# US 2022/0293314 A1 · Amorphous nanocrystalline soft magnetic material, preparation method therefor and use thereof, amorphous ribbon material, amorphous nanocrystalline ribbon material, and amorphous nanocrystalline magnetic sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2022/0293314 A1
- Document ID: US20220293314A1
- Status: Published application
- Kind: A1
- Application number: 17/624,979
- Filed: 2020-06-09
- Published: 2022-09-15
- Earliest claimed: 2019-07-19
- Assignees: Hengdian Group Dmegc Magnetics Co., Ltd
- Applicants: Hengdian Group Dmegc Magnetics Co., Ltd
- Inventors: Yangyang Liu; Yaqi Fu
- Web page: https://patentgrep.com/patent/US20220293314A1

## CPC

- H01F 1/15333: {containing nanocrystallites, e.g. obtained by annealing}
- C21D 1/26: Methods of annealing
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 1/78: Combined heat-treatments not provided for above
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0236: {Cold rolling}
- C21D 8/1244: characterised by the heat treatment
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C22C 33/003: {making amorphous alloys}
- C22C 45/02: with iron as the major constituent
- H01F 1/15341: {Preparation processes therefor}
- C21D 2201/03: Amorphous or microcrystalline structure
- C22C 2200/02: Amorphous
- C22C 2202/02: Magnetic
- H01F 27/366: {made of ferromagnetic material}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Disclosed are an amorphous nanocrystalline soft magnetic material, a preparation method therefor and an application thereof, an amorphous ribbon material, an amorphous nanocrystalline ribbon material, and an amorphous nanocrystalline magnetic sheet. The soft magnetic material comprises an amorphous matrix phase, a nanocrystalline phase distributed in the amorphous matrix phase, and fine crystalline particles distributed in the amorphous matrix phase and the nanocrystalline phase. The amorphous matrix phase comprises Fe, Si, and B, the fine crystalline particles comprise metal carbides, and the soft magnetic material comprises Fe, Si, B, P, and Cu.

## Claims

### Claim 1

An amorphous nanocrystalline soft magnetic material, comprising an amorphous matrix phase, a nanocrystalline phase distributed in the amorphous matrix phase, and a fine crystalline particle distributed in the amorphous matrix phase and the nanocrystalline phase, wherein the amorphous matrix phase comprises Fe, Si and B; the fine crystalline particle comprises metal carbides; and the amorphous nanocrystalline soft magnetic material comprises Fe, Si, B, P and Cu.

### Claim 2 (depends on 1)

The amorphous nanocrystalline soft magnetic material according to claim 1, wherein the amorphous nanocrystalline soft magnetic material has a molecular formula of FeaSibBcCudPeMf(XC)h, wherein M is selected from any one or a combination of at least two of Ta, W, Mo, Ge, Zr, Hf or Y; X is Nb and/or V; 1≤b≤12, 3≤c≤10, 0.5≤d≤3, 1≤e≤7, 0≤f≤8, 0.1≤h≤2, and a+b+c+d+e+f+h=100.

### Claim 3 (depends on 2)

The amorphous nanocrystalline soft magnetic material according to claim 2, wherein the amorphous matrix phase further comprises M.

### Claim 4 (depends on 2)

The amorphous nanocrystalline soft magnetic material according to claim 2, wherein the amorphous matrix phase further comprises P and Cu;
optionally, the nanocrystalline phase comprises α-Fe;
optionally, the metal carbide is XC.

### Claim 5 (depends on 1)

The amorphous nanocrystalline soft magnetic material according to claim 1, wherein the nanocrystalline phase has an average particle size of less than or equal to 30 nm; optionally, the nanocrystalline phase has the average particle size of 10 nm to 20 nm;
optionally, the fine crystalline particle has an average particle size of less than or equal to 10 nm; optionally, the fine crystalline particle has the average particle size of 5 nm to 8 nm;
optionally, in the amorphous nanocrystalline soft magnetic material, the nanocrystalline phase has an atomic percentage of 50 at % to 70 at %;
optionally, in the amorphous nanocrystalline soft magnetic material, the fine crystalline particle has an atomic percentage of 0.1 at % to 2 at %.

### Claim 6 (depends on 1)

A preparation method for the amorphous nanocrystalline soft magnetic material according to claim 1, wherein the method comprises the following steps:
(1) proportioning a raw material of formulation amount followed by preparing an amorphous alloy; and
(2) subjecting the amorphous alloy described in step (1) to a two-stage crystallization under a protective condition, and cooling to obtain the amorphous nanocrystalline soft magnetic material, wherein the crystallization temperature of the second stage is higher than the crystallization temperature of the first stage.

### Claim 7 (depends on 6)

The preparation method according to claim 6, wherein the crystallization temperature of the first stage in step (2) is 5° C. to 20° C. below the onset temperature of the first crystallization peak of the amorphous alloy in step (1).

### Claim 8 (depends on 6)

The preparation method according to claim 6, wherein, optionally, the crystallization temperature of the second stage in step (2) is 30° C. to 100° C. above the onset temperature of the first crystallization peak of the amorphous alloy in step (1).

### Claim 9 (depends on 6)

The preparation method according to claim 6, wherein a method of preparing the amorphous alloy in step (1) comprises the following steps:
(11) melting the proportioned raw material under a protective condition to obtain an alloy liquid or an alloy ingot;
(12) cooling the alloy liquid in step (11) to obtain the amorphous alloy; or
remelting the alloy ingot in step (11) and cooling to obtain the amorphous alloy;
optionally, a purity of the raw material in step (11) is greater than 99 wt. %;
optionally, the protective condition in step (11) includes vacuum or protective gas;
optionally, the protective gas includes nitrogen or argon;
optionally, a temperature of melting in step (11) is 1300° C. to 1500° C.;
optionally, a method of melting in step (11) includes any one of arc melting, intermediate frequency induction melting or high frequency induction melting;
optionally, a cooling rate of cooling in step (12) is greater than or equal to 106° C./s;
optionally, a method of cooling in step (12) includes a single-roll cold method, a copper mold blow-casting method, a copper mold suction casting method or a Taylor method, and optionally, the single-roll cold method;
optionally, the protective condition in step (2) includes vacuum or protective gas;
optionally, the protective gas includes nitrogen and/or argon;
optionally, a heating rate to the crystallization temperature of the first stage in step (2) is 5° C./min to 10° C./min;
optionally, a holding time at the crystallization temperature of the first stage in step (2) is 5 min to 30 min;
optionally, the onset temperature of the first crystallization peak of the amorphous alloy is measured and obtained by a differential scanning calorimetry;
optionally, a heating rate to the crystallization temperature of the second stage in step (2) is 5° C./min to 10° C./min;
optionally, a holding time at the crystallization temperature of the second stage in step (2) is 30 min to 60 min.

### Claim 10 (depends on 6)

The preparation method according to claim 6, wherein the method comprises the following steps:
(11) proportioning the raw material with a purity of more than 99% in a formulation amount, melting the proportioned raw material into alloy ingot at a temperature of 1300° C. to 1500° C. under a condition of vacuuming and/or filling with protective gas;
(12) remelting the alloy ingot in step (11) and then cooling the melt by the single-roll cold method, wherein a cooling rate of the cooling is greater than or equal to 106° C./s, to obtain an amorphous alloy; and
(2) under a condition of vacuuming or filling with protective gas, heating the amorphous alloy in step (12) to a crystallization temperature of the first stage at a heating rate of 5° C./min to 10° C./min, keeping the temperature for 5 min to 30 min, then heating to a crystallization temperature in the second stage at a heating rate of 5° C./min to 10° C./min, keeping the temperature for 30 min to 60 min, and cooling to obtain the amorphous nanocrystalline soft magnetic material; wherein the crystallization temperature in the first stage is 5° C. to 20° C. below the onset temperature of the first crystallization peak of the amorphous alloy in step (12), and the crystallization temperature in the second stage is 30° C. to 100° C. above the onset temperature of the first crystallization peak of the amorphous alloy in step (12).

### Claim 11 (depends on 6)

An amorphous ribbon, wherein the amorphous ribbon is composed of the amorphous alloy prepared in step (1) of the preparation method according to claim 6.

### Claim 12 (depends on 1)

An amorphous nanocrystalline ribbon, wherein the amorphous nanocrystalline ribbon is composed of the amorphous nanocrystalline soft magnetic material according to claim 1.

### Claim 13 (depends on 1)

An amorphous nanocrystalline magnetic sheet, wherein the amorphous nanocrystalline magnetic sheet is prepared from the amorphous nanocrystalline soft magnetic material according to claim 1.

### Claim 14

(canceled)