a semiconductor device, comprising:
depositing on a substrate a layer to be patterned;
depositing over the layer to be patterned a mask layer having an internal stress;
at least partially compensating for the internal stress of the mask layer; and
patterning the mask layer after the step of at least partially compensating for the internal stress.

### Claim 11 (depends on 10)

The method of claim 10, wherein the step of at least partially compensating for the internal stress of the mask layer includes subjecting the mask layer to a thermal treatment to relax the internal stress.

### Claim 12 (depends on 10)

The method of claim 10, wherein the step of at least partially compensating for the internal stress of the mask layer includes depositing a second mask layer having a second internal stress that offsets the internal stress of the mask layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the internal stress is tensile or compressive and the second internal stress is compressive or tensile, respectively.

### Claim 14 (depends on 13)

The method of claim 13, wherein the compressive internal stress and the tensile internal stress have the same magnitude.

### Claim 15 (depends on 10)

The method of claim 10, further comprising:
patterning the layer to be patterned after patterning the mask layer, through etching, selective doping, or selective growth of material on the layer to be patterned.

### Claim 16 (depends on 10)

The method of claim 10 wherein the mask layer is a material selected from the group consisting of silicon oxide, silicon nitride, silicon oxy-nitride, a metal nitride, and a metal oxide.

### Claim 17

A method of forming a semiconductor device, comprising:
forming a material layer on a substrate;
depositing a mask layer on the material layer, the mask layer having an internal stress value;
reducing the internal stress value of the mask layer; and
patterning the mask layer after the step of reducing the internal stress value of the mask layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the step of reducing the internal stress value of the mask layer includes subjecting the mask layer to a heat treatment to reduce the internal stress.

### Claim 19 (depends on 17)

The method of claim 17, wherein the step of reducing the internal stress value of the mask layer includes forming a first mask sub-layer having a first stress and forming on the first mask sub-layer a second mask sub-layer having a second stress, the second stress offsetting the first stress.

### Claim 20 (depends on 19)

The method of claim 19, wherein the first stress is compressive and the second stress is tensile.