# US 2022/0293315 A1 · Internally Embedded Copper Plate-Type Soft Magnetic Powder Core Inductor, Preparation Method Therefor, and Use Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293315 A1
- Document ID: US20220293315A1
- Status: Published application
- Kind: A1
- Application number: 17/631,341
- Filed: 2020-06-30
- Published: 2022-09-15
- Earliest claimed: 2020-01-17
- Assignees: Shenzhen Boke New Material Co., Ltd.; Huizhou Poco Magnetic Co., Ltd.; Huizhou Boke Industry Co., Ltd.
- Applicants: Shenzhen Boke New Material Co., Ltd.; Huizhou Poco Magnetic Co., Ltd.; Huizhou Boke Industry Co., Ltd.
- Inventors: Yunfan Zhang; Xiongzhi Guo; Qiang Xiao; Guohua Wang; Yixuan Li; Kai He; Xuemin Chen; Jialin Ruan; Yunkai Cao; Zhengping Li
- Web page: https://patentgrep.com/patent/US20220293315A1

## CPC

- H01F 1/26: by macromolecular organic substances
- H01F 17/04: with magnetic core
- H01F 1/14758: {by macromolecular organic substances}
- H01F 1/14791: {Fe-Si-Al based alloys, e.g. Sendust}
- H01F 27/245: made from sheets, e.g. grain-oriented (H01F27/26 takes precedence)
- H01F 27/255: made from particles (H01F27/26 takes precedence)
- H01F 27/2847: {Sheets; Strips (H01F27/2866 takes precedence)}
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- H01F 41/125: {Other insulating structures; Insulating between coil and core, between different winding sections, around the coil}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The present application relates to an internally embedded copper plate-type soft magnetic powder core inductor, a preparation method therefor, and a use thereof. The internally embedded copper plate-type soft magnetic powder core inductor comprises a copper plate, a surface of the copper plate is covered with a soft magnetic material, and an interfacing area of the soft magnetic material and the copper plate includes an insulating resin material. The internally embedded copper plate-type soft magnetic powder core inductor possesses high density, high magnetic core magnetic permeability, high inductance, high saturated magnetic flux density, low volume, and low magnetic flux leakage, if said powder core inductor is used to replace a ferrite inductor of a same inductance for a low voltage DC/DC converter circuit, the same or greater efficiency can be achieved, and inductor volume can be reduced by at least half; the withstand voltage of the internally embedded copper plate type soft magnetic powder core inductor can reach over 15V, and the preparation method for said inductor is simple, possessing high production efficiency and suitable for large-scale automated production.

## Claims

### Claim 1

A copper sheet-embedded soft magnetic powder core inductor, comprising:
a copper sheet,
a soft magnetic material covered on a surface of the copper sheet, and
an insulating resin material contained on an interface between the copper sheet and the soft magnetic material.

### Claim 2 (depends on 1)

The copper sheet-embedded soft magnetic powder core inductor according to claim 1, wherein the soft magnetic material in the copper sheet-embedded soft magnetic powder core inductor has a density of 5.5-6.5 g/cm3.

### Claim 3 (depends on 1)

The copper sheet-embedded soft magnetic powder core inductor according to claim 1, wherein the soft magnetic material is obtained through soft magnetic metal powder subjected to press molding.

### Claim 4 (depends on 1)

A method for preparing the copper sheet-embedded soft magnetic powder core inductor according to claim 1, the method comprising the following steps:
(a) coating an insulating resin material on a surface of a copper sheet, baking and curing; and
(b) placing the copper sheet coated with the insulating resin material and obtained in step (a) in soft magnetic metal powder, press molding, and annealing in an inert atmosphere to obtain the copper sheet embedded soft magnetic powder core inductor.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the soft magnetic metal powder in step (b) has an average particle size of 2-25 μm.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the annealing in step (b) is carried out at a temperature of 550-700° C.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the insulating resin material in step (a) comprises an organosilicon resin material.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the press molding in step (b) is carried out at a pressure of 12-18 T/cm2.

### Claim 9 (depends on 4)

The method according to claim 4, wherein the inert atmosphere is nitrogen.

### Claim 10 (depends on 1)

A method for preparing the copper sheet-embedded soft magnetic powder core inductor according to claim 1, the method comprising the following steps:
(a) coating an organosilicon resin material on a surface of a copper sheet, baking and curing; and
(b) placing the copper sheet coated with the organosilicon resin material and obtained in step (a) in soft magnetic metal powder with an average particle size of 10 μm, press molding at a pressure of 12-18 T/cm2 to obtain a molded body, and placing the molded body in an annealing furnace for annealing at 550-700° C. in an inert atmosphere for 1-3 hours to obtain the copper sheet-embedded soft magnetic powder core inductor.

### Claim 11 (depends on 1)

A low-voltage DC/DC converter circuit comprising the copper sheet-embedded soft magnetic powder core inductor according to claim 1.

### Claim 12 (depends on 3)

The copper sheet-embedded soft magnetic powder core inductor according to claim 3, wherein the soft magnetic metal powder comprises any one selected from the group consisting of iron powder, iron-silicon powder, iron-silicon-aluminium powder, iron-nickel powder, iron-nickel-molybdenum powder, and a combination of at least two selected therefrom.

### Claim 13 (depends on 1)

The copper sheet-embedded soft magnetic powder core inductor according to claim 1, wherein the insulating resin material comprises an organosilicon resin material.

### Claim 14 (depends on 4)

The method according to claim 4, wherein the annealing in step (b) is carried out for 1-3 hours.

### Claim 15 (depends on 4)

The method according to claim 4, wherein the soft magnetic metal powder in step (b) comprises any one selected from the group consisting of iron powder, iron-silicon powder, iron-silicon-aluminium powder, iron-nickel powder, iron-nickel-molybdenum powder, and a combination of at least two selected therefrom.