# US 2022/0293316 A1 · Magnetic base body, coil component, and circuit board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293316 A1
- Document ID: US20220293316A1
- Status: Published application
- Kind: A1
- Application number: 17/672,575
- Filed: 2022-02-15
- Published: 2022-09-15
- Earliest claimed: 2021-03-12
- Assignees: Taiyo Yuden Co., Ltd.
- Applicants: Taiyo Yuden Co., Ltd.
- Inventors: Kazuki MISAWA; Takashi NAKAJIMA
- Web page: https://patentgrep.com/patent/US20220293316A1

## CPC

- H01F 1/33: mixtures of metallic and non-metallic particles; metallic particles having oxide skin
- H01F 1/14766: {Fe-Si based alloys}
- H01F 1/24: the particles being insulated
- H01F 27/255: made from particles (H01F27/26 takes precedence)
- H01F 17/0013: {with stacked layers}
- H01F 17/045: {with core of cylindric geometry and coil wound along its longitudinal axis, i.e. rod or drum core}
- H01F 2017/048: {with encapsulating core, e.g. made of resin and magnetic powder}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A magnetic base body is constituted by: metal magnetic grains containing Fe, and Si as an optional component, where the total content of the Fe and Si is 99% by mass or higher; and oxide layers present between the metal magnetic grains; wherein the ratio (IFe2SiO4/IFe) of the strongest diffraction line intensity (IFe2SiO4) observed in a range of 30.8°≤2θ≤32.2° to the strongest diffraction line intensity (IFe) observed in a range of 43.8°≤2θ≤45.2° in X-ray diffraction measurement using the CuKα ray is 0.0020 or higher; and the ratio (IFe2O3/IFe) of the strongest diffraction line intensity (IFe2O3) observed in a range of 33.0°≤2θ≤34.4° to the IFe in X-ray diffraction measurement using the CuKα ray is lower than 0.0010.

## Claims

### Claim 1

A magnetic base body, comprising:
metal magnetic grains containing Fe, and Si as an optional component, where a total content of the Fe and Si is 99% by mass or higher; and
oxide layers present between the metal magnetic grains;
wherein a ratio (IFe2SiO4/IFe) of a strongest diffraction line intensity (IFe2SiO4) observed in a range of 30.8°≤2θ≤32.2° to a strongest diffraction line intensity (IFe) observed in a range of 43.8°≤2θ≤45.2° in X-ray diffraction measurement using a CuKα ray is 0.0020 or higher; and
a ratio (IFe2O3/IFe) of a strongest diffraction line intensity (IFe2O3) observed in a range of 33.0°≤2θ≤34.4° to the IFe in X-ray diffraction measurement using a CuKα ray is lower than 0.0010.

### Claim 2 (depends on 1)

The magnetic base body according to claim 1, wherein the oxide layers have:
first regions where a molar ratio of Si to Fe (Si/Fe) is 2 or higher; and
second regions where a molar ratio (Si/Fe) is 1 or lower.

### Claim 3 (depends on 2)

The magnetic base body according to claim 2, wherein the first regions are present in a manner sandwiching the second regions.

### Claim 4 (depends on 1)

A coil component, comprising the magnetic base body according to claim 1, and a conductor placed inside or on a surface of the magnetic base body.

### Claim 5 (depends on 4)

A circuit board on which the coil component according to claim 4 is mounted.